JP5636789B2 - Paper container - Google Patents

Paper container Download PDF

Info

Publication number
JP5636789B2
JP5636789B2 JP2010168111A JP2010168111A JP5636789B2 JP 5636789 B2 JP5636789 B2 JP 5636789B2 JP 2010168111 A JP2010168111 A JP 2010168111A JP 2010168111 A JP2010168111 A JP 2010168111A JP 5636789 B2 JP5636789 B2 JP 5636789B2
Authority
JP
Japan
Prior art keywords
paper box
resin film
ruled line
paper
flange
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP2010168111A
Other languages
Japanese (ja)
Other versions
JP2012025470A (en
Inventor
宏太朗 雨河
宏太朗 雨河
谷口 正幸
谷口  正幸
祥子 有本
祥子 有本
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toppan Inc
Original Assignee
Toppan Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toppan Inc filed Critical Toppan Inc
Priority to JP2010168111A priority Critical patent/JP5636789B2/en
Publication of JP2012025470A publication Critical patent/JP2012025470A/en
Application granted granted Critical
Publication of JP5636789B2 publication Critical patent/JP5636789B2/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、例えば、食品の流通用や食事用、トイレタリー用品の流通に用いられる紙製容器に関し、バリア性、耐水性、レトルト耐性などの機能に優れ、複数の種類の内容物を充填することができる紙製容器に関する。 The present invention relates to, for example, a paper container used for the distribution of food, meals, and toiletries, and is excellent in functions such as barrier properties, water resistance, and retort resistance, and is filled with a plurality of types of contents. about the paper container that can.

食品やトイレタリー用品の一次容器として用いられる紙製の容器は、内容物が紙製容器に直接収容されているため、内容物と紙製容器の内面が直接接触している。こうした一次容器としては、紙箱の内面に熱可塑性プラスチックシートを積層した紙製容器が用いられている(特許文献1参照)。   In a paper container used as a primary container for foods and toiletries, the contents are directly stored in the paper container, so the contents and the inner surface of the paper container are in direct contact. As such a primary container, a paper container in which a thermoplastic sheet is laminated on the inner surface of a paper box is used (see Patent Document 1).

しかしながら、この紙製容器は、紙箱の内面にのみ熱可塑性プラスチックシートを積層しているため、紙箱の外面は、防水性などを有しておらず、温水殺菌や調理する際に、紙箱の外面が吸水してしまうという問題があった。紙箱の外面が吸水した際、紙の層間剥離などが起こり、紙製容器は強度低下による変形や、紙箱の外面が印刷層である場合には、印刷層の剥がれによる美称性や必要情報の欠損など、さまざまな不具合が生じる。   However, since this paper container has a thermoplastic sheet laminated only on the inner surface of the paper box, the outer surface of the paper box is not waterproof and the outer surface of the paper box when sterilizing or cooking with hot water. Had the problem of water absorption. When the outer surface of the paper box absorbs water, delamination of the paper occurs, and the paper container is deformed due to a decrease in strength, and when the outer surface of the paper box is a printed layer, the nickname and lack of necessary information due to the peeling of the printed layer Various problems occur.

また通常の紙製容器では、ブランクを用いて紙箱を製函しており、紙箱の四側面上端縁に連結されたフランジは、フランジ重ね片により隣り合うフランジ同士が互いに重なり合う構造となり、フランジ上面に紙1枚分の段差が生じる。段差を有するフランジ上面に蓋材を接着すると、この段差により内容物が漏れ、蓋材の接着強度が低下するなどの不具合が生じることが指摘されている。   Moreover, in a normal paper container, a paper box is manufactured using a blank, and the flange connected to the upper edge of the four side surfaces of the paper box has a structure in which adjacent flanges overlap each other by overlapping flange pieces, and the upper surface of the flange is A level difference is generated for one sheet of paper. It has been pointed out that when a lid member is bonded to the upper surface of a flange having a step, problems such as leakage of contents due to the step and a decrease in the bonding strength of the lid member occur.

前記不具合に対して、内紙箱と外紙箱からなる紙箱の内面及び外面の各面に樹脂フィルムを積層し、紙製容器の内面のみならず外面にも耐性を付与することが提案されている。これによれば、内面樹脂フィルムと外面樹脂フィルムが紙箱を覆うように接着されているためフランジ端面からの吸水も防止し、紙の層間剥離などによる、紙製容器の強度低下による変形や、紙箱の外面に印刷層がある場合でも、印刷層の剥がれによる美称性や必要情報の欠損などのさまざまな不具合が生じることがない。そのため、バリア性、耐水性、レトルト耐性などの機能に優れる。また、紙製容器を蓋材とヒートシールした時に、シール漏れなどのシール不良が起こらず、しかも紙箱と樹脂フィルムの間に空気が溜まることがない(特許文献2参照)。   In order to cope with the problem, it has been proposed that resin films are laminated on the inner and outer surfaces of a paper box composed of an inner paper box and an outer paper box to give resistance not only to the inner surface of the paper container but also to the outer surface. According to this, since the inner surface resin film and the outer surface resin film are bonded so as to cover the paper box, water absorption from the end surface of the flange is also prevented, deformation due to a decrease in strength of the paper container due to delamination of the paper, and the paper box Even when there is a printed layer on the outer surface, various problems such as aesthetics due to peeling of the printed layer and loss of necessary information do not occur. Therefore, it is excellent in functions such as barrier properties, water resistance, and retort resistance. Further, when the paper container is heat-sealed with the lid, no sealing failure such as seal leakage occurs, and air does not collect between the paper box and the resin film (see Patent Document 2).

