JP4083912B2 - ケミカルフィルタとその製造方法 - Google Patents

ケミカルフィルタとその製造方法 Download PDF

Info

Publication number
JP4083912B2
JP4083912B2 JP01421899A JP1421899A JP4083912B2 JP 4083912 B2 JP4083912 B2 JP 4083912B2 JP 01421899 A JP01421899 A JP 01421899A JP 1421899 A JP1421899 A JP 1421899A JP 4083912 B2 JP4083912 B2 JP 4083912B2
Authority
JP
Japan
Prior art keywords
adsorbent
filter
adhesive
chemical filter
heat
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP01421899A
Other languages
English (en)
Other versions
JP2000210523A (ja
Inventor
次郎 柴田
健一 堀内
大輔 高祖
和也 林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nitta Corp
Original Assignee
Nitta Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nitta Corp filed Critical Nitta Corp
Priority to JP01421899A priority Critical patent/JP4083912B2/ja
Publication of JP2000210523A publication Critical patent/JP2000210523A/ja
Application granted granted Critical
Publication of JP4083912B2 publication Critical patent/JP4083912B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

【0001】
【発明の属する技術分野】
この発明は、ケミカルフィルタとその製造方法に関するものである。
【0002】
【従来の技術】
ケミカルフィルタとしては、例えば、ウレタン等の発泡体に活性炭等の粒子状の吸着剤を接着して成るものがある。このフィルタは、発泡体に液状の接着剤を塗布させた後、前記接着剤がウエット(WET)状態である間に大量の吸着剤を発泡体に降りそそぐ態様で発泡体に吸着剤を接着させ、その後、熱をかけて接着剤を固めるようにして製造される。
【0003】
しかしながら、このケミカルフィルタでは、図3に示すように基材90に塗布された接着剤91が吸着剤92を広い範囲で覆うものとなり、このため吸着効率が低いという問題があった。このような問題が発生する原因としては、以下の▲1▼〜▲3▼が挙げられる。
▲1▼ウエットの柔らかい接着剤層に吸着剤がめり込んでしまう(めり込み部を符号Aで示す)。
▲2▼液体である接着剤が表面張力により吸着剤表面をより広く覆ってしまう(表面張力により覆われた部分を符号Bで示す)。
▲3▼吸着剤が発泡体内部に到達するまでの間に、吸着剤表面の所々に付着する(付着部を符号Cで示す)。
【0004】
なお、上記吸着効率を向上させる手段として接着剤の量を減少させることが考えられるが、このような手段では吸着剤が発泡体に十分に接着されず、発泡体から吸着剤が脱離してしまうことから好ましくない。
【0005】
したがって、ケミカルフィルタを製造・販売・使用する業界では、フィルタ基材から吸着剤が脱離せず且つ吸着効率が高いケミカルフィルタ及びその製造方法が開発されることを待ち望んでいる。
【0006】
【発明が解決しようとする課題】
そこで、この発明では、フィルタ基材から吸着剤が脱離せず且つ吸着効率が高いケミカルフィルタとその製造方法を提供することを課題とする。
【0007】
【課題を解決するための手段】
(請求項1記載の発明)
この発明のケミカルフィルタは、三次元網状骨格構造を有するフィルタ基材1に、小粒子状の吸着剤2をヒートシール型接着剤3により固着して成る。
(請求項2記載の発明)
この発明のケミカルフィルタは、上記請求項1記載の発明に関して、フィルタ基材1が、発泡体、繊維を絡めて形成した繊維体、ハニカム構造体のうちのいずれかである。
(請求項3記載の発明)
この発明のケミカルフィルタは、上記請求項1又は2記載の発明に関して、フィルタ基材1の表裏面のうち少なくとも一方の形状が凹凸立体構造である。
(請求項4記載の発明)
この発明のケミカルフィルタの製造方法は、三次元網状骨格構造を有するフィルタ基材1にヒートシール型接着剤3を塗布又は含浸させ、このヒートシール型接着剤3を塗布又は含浸させたフィルタ基材1を小粒子状の吸着剤2が入った容器内に埋め込んだ状態で、ヒートシール型接着剤3を加熱し、加熱によって接着性を取り戻したヒートシール型接着剤3により吸着剤2をフィルタ基材1に固着させるようにしてある。
(請求項5記載の発明)
この発明のケミカルフィルタの製造方法は、上記請求項4記載の発明に関して、吸着剤2をフィルタ基材1に圧接させた状態で、ヒートシール型接着剤3を加熱して、吸着剤2をフィルタ基材1に固着させるようにしてある。
(請求項6記載の発明)
この発明のケミカルフィルタの製造方法は、上記請求項4又は5記載の発明に関して、フィルタ基材1の表裏面のうち少なくとも一方の形状が凹凸立体構造である。
(請求項7記載の発明)
この発明のケミカルフィルタの製造方法は、上記請求項4乃至6のいずれかに記載の発明に関して、フィルタ基材1が、発泡体、繊維を絡めて形成した繊維体、ハニカム構造体のうちのいずれかである。
【0008】
なお、このケミカルフィルタ及びその製造方法の機能については、以下の発明の実施の形態の欄で説明する。
【0009】
【発明の実施の形態】
以下、この発明の実施の形態を図面に従って説明する。
【0010】
このケミカルフィルタFは、図1や図2に示すように、三次元網状骨格構造を有するフィルタ基材1に、小粒子状の吸着剤2をヒートシール型接着剤3により固着して構成されている。
【0011】
フィルタ基材1は、図1に示すように、ポリウレタンの発泡体であり、加熱と強風とにより泡を爆破処理して形成されている。
【0012】
吸着剤2は、直径が0.1 〜5mmに設定された活性炭により構成されている。
【0013】
ヒートシール型接着剤3としては、可塑剤を含まないポリ酢酸ビニルエマルジョンにより構成されたものが使用されている。
【0014】
上記ケミカルフィルタFは、以下の第1、第2工程により製造できる。
第1工程
フィルタ基材1にヒートシール型接着剤3を塗布又は含浸させ、その後前記ヒートシール型接着剤3を乾燥させる。
第2工程
ヒートシール型接着剤3が塗布又は含浸された上記フィルタ基材1を、小粒子状の吸着剤2が入った容器内に埋め込み、この状態でヒートシール型接着剤3を加熱する。なお、ヒートシール型接着剤3の加熱時において吸着剤2がフィルタ基材1に押し付けられた状態(加圧状態)であることが好ましい。
【0015】
上記第2工程により、ヒートシール型接着剤3が接着性を取り戻し、前記ヒートシール型接着剤3を介して吸着剤2がフィルタ基材1に固着されることとなるが、ヒートシール型接着剤3は従来の接着剤のようにウエット(WET)になららいため、吸着剤2が大きく接着剤内にめり込むことはなく且つ表面張力も非常に弱く、更に、ヒートシール型接着剤3が乾燥した状態で吸着剤2と接触するので吸着剤2の所々に接着剤が付着するようなこともない。したがって、このケミカルフィルタは、フィルタ基材1から吸着剤2が脱離せず且つ吸着効率が高いものとなる。
【0016】
なお、上記実施形態ではフィルタ基材1をポリウレタンの発泡体により構成したが、他の材料の発泡体、繊維を絡めて形成した繊維体、ハニカム構造体等によりフィルタ基材1を構成するようにしてもよい。
【0017】
また、上記実施形態のフィルタ基材1にかえて、フィルタ基材1の表裏面のうち少なくとも一方の形状が凹凸を有する立体構造であるものとすることができる。
【0018】
他方、上記実施形態では吸着剤2を活性炭としたが、他の種類のもの、例えばイオン交換樹脂、シリカゲル等を採用してもよい。
【0019】
【発明の効果】
この発明は上記のような構成であるから、次の効果を有する。
【0020】
上記した発明の実施形態の欄に記載した内容から、フィルタ基材から吸着剤が脱離せず且つ吸着効率が高いケミカルフィルタとその製造方法を提供できた。
【図面の簡単な説明】
【図1】この発明の実施形態のケミカルフィルタにおけるフィルタ基材の斜視図。
【図2】前記ケミカルフィルタの部分拡大図。
【図3】従来の方法により製造されたケミカルフィルタの部分拡大図。
【符号の説明】
1 フィルタ基材
2 吸着剤
3 ヒートシール型接着剤

Claims (3)

  1. 三次元網状骨格構造を有し、発泡体、又はハニカム構造体であるフィルタ基材(1)にヒートシール型接着剤(3)を塗布又は含浸させて乾燥し、このウエットではないヒートシール型接着剤(3)を塗布又は含浸させたフィルタ基材(1)を小粒子状の吸着剤(2)が入った容器内に埋め込んだ状態で、ヒートシール型接着剤(3)を加熱し、加熱によって接着性を取り戻したヒートシール型接着剤(3)により吸着剤(2)をフィルタ基材(1)に固着させるようにしたことを特徴とするケミカルフィルタの製造方法。
  2. 吸着剤(2)をフィルタ基材(1)に圧接させた状態で、ヒートシール型接着剤(3)を加熱して、吸着剤(2)をフィルタ基材(1)に固着させるようにしたことを特徴とする請求項記載のケミカルフィルタの製造方法。
  3. フィルタ基材(1)の表裏面のうち少なくとも一方の形状が凹凸立体構造であることを特徴とする請求項1又は2記載のケミカルフィルタの製造方法。
JP01421899A 1999-01-22 1999-01-22 ケミカルフィルタとその製造方法 Expired - Fee Related JP4083912B2 (ja)