JP2536683B2 - 密閉形鉛蓄電池 - Google Patents
密閉形鉛蓄電池Info
- Publication number
- JP2536683B2 JP2536683B2 JP2254595A JP25459590A JP2536683B2 JP 2536683 B2 JP2536683 B2 JP 2536683B2 JP 2254595 A JP2254595 A JP 2254595A JP 25459590 A JP25459590 A JP 25459590A JP 2536683 B2 JP2536683 B2 JP 2536683B2
- Authority
- JP
- Japan
- Prior art keywords
- battery
- sealed lead
- acid battery
- lead acid
- cell
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Description
横方向に積層する構造となっていた。
いるため、充放電に伴う反応熱が放熱しにくく、容量低
下や短寿命化を惹起する惧れがあった。又、各セルを交
互に積層するため、積層誤りを起す可能性もあった。又
外観の変更によってはセル電池の寸法を変更する必要が
あった。
電池であり、従来の電池に比べて充放電時における反応
熱を効率よく放熱するものである。
充放電に伴う反応熱を放熱し易く、容量低下や短寿命化
を防止でき、また各セル交互積層による積層誤りを防止
できる。又、電池外観も従来のように厚くもなく薄くも
ない中間的な大きさとなり、傾斜角度の変更により同一
の単セル積層においても自由にその外観を変える事がで
きる。
態に配列されるように電槽2に収納する。3は電池固定
治具で、セル電池1が固定されている。4は接続体でセ
ル電池1同志を接続している。5は端部セル電池1の端
子である。
電池1が斜め状態に附要数積層されて配列されている。
態の密閉形鉛蓄電池Bとをサイクル寿命試験を行ったと
ころ、第2図の結果が得られた。
池Bは約200サイクルで寿命となったが、本発明の密閉
形鉛蓄電池Aでは、約300サイクルで寿命となり、積層
時における電池の容量低下及び短寿命化を防止できた。
横方向の積層電池に比べ、容量低下や短寿命化を防止で
きた。又、電池外観を、容易に変更できるので、家電製
品などの小型機器製品の要求に対して十分に応じられる
ようとなる等工業的価値甚だ大なるものである。
発明の密閉形鉛蓄電池と従来の密閉形鉛蓄電池のサイク
ル寿命試験結果を示す曲線図である。 1はセル電池、2は電槽、3は電池固定具、4は接続体
Claims (1)
- 【請求項1】陰極板と陽極板とを隔離体を介して所要数
積層した極板群を有するセル電池を所要数同一斜方向に
電槽に収納して同一斜方向にあるセル電池間を接続する
ことにより積層電池とすることを特徴とする密閉形鉛蓄
電池。