また製函の際にフランジを折り曲げても戻ってしまう現象があり、成形時にフィルムが破れ、製函を行うと、フランジ部に罫線が罫割れを起こし、成形フィルムを突き破ってバリア性を消失させてしまう不具合が発生することがあった。これを解決するために、内面樹脂フィルムを内面に積層し、内面側から折れ罫線を設けた内紙箱と、外面樹脂フィルムを外面に積層下外面側から折れ罫線を設けた外紙箱からなる紙製容器が提案されている(特許文献3参照)。   Also, there is a phenomenon that even if the flange is bent during box making, the film breaks during molding, and when box making, the ruled line breaks in the flange part, breaking the molded film and eliminating the barrier property There was a problem that would occur. In order to solve this, a paper made of an inner paper box in which an inner resin film is laminated on the inner surface and a crease line is provided from the inner surface side, and an outer paper box in which an outer resin film is laminated on the outer surface from the lower outer surface side is provided. A container has been proposed (see Patent Document 3).

しかしながら、容器に仕切り板がないため、複数の種類の内容物を充填することができない。今までは別々の容器、もしくは小包装に充填していたが、コストの上昇につながってしまっていた。   However, since there is no partition plate in the container, a plurality of types of contents cannot be filled. Until now, it was filled in separate containers or small packages, but this led to increased costs.

特開平9−254280号公報JP-A-9-254280 特願2009−246409号公報Japanese Patent Application No. 2009-246409 特願2010−162719号公報Japanese Patent Application No. 2010-162719

本発明は、前記の不具合を解消するために、内紙箱に折りこみを設け、仕切り板として複数の内容物を充填できるようにすると、罫線が罫割れを起こし、成形時にフィルムが破れ、製函を行うと成形フィルムを突き破ってバリア性を消失させてしまう不具合が発生することがあり、バリア性、耐水性、レトルト耐性などの機能に優れた、また、紙製容器を蓋材とヒートシールした時に、シール漏れなどのシール不良が起こりにくい、複数の種類の内容物を充填することができる仕切り板を持った紙製容器とその製造方法を提供することを目的とする。   In order to solve the above-mentioned problems, the present invention provides a folding in the inner paper box so that a plurality of contents can be filled as a partition plate. May cause problems that break through the molded film and lose the barrier properties, and has excellent functions such as barrier properties, water resistance, retort resistance, and heat sealed paper containers with the lid It is an object of the present invention to provide a paper container having a partition plate that can be filled with a plurality of types of contents, and a method of manufacturing the same.

上記の課題を解決するための手段として、請求項1に記載の発明は、底部、胴部、フランジ部、仕切り板が各々折れ罫線により連設し、かつ一枚のブランクからなる内紙箱と、内紙箱の内面に積層された該内紙箱の内面より大きい内面樹脂フィルムと底部、胴部、フランジ部、仕切り板が各々折れ罫線により連設し、かつ一枚のブランクからなる外紙箱と外紙箱の外面に積層された該外紙箱の外面より大きい外面樹脂フィルムとからなり、前記内紙箱の外面と前記外紙箱の内面が重ね合わされ、前記内面樹脂フィルムと前記外面樹脂フィルムの周縁部が貼り合わされてなる折れ罫線は、内紙箱の内面側から罫線を形成したものであり前記外紙箱の胴部とフランジ部との境界となる折れ罫線は、外紙箱の外面側から罫線を形成したものであることを特徴とする紙製容器である。   As means for solving the above-mentioned problems, the invention according to claim 1 is characterized in that the bottom portion, the trunk portion, the flange portion, and the partition plate are continuously arranged by a crease line, and an inner paper box consisting of a single blank, An outer paper box and an outer paper box made of a single blank, in which the inner resin film, which is laminated on the inner surface of the inner paper box, is larger than the inner surface of the inner paper box, and the bottom, body, flange, and partition plate are connected by crease lines. An outer surface resin film larger than the outer surface of the outer paper box laminated on the outer surface of the inner paper box, the outer surface of the inner paper box and the inner surface of the outer paper box are overlapped, and the peripheral portion of the inner surface resin film and the outer surface resin film are bonded together. The folded ruled line is formed from the inner surface side of the inner paper box, and the folded ruled line that forms the boundary between the body portion and the flange portion of the outer paper box is formed from the outer surface side of the outer paper box. A paper container according to claim.

また、請求項2に記載の発明は、前記内紙箱の仕切り板が、内紙箱の内面側から罫を入れ、前記内紙箱の中央部を内面側から見て山折し、底部となる部分を谷折して成形されていることを特徴とする請求項1に記載の紙製容器である。   In the invention according to claim 2, the partition plate of the inner paper box has a ruled line from the inner surface side of the inner paper box, folds the mountain when the central portion of the inner paper box is viewed from the inner surface side, and the bottom portion is a valley. The paper container according to claim 1, wherein the paper container is formed by folding.

また、請求項3に記載の発明は、内紙箱あるいは外紙箱にフランジを有し、内紙箱の内面側から罫を入れ、フランジ部の罫を山折りにすることを特徴とする請求項1または2に記載の紙製容器である。   The invention according to claim 3 is characterized in that the inner paper box or the outer paper box has a flange, the ruled line is formed from the inner surface side of the inner paper box, and the ruled line of the flange portion is folded in a mountain. 2. A paper container according to 2.

