JP3397904B2 - レーザ加工における金属材料被加工物の前処理方法 - Google Patents
レーザ加工における金属材料被加工物の前処理方法Info
- Publication number
- JP3397904B2 JP3397904B2 JP22287594A JP22287594A JP3397904B2 JP 3397904 B2 JP3397904 B2 JP 3397904B2 JP 22287594 A JP22287594 A JP 22287594A JP 22287594 A JP22287594 A JP 22287594A JP 3397904 B2 JP3397904 B2 JP 3397904B2
- Authority
- JP
- Japan
- Prior art keywords
- coating
- laser
- laser processing
- metal material
- workpiece
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Laser Beam Processing (AREA)
- Physical Vapour Deposition (AREA)
- Chemical Vapour Deposition (AREA)
- Other Surface Treatments For Metallic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22287594A JP3397904B2 (ja) | 1994-09-19 | 1994-09-19 | レーザ加工における金属材料被加工物の前処理方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22287594A JP3397904B2 (ja) | 1994-09-19 | 1994-09-19 | レーザ加工における金属材料被加工物の前処理方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH0885819A JPH0885819A (ja) | 1996-04-02 |
| JPH0885819A5 JPH0885819A5 (enExample) | 1998-10-06 |
| JP3397904B2 true JP3397904B2 (ja) | 2003-04-21 |
Family
ID=16789263
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP22287594A Expired - Fee Related JP3397904B2 (ja) | 1994-09-19 | 1994-09-19 | レーザ加工における金属材料被加工物の前処理方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3397904B2 (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP3643444A1 (en) * | 2018-10-25 | 2020-04-29 | Citic Dicastal Co., Ltd. | Surface laser remelting treatment method for aluminum alloy |
Families Citing this family (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3185869B2 (ja) * | 1997-10-21 | 2001-07-11 | 日本電気株式会社 | レーザ加工方法 |
| US6036873A (en) * | 1997-11-26 | 2000-03-14 | Eastman Kodak Company | Process for generating precision polished non-plannar aspherical surfaces |
| JP4058448B2 (ja) * | 2005-12-26 | 2008-03-12 | 宗春 沓名 | レーザピーニング処理方法及びレーザ吸収粉体層シート |
| JP2007169754A (ja) * | 2005-12-26 | 2007-07-05 | Muneharu Kutsuna | 表面処理方法、レーザ吸収粉体層シート及びレーザピーニング用粉体スプレー |
| WO2020212735A1 (en) | 2019-04-17 | 2020-10-22 | Arcelormittal | A method for the manufacture of an assembly by submerged arc welding (saw) |
| WO2020212737A1 (en) * | 2019-04-17 | 2020-10-22 | Arcelormittal | A method for the manufacture of a coated metallic substrate by laser metal deposition |
| WO2020212736A1 (en) * | 2019-04-17 | 2020-10-22 | Arcelormittal | A method for the manufacture of an assembly by laser welding |
| EP3822712A1 (fr) * | 2019-11-13 | 2021-05-19 | Rolex Sa | Composant pour pièce d'horlogie |
| PL242889B1 (pl) * | 2020-09-12 | 2023-05-08 | Wysokinski Karol | Metoda modyfikowania metali za pomocą lasera |
| CN118951202B (zh) * | 2024-10-14 | 2024-12-27 | 浙江工业大学 | 采用双层结构钎料的玻璃与金属激光焊接方法及其钎料 |
-
1994
- 1994-09-19 JP JP22287594A patent/JP3397904B2/ja not_active Expired - Fee Related
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP3643444A1 (en) * | 2018-10-25 | 2020-04-29 | Citic Dicastal Co., Ltd. | Surface laser remelting treatment method for aluminum alloy |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0885819A (ja) | 1996-04-02 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Ayers et al. | A laser processing technique for improving the wear resistance of metals | |
| CN107532272B (zh) | 基材的表面粗化方法、基材的表面处理方法、喷涂覆膜被覆部件及其制造方法 | |
| Zeng et al. | The formed surface characteristics of SiCf/SiC composite in the nanosecond pulsed laser ablation | |
| CN101421071A (zh) | 制造高质量表面的方法和具有高质量表面的产品 | |
| JPH0885819A (ja) | レーザ加工における被加工物の前処理方法 | |
| Fedorov et al. | Effect of structural and phase transformations in alloyed subsurface layer of hard-alloy tools on their wear resistance during cutting of high-temperature alloys | |
| KR102651664B1 (ko) | 레이저 용접에 의한 조립체의 제조 방법 | |
| JPS59159982A (ja) | 高融点金属の耐熱性化合物の耐摩耗性コ−テイングを有する切削工具およびその製法 | |
| Yilbas et al. | Surface engineering towards self-cleaning applications: laser textured silicon surface | |
| Sure et al. | Surface modification of plasma sprayed Al2O3–40 wt% TiO2 coatings by pulsed Nd: YAG laser melting | |
| Fedorov et al. | Formation of titanium nitride, titanium carbide, and silicon carbide surfaces by high power femtosecond laser treatment | |
| JP2009527359A5 (enExample) | ||
| JP2009527359A (ja) | レーザ蒸散により表面および材料を提供する方法 | |
| Yuan et al. | Study on processing characteristics and mechanisms of thermally assisted laser materials processing | |
| Piatkowski et al. | Simultaneous carburization, oxidation, and nitridation of titanium surface using ablation by femtosecond laser in n‐Heptane | |
| Yuan et al. | Study of laser surface texturing of 6061 aluminium with thermal assistance | |
| Egorova et al. | Hardness enhancement by laser modification of titanium under an auxiliary graphite layer | |
| Meneau et al. | Laser surface modification: structural and tribological studies of AlN coatings | |
| Chang et al. | Effect of femtosecond laser power on the removal mechanism and surface properties of surface paint layer on 7075 aluminium alloy | |
| US20260015710A1 (en) | Superhydrophobic substrates and methods for producing the same | |
| Xue et al. | Laser gas nitriding of Ti-6AI-4V alloy | |
| Aleksandrov et al. | Laser surface alloying of aluminum alloys | |
| Ji et al. | Effect of double laser beam surface treatment on the surface morphological characteristics of Ti6Al4V at different heat source incidence angles | |
| RU2425908C2 (ru) | Способ нанесения покрытия с помощью импульсного лазера и объект с покрытием, нанесенным этим способом | |
| Yamaguchi et al. | Surface alloying of titanium using a nanosecond laser with a light-transmitting resin |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| LAPS | Cancellation because of no payment of annual fees |