JP4471249B2 - 磁性体 - Google Patents
磁性体 Download PDFInfo
- Publication number
- JP4471249B2 JP4471249B2 JP2000268192A JP2000268192A JP4471249B2 JP 4471249 B2 JP4471249 B2 JP 4471249B2 JP 2000268192 A JP2000268192 A JP 2000268192A JP 2000268192 A JP2000268192 A JP 2000268192A JP 4471249 B2 JP4471249 B2 JP 4471249B2
- Authority
- JP
- Japan
- Prior art keywords
- transition
- magnetic
- exhibits
- magnetostriction
- hydrogen
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Micromachines (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2000268192A JP4471249B2 (ja) | 2000-09-05 | 2000-09-05 | 磁性体 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2000268192A JP4471249B2 (ja) | 2000-09-05 | 2000-09-05 | 磁性体 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2002069596A JP2002069596A (ja) | 2002-03-08 |
| JP2002069596A5 JP2002069596A5 (OSRAM) | 2007-08-16 |
| JP4471249B2 true JP4471249B2 (ja) | 2010-06-02 |
Family
ID=18755000
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2000268192A Expired - Fee Related JP4471249B2 (ja) | 2000-09-05 | 2000-09-05 | 磁性体 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP4471249B2 (OSRAM) |
Families Citing this family (20)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| AU2003281305A1 (en) * | 2002-07-05 | 2004-01-23 | Matsushita Electric Industrial Co., Ltd. | Reader and authentication device including the same |
| JP3630164B2 (ja) * | 2002-08-21 | 2005-03-16 | 株式会社Neomax | 磁性合金材料およびその製造方法 |
| US7186303B2 (en) | 2002-08-21 | 2007-03-06 | Neomax Co., Ltd. | Magnetic alloy material and method of making the magnetic alloy material |
| JP3947066B2 (ja) * | 2002-09-05 | 2007-07-18 | 株式会社Neomax | 磁性合金材料 |
| AU2003301577A1 (en) | 2002-10-25 | 2004-05-13 | Showa Denko K.K. | Alloy containing rare earth element, production method thereof, magnetostrictive device, and magnetic refrigerant material |
| JP4399771B2 (ja) * | 2003-10-08 | 2010-01-20 | 日立金属株式会社 | 磁性粒子とその製造方法、及び磁性粒子ユニット |
| JP4218032B2 (ja) * | 2004-02-13 | 2009-02-04 | 日立金属株式会社 | 磁性合金及びその製造方法 |
| JP2006124783A (ja) * | 2004-10-29 | 2006-05-18 | Hitachi Metals Ltd | 磁性粒子及びその製造方法 |
| US7578892B2 (en) | 2005-03-31 | 2009-08-25 | Hitachi Metals, Ltd. | Magnetic alloy material and method of making the magnetic alloy material |
| US7815752B2 (en) | 2005-04-05 | 2010-10-19 | Hitachi Metals, Ltd. | Magnetic alloy and method for producing same |
| GB2459066B (en) * | 2007-02-12 | 2012-02-15 | Vacuumschmelze Gmbh & Co Kg | Article for magnetic heat exchange and method of manufacturing the same |
| KR101088535B1 (ko) | 2007-02-12 | 2011-12-05 | 바쿰슈멜체 게엠베하 운트 코. 카게 | 자기 열교환용 물품 및 그 제조 방법 |
| WO2009090442A1 (en) | 2007-12-27 | 2009-07-23 | Vacuumschmelze Gmbh & Co. Kg | Composite article with magnetocalorically active material and method for its production |
| DE112008003830B4 (de) | 2008-10-01 | 2025-01-09 | Vacuumschmelze Gmbh & Co. Kg | Verfahren zum Bearbeiten eines Gegenstandes mit mindestens einer magnetokalorisch aktiven Phase |
| GB2463931B (en) | 2008-10-01 | 2011-01-12 | Vacuumschmelze Gmbh & Co Kg | Method for producing a magnetic article |
| DE102008054522B4 (de) * | 2008-12-11 | 2013-11-21 | Leibniz-Institut Für Festkörper- Und Werkstoffforschung Dresden E.V. | Verfahren zur Beschichtung der Oberflächeeines magnetischen Legierungsmaterials sowie ein solches Legierungsmaterial |
| US9773591B2 (en) | 2009-05-06 | 2017-09-26 | Vacuumschmelze Gmbh & Co. Kg | Article for magnetic heat exchange and method of fabricating an article for magnetic heat exchange |
| CN101882493B (zh) * | 2009-05-08 | 2015-09-09 | 包头稀土研究院 | 磁性合金材料及其制造方法以及磁制冷系统 |
| US9895748B2 (en) | 2009-10-14 | 2018-02-20 | Vacuumschmelze & Gmbh & Co. Kg | Article for magnetic heat exchange and method of manufacturing the same |
| GB2482880B (en) | 2010-08-18 | 2014-01-29 | Vacuumschmelze Gmbh & Co Kg | An article for magnetic heat exchange and a method of fabricating a working component for magnetic heat exchange |
-
2000
- 2000-09-05 JP JP2000268192A patent/JP4471249B2/ja not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| JP2002069596A (ja) | 2002-03-08 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP4471249B2 (ja) | 磁性体 | |
| JP2002069596A5 (OSRAM) | ||
| Takenaka et al. | Magnetovolume effect and negative thermal expansion in Mn3 (Cu1− xGex) N | |
| Clark | Magnetostrictive RFe2 intermetallic compounds | |
| JP3466481B2 (ja) | 超磁歪材料 | |
| Wang et al. | Characterization of polycrystalline Fe2B compound with high saturation magnetization | |
| Hu et al. | Anisotropy compensation and magnetostrictive properties in Tbx Dy1− x (Fe0. 9Mn0. 1) 1.93 Laves compounds: Experimental and theoretical analysis | |
| Dai et al. | Magnetism, elasticity, and magnetostriction of FeCoGa alloys | |
| Levin et al. | Reversible spin-flop and irreversible metamagneticlike transitions induced by a magnetic field in the layered Gd 5 Ge 4 antiferromagnet | |
| JP3452210B2 (ja) | 磁歪材の製造方法 | |
| JP2970809B2 (ja) | 希土類永久磁石 | |
| Szymczak | From almost zero magnetostriction to giant magnetostrictive effects: recent results | |
| Zhang et al. | Design of high resistivity light-rare-earth-based PrFe1. 93 magnetostrictive alloys: Si doping and high-pressure annealing | |
| Du et al. | Magnetostriction in twin-free single crystals Tb y Dy 1− y Fe 2 with the addition of aluminum or manganese | |
| Wecker et al. | Magnetic hardening of (Sm, Zr) Fe3 alloys | |
| Wang et al. | Magnetic properties of Sm Fe Ti V alloys | |
| Hu et al. | Structural, magnetic and magnetostrictive behavior in Nd (Fe1− xCox) 1.9 compounds | |
| Takenaka et al. | Magnetostructural Correlations in Nitrogen-Deficient Antiperovskite Mn3CuN1-δ | |
| Stern et al. | Fe 3 Pd ferromagnetic shape memory alloys | |
| US6451131B1 (en) | Terbium-dysprosium-iron magnetostrictive materials and devices using these materials | |
| Duc | Development of giant low-field magnetostriction in a-TerfecoHan-based single layer, multilayer and sandwich films | |
| JP6930230B2 (ja) | 金属−絶縁体系ナノグラニュラー薄膜、及び薄膜磁気センサ | |
| Guo et al. | Structure, magnetic properties, and magnetostriction of Sm 0.88 Dy 0.12 (Fe 1− x M x) 2 (M= Mn, Al)(0⩽ x⩽ 0.2) | |
| Gabay et al. | Effect of Mg content in melt-spun Mn–Bi–Mg–Sb–In alloys on the structure and properties of field-annealed magnets | |
| JP5023103B2 (ja) | 永久磁石材料 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A711 | Notification of change in applicant |
Free format text: JAPANESE INTERMEDIATE CODE: A711 Effective date: 20050707 |
|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A821 Effective date: 20050707 |
|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20070704 |
|
| A621 | Written request for application examination |
Free format text: JAPANESE INTERMEDIATE CODE: A621 Effective date: 20070810 |
|
| A977 | Report on retrieval |
Free format text: JAPANESE INTERMEDIATE CODE: A971007 Effective date: 20090917 |
|
| A131 | Notification of reasons for refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A131 Effective date: 20090929 |
|
| RD05 | Notification of revocation of power of attorney |
Free format text: JAPANESE INTERMEDIATE CODE: A7425 Effective date: 20091117 |
|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20091127 |
|
| RD03 | Notification of appointment of power of attorney |
Free format text: JAPANESE INTERMEDIATE CODE: A681 Effective date: 20091117 |
|
| RD05 | Notification of revocation of power of attorney |
Free format text: JAPANESE INTERMEDIATE CODE: A7425 Effective date: 20091117 |
|
| A131 | Notification of reasons for refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A131 Effective date: 20100108 |
|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20100203 |
|
| TRDD | Decision of grant or rejection written | ||
| A01 | Written decision to grant a patent or to grant a registration (utility model) |
Free format text: JAPANESE INTERMEDIATE CODE: A01 Effective date: 20100226 |
|
| A01 | Written decision to grant a patent or to grant a registration (utility model) |
Free format text: JAPANESE INTERMEDIATE CODE: A01 |
|
| A61 | First payment of annual fees (during grant procedure) |
Free format text: JAPANESE INTERMEDIATE CODE: A61 Effective date: 20100226 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20130312 Year of fee payment: 3 |
|
| R150 | Certificate of patent or registration of utility model |
Free format text: JAPANESE INTERMEDIATE CODE: R150 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20130312 Year of fee payment: 3 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20140312 Year of fee payment: 4 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| LAPS | Cancellation because of no payment of annual fees |