また、請求項4に記載の発明は、前記フランジを有する内紙箱が、一枚のブランクを製函してなり、前記紙箱の四面上端縁に連結されたフランジは、隣り合うフランジどうしの端部が突き合わせになっており、互いに重なり合っていないことを特徴とする請求項1から3のいずれか一項に記載の紙製容器である。 The invention according to claim 4, the inner carton with the flange, made by Seihako a single blank, the flange which is connected to the four side surfaces upper edge of the paper box, each other adjacent flanges The paper container according to any one of claims 1 to 3, wherein the ends are butted and do not overlap each other.

内紙箱2の内面に内紙箱2の内面より大きい内面樹脂フィルム3を積層し、内紙箱には、仕切り板17を、内紙箱の内面側から罫を入れ、前記内紙箱の中央部を内面側から見て山折し、底部となる部分を谷折し、一方外紙箱5の外面には外紙箱5の外面より大きい外面樹脂フィルム4が積層し、内紙箱2の外面と外紙箱5の内面が重なるように、内面樹脂フィルム3と外面樹脂フィルム4の周縁部を貼り合わさることにより、紙製容器1の内面のみならず外面にも耐水性が付与され、しかも、内面樹脂フィルム3と外面樹脂フィルム4が内紙箱2と外紙箱5を覆うように張り合わせられているため、紙の端面からの吸水も起こらず、紙の吸水による強度劣化が起きないので、レトルト殺菌処理や、湯煎などを行うことが可能となる。   An inner surface resin film 3 larger than the inner surface of the inner paper box 2 is laminated on the inner surface of the inner paper box 2, and a partition plate 17 is provided in the inner paper box from the inner surface side of the inner paper box. When viewed from the top, the bottom portion is folded in a valley, while the outer surface of the outer paper box 5 is laminated with an outer surface resin film 4 larger than the outer surface of the outer paper box 5, and the outer surface of the inner paper box 2 and the inner surface of the outer paper box 5 are By bonding the peripheral portions of the inner surface resin film 3 and the outer surface resin film 4 so as to overlap, water resistance is imparted not only to the inner surface of the paper container 1 but also to the outer surface, and the inner surface resin film 3 and the outer surface resin film. Since 4 is laminated so as to cover the inner paper box 2 and the outer paper box 5, water absorption from the end surface of the paper does not occur, and strength deterioration due to water absorption of the paper does not occur. Is possible.

内紙箱2の内面に該内紙箱2の内面より大きい内面樹脂フィルム3を積層し、外紙箱5の外面に該外紙箱5の外面より大きい外面樹脂フィルム4が積層し、前記内紙箱2の外面と前記外紙箱5の内面を重ね合わせ、前記内面樹脂フィルム3と前記外面樹脂フィルム4の周縁部を貼り合わせることにより、紙箱と樹脂フィルムの間に空気が溜まることがなく、それによる樹脂フィルムの破れが生ずることがない。   An inner surface resin film 3 larger than the inner surface of the inner paper box 2 is laminated on the inner surface of the inner paper box 2, and an outer surface resin film 4 larger than the outer surface of the outer paper box 5 is laminated on the outer surface of the outer paper box 5. And the inner surface of the outer paper box 5 are overlapped, and the peripheral portions of the inner resin film 3 and the outer resin film 4 are bonded to each other, so that air does not collect between the paper box and the resin film. No tearing will occur.

また内紙箱2の内面に該内紙箱2の内面より大きい内面樹脂フィルム3を積層し、内面樹脂フィルム3を真空成形法又は/及び圧空成形法により成形型12内に設置した内紙箱2に積層させることにより、内面樹脂フィルム3を、真空成形法又は/及び圧空成形法により内紙箱3に密着させているため、内面樹脂フィルム3は、内紙箱2の形状に追随するように精度良く積層することができる。   Further, an inner surface resin film 3 larger than the inner surface of the inner paper box 2 is laminated on the inner surface of the inner paper box 2, and the inner surface resin film 3 is laminated on the inner paper box 2 installed in the molding die 12 by a vacuum forming method and / or a pressure forming method. Since the inner surface resin film 3 is brought into close contact with the inner paper box 3 by the vacuum forming method and / or the pressure forming method, the inner surface resin film 3 is accurately laminated so as to follow the shape of the inner paper box 2. be able to.

また外紙箱5の外面に該外紙箱5の外面より大きい外面樹脂フィルム4が積層し、外面樹脂フィルム4を真空成形法又は/及び圧空成形法により成形型12内に設置した外紙箱5に積層させることにより、外面樹脂フィルム4を、真空成形法又は/及び圧空成形法により外紙箱5に密着させているため、外面樹脂フィルム4は、外紙箱5の形状に追随するように精度良く積層することができる。   Further, an outer surface resin film 4 larger than the outer surface of the outer paper box 5 is laminated on the outer surface of the outer paper box 5, and the outer surface resin film 4 is laminated on the outer paper box 5 installed in the molding die 12 by a vacuum forming method and / or a pressure forming method. Since the outer surface resin film 4 is brought into close contact with the outer paper box 5 by the vacuum forming method and / or the pressure forming method, the outer surface resin film 4 is accurately laminated so as to follow the shape of the outer paper box 5. be able to.

