JP3224136B2 - 液晶性ポリマーを含有する再成形品の製造方法 - Google Patents
液晶性ポリマーを含有する再成形品の製造方法Info
- Publication number
- JP3224136B2 JP3224136B2 JP25219391A JP25219391A JP3224136B2 JP 3224136 B2 JP3224136 B2 JP 3224136B2 JP 25219391 A JP25219391 A JP 25219391A JP 25219391 A JP25219391 A JP 25219391A JP 3224136 B2 JP3224136 B2 JP 3224136B2
- Authority
- JP
- Japan
- Prior art keywords
- liquid crystal
- resin
- crystalline polymer
- liquid crystalline
- melting point
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Extrusion Moulding Of Plastics Or The Like (AREA)
- Compositions Of Macromolecular Compounds (AREA)
Priority Applications (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP25219391A JP3224136B2 (ja) | 1991-09-30 | 1991-09-30 | 液晶性ポリマーを含有する再成形品の製造方法 |
| EP19920116771 EP0535650A3 (en) | 1991-09-30 | 1992-09-30 | Molding resin composition |
| KR1019920017834A KR960006785B1 (ko) | 1991-09-30 | 1992-09-30 | 성형용 수지조성물 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP25219391A JP3224136B2 (ja) | 1991-09-30 | 1991-09-30 | 液晶性ポリマーを含有する再成形品の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH0586257A JPH0586257A (ja) | 1993-04-06 |
| JPH0586257A5 JPH0586257A5 (enExample) | 1999-08-24 |
| JP3224136B2 true JP3224136B2 (ja) | 2001-10-29 |
Family
ID=17233798
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP25219391A Expired - Fee Related JP3224136B2 (ja) | 1991-09-30 | 1991-09-30 | 液晶性ポリマーを含有する再成形品の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3224136B2 (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100557684B1 (ko) * | 2003-12-23 | 2006-03-07 | 제일모직주식회사 | 내피로 특성이 우수한 폴리카보네이트계 수지 조성물 |
-
1991
- 1991-09-30 JP JP25219391A patent/JP3224136B2/ja not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0586257A (ja) | 1993-04-06 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2838406B2 (ja) | 自己補強性重合体複合物及びその製法 | |
| EP0566149B1 (en) | Molding composite composition and method for preparing the same | |
| KR101685761B1 (ko) | 백색도 및 기계적 물성이 향상된 생분해성 수지 조성물을 이용한 3차원 프린터용 필라멘트 | |
| KR960007471B1 (ko) | 액정수지 복합체의 성형방법 | |
| JP3119508B2 (ja) | 液晶ポリマーを含有する再成形品の製造方法 | |
| JP3217091B2 (ja) | 液晶ポリマーを含有する再成形品 | |
| JP3224137B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JP3217092B2 (ja) | 液晶ポリマーを含有する再成形品 | |
| JP3162124B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JP3124587B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JP3186858B2 (ja) | 液晶樹脂複合体の成形方法 | |
| JP3159741B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JP3115655B2 (ja) | 液晶性ポリマーを含有する再成形品の製造方法 | |
| JP3241404B2 (ja) | 成形用樹脂組成物とその樹脂成形品の製造方法 | |
| KR960006785B1 (ko) | 성형용 수지조성물 | |
| JPH0586257A (ja) | 成形用樹脂組成物 | |
| JP3176131B2 (ja) | 液晶樹脂複合体の再成形方法 | |
| JP3241482B2 (ja) | 成形用複合樹脂組成物及びそれを用いた成形方法 | |
| JPH0586286A5 (enExample) | ||
| JPH0586288A5 (enExample) | ||
| JPH08290428A (ja) | ガラス繊維配合熱可塑性樹脂回収材を用いる成形方法 | |
| CN111647259A (zh) | 一种生物降解的复合电缆及其制备方法 | |
| KR960007276B1 (ko) | 액정수지복합체의 사출성형방법 및 성형물품 | |
| EP0524655B1 (en) | Method for reforming a liquid crystal resin composite | |
| JPH0747546A (ja) | 液晶樹脂複合体成形用素材およびそれを用いる成形方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |