JP3041730B2 - 鉛蓄電池の極板ペーストの製造方法 - Google Patents

鉛蓄電池の極板ペーストの製造方法

Info

Publication number
JP3041730B2
JP3041730B2 JP3201598A JP20159891A JP3041730B2 JP 3041730 B2 JP3041730 B2 JP 3041730B2 JP 3201598 A JP3201598 A JP 3201598A JP 20159891 A JP20159891 A JP 20159891A JP 3041730 B2 JP3041730 B2 JP 3041730B2
Authority
JP
Japan
Prior art keywords
paste
kneading
water
sludge
lead
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP3201598A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0547382A5 (enExample
JPH0547382A (ja
Inventor
一広 岡村
利弘 井上
昭彦 佐野
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Panasonic Corp
Panasonic Holdings Corp
Original Assignee
Panasonic Corp
Matsushita Electric Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Family has litigation
First worldwide family litigation filed litigation Critical https://patents.darts-ip.com/?family=16443710&utm_source=google_patent&utm_medium=platform_link&utm_campaign=public_patent_search&patent=JP3041730(B2) "Global patent litigation dataset” by Darts-ip is licensed under a Creative Commons Attribution 4.0 International License.
Application filed by Panasonic Corp, Matsushita Electric Industrial Co Ltd filed Critical Panasonic Corp
Priority to JP3201598A priority Critical patent/JP3041730B2/ja
Publication of JPH0547382A publication Critical patent/JPH0547382A/ja
Publication of JPH0547382A5 publication Critical patent/JPH0547382A5/ja
Application granted granted Critical
Publication of JP3041730B2 publication Critical patent/JP3041730B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Classifications

    • Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10—Energy storage using batteries

Landscapes

  • Battery Electrode And Active Subsutance (AREA)
JP3201598A 1991-08-12 1991-08-12 鉛蓄電池の極板ペーストの製造方法 Expired - Lifetime JP3041730B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP3201598A JP3041730B2 (ja) 1991-08-12 1991-08-12 鉛蓄電池の極板ペーストの製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP3201598A JP3041730B2 (ja) 1991-08-12 1991-08-12 鉛蓄電池の極板ペーストの製造方法

Publications (3)

Publication Number Publication Date
JPH0547382A JPH0547382A (ja) 1993-02-26
JPH0547382A5 JPH0547382A5 (enExample) 1999-04-23
JP3041730B2 true JP3041730B2 (ja) 2000-05-15

Family

ID=16443710

Family Applications (1)

Application Number Title Priority Date Filing Date
JP3201598A Expired - Lifetime JP3041730B2 (ja) 1991-08-12 1991-08-12 鉛蓄電池の極板ペーストの製造方法

Country Status (1)

Country Link
JP (1) JP3041730B2 (enExample)

Also Published As

Publication number Publication date
JPH0547382A (ja) 1993-02-26

Similar Documents

Publication Publication Date Title
JP2000503467A (ja) 電気化学電池の亜鉛アノード
JP5851491B2 (ja) 鉛蓄電池用正極活性組成物を製造するための添加剤
US2865974A (en) Negative plates and the production thereof
JP3178015B2 (ja) 鉛蓄電池用正極板およびその製造法
EP0834946B1 (en) Valve regulated type lead-acid battery and producing method thereof
JP4186197B2 (ja) 鉛蓄電池用正極板
JPH11126604A (ja) 密閉形鉛蓄電池およびその製造方法
JPH0547382A (ja) 鉛蓄電池の極板ペーストの製造方法
US6027832A (en) Lead acid storage battery and method for producing the same
JP2536251B2 (ja) 鉛蓄電池
JPH11162456A (ja) 鉛蓄電池
JP3186071B2 (ja) 鉛蓄電池用極板及び凝集粒の製造方法
JPS6255273B2 (enExample)
JP2983662B2 (ja) アルカリ蓄電池用ペースト式カドミウム負極の製造方法
JPH0850896A (ja) 鉛蓄電池の製造法
JPH02201872A (ja) 鉛蓄電池用極板
JP2792882B2 (ja) アルカリ蓄電池用非焼結式カドミウム負極及びその製造方法
JP2985232B2 (ja) 鉛電池の製造方法
JPH0799052A (ja) アルカリ蓄電池
JPH06140030A (ja) 密閉形鉛蓄電池
JPS61114471A (ja) クラツド式鉛電池正極板
JP2968813B2 (ja) アルカリ蓄電池用カドミウム負極の製造方法
JP2526741B2 (ja) 鉛蓄電池陽極板用鉛粉および陽極板の製造法
JPH0528997A (ja) 鉛蓄電池の製造方法
JPS6316554A (ja) アルカリ蓄電池用非焼結式カドミウム陰極