内紙箱2は内面側から折り罫線10を入れることで、仕切り板17上部とフランジ部7の罫が山折りとなり、折り曲げた仕切り板17上部とフランジ部7は形状が維持されやすい。一方仕切り板17の下部と内紙箱2の胴部15は内面側から折り罫線10を入れることで、谷折りとなり、切り板17の下部と胴部15は元の形状に戻りやすい。外紙箱4は外面側から折り罫線10を入れることで、折り曲げた胴部15は形状が維持され易く、外紙箱5は、内紙箱2が広がる力を抑制するため、成形性が向上する。   The inner paper box 2 is provided with a crease line 10 from the inner surface side, whereby the upper part of the partition plate 17 and the ruled part of the flange part 7 are fold-folded, and the shape of the folded upper part of the partition board 17 and the flange part 7 is easily maintained. On the other hand, the lower part of the partition plate 17 and the body part 15 of the inner paper box 2 are valley-folded by inserting the crease line 10 from the inner surface side, and the lower part of the cut plate 17 and the body part 15 are likely to return to the original shape. Since the outer paper box 4 is provided with the crease lines 10 from the outer surface side, the shape of the folded body part 15 is easily maintained, and the outer paper box 5 suppresses the force that the inner paper box 2 spreads, so that the formability is improved.

仕切り板を持つ内紙箱用ブランク18の外側から折り罫線10を形成すると、仕切り板17下部及びフランジ部7を折り曲げても元の形状に戻り易い。したがって、製函の過程において、仕切り板17とフランジ部7が傷つき、フィルムにピンホールが開くなどの不具合があった。本発明では、内紙箱2では内側から折れ罫線10を形成しているため、元に戻るとすると外紙箱4のフランジ部7を、内紙箱2のフランジ部7が押さえつけるため、内紙箱底部を折り曲げて仕切り板17を形成しても、成形性を維持し、フィルムにピンホールが開くなどの不具合を解消しつつ、更に複数の種類の内容物を充填することができる。   When the folded ruled line 10 is formed from the outside of the inner paper box blank 18 having the partition plate, the original shape is easily restored even when the lower portion of the partition plate 17 and the flange portion 7 are folded. Therefore, in the box making process, the partition plate 17 and the flange portion 7 are damaged, and there are problems such as pinholes opening in the film. In the present invention, since the inner paper box 2 has a folded ruled line 10 from the inside, when returning to the original, the flange portion 7 of the outer paper box 4 is pressed against the flange portion 7 of the inner paper box 2, so the bottom of the inner paper box 2 is bent. Even if the partition plate 17 is formed, it is possible to fill a plurality of types of contents while maintaining the moldability and solving the problems such as pinholes opening in the film.

本発明により、バリア機能を有する紙製複合容器において課題となっている廃棄ごみの減量化ができ、電子レンジでの加熱、器としての使用ができ、割れる等の危険がないという従来からの特長を保持しつつ、フランジの戻りを抑えることで成形性を向上させ、製函
工程におけるフランジ部での罫線割れによる、成形フィルムの破れによるバリア性の消失事故を防ぎ、複数の種類の内容物を充填することができる仕切り板を持った紙製容器を提供できる。
According to the present invention, it is possible to reduce waste waste, which is a problem in a paper composite container having a barrier function, heating in a microwave oven, use as a container, and there is no risk of cracking etc. The moldability is improved by suppressing the return of the flange while holding the film, preventing the loss of the barrier property due to the tearing of the molded film due to the ruled line cracking in the flange part in the box making process. A paper container having a partition plate that can be filled can be provided.

本発明の実施形態に係る紙製容器1の斜視図1 is a perspective view of a paper container 1 according to an embodiment of the present invention. 図1に示す紙製容器1のA−A´線における断面図Sectional drawing in the AA 'line of the paper container 1 shown in FIG. 本発明で使用する仕切り板付き内紙箱ブランクの一例を示す平面図The top view which shows an example of the inner paper box blank with a partition plate used by this invention 本発明で使用する外紙箱ブランクの一例を示す平面図The top view which shows an example of the outer paper box blank used by this invention 本発明の実施形態に係る紙製容器1の製造方法を説明する成形型の断面図Sectional drawing of the shaping | molding die explaining the manufacturing method of the paper container 1 which concerns on embodiment of this invention 本発明の実施形態に係る紙製容器1の製造工程の説明図Explanatory drawing of the manufacturing process of the paper container 1 which concerns on embodiment of this invention. 本発明の内紙箱の内面側から罫を入れた仕切り板、フランジ部の状態を示した断面図Sectional drawing which showed the state of the partition plate which put the ruled from the inner surface side of the inner paper box of this invention, and a flange part 本発明の外紙箱の外面側から罫を入れたフランジ部の状態を示した断面図Sectional drawing which showed the state of the flange part which ruled from the outer surface side of the outer paper box of this invention 本発明の内紙箱の内面側から罫を入れた仕切り板、胴部の状態を示した断面図Sectional drawing which put the ruled from the inner surface side of the inner paper box of this invention, and showed the state of the trunk 本発明の外紙箱の外面側から罫を入れた胴部の状態を示した断面図Sectional drawing which showed the state of the trunk | drum which put a rule from the outer surface side of the outer paper box of this invention 本発明の罫線を施した内紙箱、外紙箱それぞれの罫線部膨らみを示した断面図Sectional drawing which showed the swell of the ruled line part of each inner paper box and outer paper box which gave the ruled line of this invention

以下本発明を実施するための形態を、図面を用いて詳細に説明する。図1は、本発明の一実施形態に係る仕切り板を持つ紙製容器1の斜視図である。図2は、図1に示す紙製容器1のA−A´線における断面図である。   DESCRIPTION OF EMBODIMENTS Hereinafter, embodiments for carrying out the present invention will be described in detail with reference to the drawings. FIG. 1 is a perspective view of a paper container 1 having a partition plate according to an embodiment of the present invention. FIG. 2 is a cross-sectional view taken along the line AA ′ of the paper container 1 shown in FIG.

図1及び2に示すように、本発明の紙製容器1は、仕切り板17とフランジ部7が付いた内紙箱2の内面に内面樹脂フィルム3を積層し、フランジ部7付き外紙箱4の外面に外面樹脂フィルム5を積層し、仕切り板17とフランジ部7付き内紙箱2の外面とフランジ部7付き外紙箱4の内面を重ね合わせ、内面樹脂フィルム3と外面樹脂フィルム5の周縁部を熱融着して、一体化してなる。   As shown in FIGS. 1 and 2, the paper container 1 of the present invention has an inner resin film 3 laminated on the inner surface of an inner paper box 2 with a partition plate 17 and a flange portion 7. The outer surface resin film 5 is laminated on the outer surface, the outer surface of the partition plate 17 and the inner paper box 2 with the flange portion 7 and the inner surface of the outer paper box 4 with the flange portion 7 are overlapped, and the peripheral portions of the inner surface resin film 3 and the outer surface resin film 5 are overlapped. It is fused and integrated.

仕切り板17とフランジ部7付き内紙箱2やフランジ部7付き外紙箱4は、ボール紙や板紙、それらと樹脂フィルム層や金属層などを貼合わせ製函してなるものや、箱型に成形されたパルプモールドなどを用いることができるが、これらに限定されるものではない。また、図1に示す紙製容器1は底が浅い四角いトレー構造であるが、その構造は、使用する目的や条件によって適宜変更される。   The partition plate 17 and the inner paper box 2 with the flange portion 7 and the outer paper box 4 with the flange portion 7 are formed by bonding cardboard and paperboard, and bonding them with a resin film layer, a metal layer, or the like, or a box shape. However, it is not limited to these. Moreover, although the paper container 1 shown in FIG. 1 is a square tray structure with a shallow bottom, the structure is suitably changed according to the purpose and conditions to be used.

図3に仕切り板17を持つ内紙箱2のブランク18の一例と図4に外紙箱5のブランク6の一例を示す。内紙箱2と外紙箱5をブランク18、ブランク6より形成し、紙箱の内面及び外面の両面に内面樹脂フィルム3及び外面樹脂フィルム4をそれぞれに積層することで十分な強度、形状安定性を付与することができる。この時仕切り板17は一つではなく複数も受けることも可能である。   FIG. 3 shows an example of the blank 18 of the inner paper box 2 having the partition plate 17 and FIG. 4 shows an example of the blank 6 of the outer paper box 5. Inner paper box 2 and outer paper box 5 are formed from blank 18 and blank 6, and sufficient strength and shape stability are imparted by laminating inner resin film 3 and outer resin film 4 on both the inner and outer surfaces of the paper box. can do. At this time, it is possible to receive a plurality of partition plates 17 instead of one.

図5は紙製容器1の製造方法を示しており、成形型12に内紙箱2、内面樹脂フィルム3を積層し、ヒーター11により一体化される。この時深絞り成形法、特に、真空成形法又は/及び圧空成形法により積層されることが好ましい。   FIG. 5 shows a method of manufacturing the paper container 1. The inner paper box 2 and the inner surface resin film 3 are laminated on the mold 12 and integrated by the heater 11. At this time, the film is preferably laminated by a deep drawing method, particularly a vacuum forming method and / or a pressure forming method.

内紙箱2や外紙箱4を構成する材料として、例えば上記した板紙を用いた場合、板紙からなるブランクを箱形状に製函する際に、重ね片16を、接着部材を用いて留める必要がある。ここでの接着部材としては、酢酸ビニル系水性接着剤、ホットメルトや、エチレンと酢酸ビニルの共重合樹脂(EVA)、塩化ビニルと酢酸ビニルの共重合体、エチレンとアクリル酸の共重合樹脂(EAA)、変性オレフィン系のヒートシールニスなどを用いる
ことができる。
When the above-described paperboard is used as a material constituting the inner paper box 2 and the outer paper box 4, for example, when a blank made of paperboard is box-shaped, it is necessary to fasten the overlapping pieces 16 using an adhesive member. . Adhesive members here include vinyl acetate water-based adhesives, hot melt, ethylene / vinyl acetate copolymer resin (EVA), vinyl chloride / vinyl acetate copolymer, ethylene / acrylic acid copolymer resin ( EAA), modified olefin heat seal varnish, and the like can be used.

内面樹脂フィルム3及び外面樹脂フィルム5としては、低密度ポリエチレン(LDPE)、中密度ポリエチレン、直鎖状低密度ポリエチレン(LLDPE)、あるいは、エチレンとアクリル酸の共重合樹脂(EAA)などのポリエチレンやその変性樹脂や、また、ホモポリプロピレン、ランダムポリプロピレン共重合体、ブロックポリプロピレン共重合体などのポリプロピレン(PP)、あるいは、6ナイロン、66ナイロン、MXD−6ナイロンなどのナイロンや、エチレンビニルアルコール(EVOH)樹脂や、ポリ塩化ビニリデン(PVDC)などの樹脂を用いることができる。
これらを単層で、あるいは、組み合わせた多層で用いることもできる。紙製容器1へ積層した後の各樹脂フィルムの膜厚としては、30μm以上、500μm以下であることが好ましい。膜厚が500μmよりと厚いと、積層時にフィルム膜厚が不均一になることがあり、好ましくない。また、30μm未満では樹脂フィルムにピンホールが発生する危険性が高い。
Examples of the inner resin film 3 and the outer resin film 5 include polyethylene such as low density polyethylene (LDPE), medium density polyethylene, linear low density polyethylene (LLDPE), or a copolymer resin (EAA) of ethylene and acrylic acid, The modified resin, polypropylene (PP) such as homopolypropylene, random polypropylene copolymer, block polypropylene copolymer, nylon such as 6 nylon, 66 nylon, MXD-6 nylon, and ethylene vinyl alcohol (EVOH) ) Resins and resins such as polyvinylidene chloride (PVDC) can be used.
These can be used in a single layer or a combination of multiple layers. The film thickness of each resin film after being laminated on the paper container 1 is preferably 30 μm or more and 500 μm or less. When the film thickness is thicker than 500 μm, the film thickness may be non-uniform during lamination, which is not preferable. Moreover, if it is less than 30 μm, there is a high risk of pinholes occurring in the resin film.

本発明における紙製容器1の作製は次の通り行う。まず、図3に示すようなブランク18を内紙箱2に組み立てる。ブランク18は、底面8、側面9、仕切り板17、側面上端縁に連結されたフランジ7とから成り、紙からなるブランク18を打ち抜いて各部が構成され、これを折り罫線に沿って折り込み組み立てて内紙箱2とする。   The paper container 1 according to the present invention is manufactured as follows. First, a blank 18 as shown in FIG. 3 is assembled in the inner paper box 2. The blank 18 includes a bottom surface 8, a side surface 9, a partition plate 17, and a flange 7 connected to the upper end edge of the side surface. A blank 18 made of paper is punched out to form each part, and this is folded and assembled along a crease line. The inner paper box 2 is assumed.

図4に示すようなブランク6を外紙箱5に組み立てる。ブランク6は、底面8、側面9、側面上端縁に連結されたフランジ7とから成り、紙からなるブランク6を打ち抜いて各部が構成され、これを折り罫線に沿って折り込み組み立てて外紙箱5とする。   A blank 6 as shown in FIG. 4 is assembled in the outer paper box 5. The blank 6 includes a bottom surface 8, a side surface 9, and a flange 7 connected to the upper edge of the side surface. The blank 6 is formed by punching out a blank 6 made of paper, and is folded along a crease line to assemble the outer paper box 5. To do.

ここで、本発明では、紙箱の四側面上端縁に連結されたフランジ7は、組み立てた時隣り合うフランジ7どうしの端部が突き合わせになっており、互いに重なり合っていないことが好ましい。紙箱の内面及び外面の両面に樹脂フィルムを積層することで十分な強度、形状安定性を付与することができる。   Here, in the present invention, it is preferable that the flanges 7 connected to the upper edge of the four side surfaces of the paper box are abutted at the ends of the adjacent flanges 7 when assembled, and do not overlap each other. Sufficient strength and shape stability can be imparted by laminating resin films on both the inner and outer surfaces of the paper box.

次に、内紙箱2の内面に内面樹脂フィルム3を積層する。内紙箱2に内面樹脂フィルム3を積層するには、深絞り成形法、特に、真空成形法又は/及び圧空成形法により積層されることが好ましい。   Next, the inner surface resin film 3 is laminated on the inner surface of the inner paper box 2. In order to laminate the inner surface resin film 3 on the inner paper box 2, it is preferred that the inner resin film 3 is laminated by a deep drawing method, in particular, a vacuum forming method and / or a pressure forming method.

図5に示すように、組み立てた内紙箱2を成形型12の中にセットし、内紙箱2の上に内面樹脂フィルム3を載置する。該フランジ部7付き内紙箱2のフランジ部7と内面樹脂フィルム3をヒートシール等の方法で接着させる(プレシール)、と同時にヒーター11を用いて内面樹脂フィルム3を加熱軟化させる(プレヒートアップ)。熱接着条件、熱風温度等は使用する内面樹脂フィルム3の材質、厚さ等によって適宜変更される。   As shown in FIG. 5, the assembled inner paper box 2 is set in a mold 12, and the inner surface resin film 3 is placed on the inner paper box 2. The flange portion 7 of the inner paper box 2 with the flange portion 7 and the inner surface resin film 3 are adhered by a method such as heat sealing (pre-sealing), and at the same time, the inner surface resin film 3 is heated and softened using the heater 11 (pre-heating up). The heat bonding conditions, hot air temperature, and the like are appropriately changed depending on the material, thickness, and the like of the inner surface resin film 3 to be used.

次に、図6に示すように、内面樹脂フィルム3を積層した仕切り板17を持つ内紙箱2と、外面樹脂フィルム4を積層した外紙箱5とを、内紙箱2と外紙箱5が接するように重ね合わせる。
その後、例えば真空ポンプのような真空源より吸引管、吸引孔13を通じて成形型12下部より空気を吸引すると、型内の空気はフランジ部7付き内紙箱2の側面間や、通気性の紙層等を通して吸引され、その内部は真空状態になるので、加熱軟化された内面樹脂フィルム3は圧力により湾曲して仕切り板17とフランジ部7付き内紙箱2の内面に密着成形され、仕切り板17とフランジ部7付き内紙箱2と一体的に形成される(真空成形法)。
Next, as shown in FIG. 6, the inner paper box 2 having the partition plate 17 on which the inner surface resin film 3 is laminated and the outer paper box 5 on which the outer surface resin film 4 is laminated so that the inner paper box 2 and the outer paper box 5 are in contact with each other. To overlay.
Thereafter, when air is sucked from the lower part of the mold 12 through a suction tube and a suction hole 13 from a vacuum source such as a vacuum pump, the air in the mold is between the side surfaces of the inner paper box 2 with the flange portion 7 or a breathable paper layer. The inner resin film 3 that has been heated and softened is bent by pressure and is closely formed on the inner surface of the partition plate 17 and the inner paper box 2 with the flange portion 7. It is formed integrally with the inner paper box 2 with the flange portion 7 (vacuum forming method).

図7は内紙箱2の内面側から折れ罫10を入れた仕切り板17とフランジ部7の状態を示しており、仕切り板17は内紙箱2の中央部を内面側から見て山折し、底部となる部分
を谷折して成形されている。フランジ部7は山折れされており、折れ罫線10を形成した逆側は膨らみ、折り曲げたフランジ部7は形状が維持され易い。内紙箱2の谷折りされるフランジ部7は、折れ罫線10の罫線部膨らみ14が紙箱の外側にくることが必要である。図8は外紙箱5の外面側から罫を入れたフランジ部7の状態を示しており、谷折りされており、折れ罫線10を形成した逆側は膨らみ、折り曲げたフランジ部7は元の形状に戻り易い。
FIG. 7 shows a state of the partition plate 17 and the flange portion 7 in which the folded ruled line 10 is inserted from the inner surface side of the inner paper box 2, and the partition plate 17 is mountain-folded by viewing the central portion of the inner paper box 2 from the inner surface side. The part that becomes is folded and formed. The flange portion 7 is folded in a mountain, the opposite side where the folded ruled line 10 is formed swells, and the shape of the bent flange portion 7 is easily maintained. The flange portion 7 of the inner paper box 2 which is valley-folded requires that the crease portion bulge 14 of the crease ruled line 10 comes to the outside of the paper box. FIG. 8 shows a state of the flange portion 7 with a ruled line from the outer surface side of the outer paper box 5. The flange portion 7 is valley-folded, the opposite side where the folded ruled line 10 is formed swells, and the bent flange portion 7 has the original shape. Easy to return to.

図9は内紙箱2の内面側から折れ罫線10を入れた仕切り板17底部と胴部15の状態を示しており、谷折れされており、折れ罫線10を形成した逆側は膨らみ、折り曲げた仕切り板17底部と胴部15は元の形状に戻り易い。図10は外紙箱5の外面側から罫を入れた胴部15の状態を示しており、山折りされており、折れ罫線10を形成した逆側は罫線部膨らみ14、折り曲げた胴部15は維持され易い。   FIG. 9 shows a state of the bottom of the partition plate 17 and the body portion 15 where the folded ruled line 10 is inserted from the inner surface side of the inner paper box 2, which is folded at the valley, and the opposite side where the folded ruled line 10 is formed is swollen and bent. The bottom part of the partition plate 17 and the body part 15 are easy to return to the original shape. FIG. 10 shows a state of the body portion 15 with a ruled line from the outer surface side of the outer paper box 5, which is folded in a mountain, the reverse side on which the folded ruled line 10 is formed is the ruled line portion bulge 14, and the folded body portion 15 is Easy to maintain.

図11は本発明の実施例における折れ罫線10の形成を示しており、内紙箱2は内面側から折れ罫線10が入っており、罫線膨らみ14が紙箱の外側に形成される。一方外紙箱5の折り罫線10は外面側から形成されている。内紙箱2の仕切り板17とフランジ部7は折り罫線10を内側すると山折りとなり、形状が保持され易いが、仕切り板17底部と胴部15は逆に谷折れとなるので、外側に罫線を施した方が良い。一方外紙箱5の胴部15は折り罫線10を外面側すると形状が保持され易く、フランジ部6は逆に山折れとなるので、内側に罫線を施した方が良い。   FIG. 11 shows the formation of the folded ruled line 10 in the embodiment of the present invention. The inner paper box 2 includes the folded ruled line 10 from the inner surface side, and the ruled line bulge 14 is formed outside the paper box. On the other hand, the crease line 10 of the outer paper box 5 is formed from the outer surface side. The partition plate 17 and the flange portion 7 of the inner paper box 2 are mountain-folded when the folding ruled line 10 is placed inside, and the shape is easily maintained, but the bottom of the partition plate 17 and the body portion 15 are conversely valley-folded. It is better to give it. On the other hand, the body portion 15 of the outer paper box 5 is easily held when the crease line 10 is on the outer surface side, and the flange portion 6 is reversely folded, so it is better to have a ruled line inside.

しかしながら、表裏に折り罫線10を設けると工程が2倍になってしまう。フランジ部7の場合、外紙箱5のフランジ部7が元に戻るとするのを、内紙箱2のフランジ部7が押さえつけるため、外紙箱5のフランジ部7の折り罫線10を内側部に設ける必要ない。同様に内紙箱2の内側から形成された仕切り板17と胴部15の折り罫線10も、内紙箱2は外側に開こうとする反発力が発生し元の形状に戻りやすいが、外紙箱5の折り曲げられた胴部15が形状を維持し易く、成型フィルムがトレー全面を覆い、内紙箱2の胴15部の戻りを抑えるため、成形性を向上し、製函工程における罫線割れによる、成形フィルムの破れによるバリア性の消失事故を防ぐことができる。   However, if the crease lines 10 are provided on the front and back, the process is doubled. In the case of the flange portion 7, the flange portion 7 of the outer paper box 5 is pressed back by the flange portion 7 of the inner paper box 2, so that the fold ruled line 10 of the flange portion 7 of the outer paper box 5 needs to be provided on the inner side. Absent. Similarly, the partition plate 17 formed from the inner side of the inner paper box 2 and the crease line 10 of the body portion 15 also generate a repulsive force to open the inner paper box 2 to the outer side and easily return to the original shape, but the outer paper box 5 The folded body 15 is easy to maintain its shape, the molded film covers the entire surface of the tray, and the return of the body 15 of the inner paper box 2 is suppressed, so that the formability is improved and the line is cracked in the box making process. It is possible to prevent the loss of barrier properties due to film tearing.

1・・・紙製容器
2・・・内紙箱
3・・・内面樹脂フィルム
4・・・外面樹脂フィルム
5・・・外紙箱
6・・・ブランク(外紙箱用)
7・・・フランジ
8・・・底面
9・・・側面
10・・・折り罫線
11・・・ヒーター
12・・・成形型
13・・・吸引口
14・・・罫線部膨らみ
15・・・胴部
16・・・重ね片
17・・・仕切り板
18・・・仕切り板を持つ内紙箱用ブランク
DESCRIPTION OF SYMBOLS 1 ... Paper container 2 ... Inner paper box 3 ... Inner surface resin film 4 ... Outer surface resin film 5 ... Outer paper box 6 ... Blank (for outer paper box)
7 ... Flange 8 ... Bottom 9 ... Side 10 ... Folded crease line 11 ... Heater 12 ... Mold 13 ... Suction port 14 ... Ruled line bulge 15 ... Body Section 16 ... Stack piece 17 ... Partition plate 18 ... Blank for inner paper box with partition plate

Claims (4)

底部、胴部、フランジ部、仕切り板が各々折れ罫線により連設し、かつ一枚のブランクからなる内紙箱と、内紙箱の内面に積層された該内紙箱の内面より大きい内面樹脂フィルムと底部、胴部、フランジ部、仕切り板が各々折れ罫線により連設し、かつ一枚のブランクからなる外紙箱と外紙箱の外面に積層された該外紙箱の外面より大きい外面樹脂フィルムとからなり、前記内紙箱の外面と前記外紙箱の内面が重ね合わされ、前記内面樹脂フィルムと前記外面樹脂フィルムの周縁部が貼り合わされてなる折れ罫線は、内紙箱の内面側から罫線を形成したものであり前記外紙箱の胴部とフランジ部との境界となる折れ罫線は、外紙箱の外面側から罫線を形成したものであることを特徴とする紙製容器。   The bottom part, the body part, the flange part, and the partition plate are each connected by a folded ruled line, and an inner paper box made of a single blank, and an inner surface resin film and a bottom part laminated on the inner surface of the inner paper box and larger than the inner surface of the inner paper box The body part, the flange part, and the partition plate are each connected by a folded ruled line, and consist of an outer paper box made of one blank and an outer surface resin film larger than the outer surface of the outer paper box laminated on the outer surface of the outer paper box, The folded ruled line in which the outer surface of the inner paper box and the inner surface of the outer paper box are overlapped, and the inner resin film and the outer peripheral resin film are bonded together is a ruled line formed from the inner surface side of the inner paper box. A paper container characterized in that a folded ruled line that forms a boundary between a body part and a flange part of an outer paper box is formed by forming a ruled line from the outer surface side of the outer paper box. 前記内紙箱の仕切り板が、内紙箱の内面側から罫を入れ、前記内紙箱の中央部を内面側から見て山折し、底部となる部分を谷折して成形されていることを特徴とする請求項1に記載の紙製容器。   The partition plate of the inner paper box is formed by putting a ruled line from the inner surface side of the inner paper box, folding the mountain as viewed from the inner surface side of the inner paper box, and valley-folding the bottom portion. The paper container according to claim 1. 内紙箱あるいは外紙箱にフランジを有し、内紙箱の内面側から罫を入れ、フランジ部の罫を山折りにすることを特徴とする請求項1または2に記載の紙製容器。   The paper container according to claim 1 or 2, wherein the inner paper box or the outer paper box has a flange, a ruled line is formed from the inner surface side of the inner paper box, and the ruled line of the flange part is folded in a mountain. 前記フランジを有する内紙箱が、一枚のブランクを製函してなり、前記紙箱の四面上端縁に連結されたフランジは、隣り合うフランジどうしの端部が突き合わせになっており、互いに重なり合っていないことを特徴とする請求項1から3のいずれか一項に記載の紙製容器。 Inner carton having a flange made to Seihako a single blank, the flange which is connected to the four side surfaces upper edge of the carton is adapted to butt the ends of each other adjacent the flange, overlap each other paper container according to any one of claims 1 3, characterized in that not.
JP2010168111A 2010-07-27 2010-07-27 Paper container Expired - Fee Related JP5636789B2 (en)