JP2019218606A5 - - Google Patents

Download PDF

Info

Publication number
JP2019218606A5
JP2019218606A5 JP2018117053A JP2018117053A JP2019218606A5 JP 2019218606 A5 JP2019218606 A5 JP 2019218606A5 JP 2018117053 A JP2018117053 A JP 2018117053A JP 2018117053 A JP2018117053 A JP 2018117053A JP 2019218606 A5 JP2019218606 A5 JP 2019218606A5
Authority
JP
Japan
Prior art keywords
lubricating
self
powder
metal
carbide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2018117053A
Other languages
English (en)
Japanese (ja)
Other versions
JP7297279B2 (ja
JP2019218606A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2018117053A priority Critical patent/JP7297279B2/ja
Priority claimed from JP2018117053A external-priority patent/JP7297279B2/ja
Publication of JP2019218606A publication Critical patent/JP2019218606A/ja
Publication of JP2019218606A5 publication Critical patent/JP2019218606A5/ja
Application granted granted Critical
Publication of JP7297279B2 publication Critical patent/JP7297279B2/ja
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

JP2018117053A 2018-06-20 2018-06-20 肉盛層、肉盛層を有する機械部品、及び肉盛層の形成方法 Active JP7297279B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2018117053A JP7297279B2 (ja) 2018-06-20 2018-06-20 肉盛層、肉盛層を有する機械部品、及び肉盛層の形成方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2018117053A JP7297279B2 (ja) 2018-06-20 2018-06-20 肉盛層、肉盛層を有する機械部品、及び肉盛層の形成方法

Publications (3)

Publication Number Publication Date
JP2019218606A JP2019218606A (ja) 2019-12-26
JP2019218606A5 true JP2019218606A5 (enExample) 2021-08-12
JP7297279B2 JP7297279B2 (ja) 2023-06-26

Family

ID=69095588

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2018117053A Active JP7297279B2 (ja) 2018-06-20 2018-06-20 肉盛層、肉盛層を有する機械部品、及び肉盛層の形成方法

Country Status (1)

Country Link
JP (1) JP7297279B2 (enExample)

Families Citing this family (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN112410644A (zh) * 2020-10-19 2021-02-26 扬州千裕电气有限公司 一种金属复合材料及其制备方法
CN113445047B (zh) * 2021-05-31 2023-04-14 沈阳理工大学 一种包含细晶钨与二硫化钨的自润滑涂层的电火花沉积制备方法
CN114457301B (zh) * 2021-06-28 2022-12-30 北京机科国创轻量化科学研究院有限公司 一种高速钢自润滑涂层及其制备方法
CN114293133B (zh) * 2021-12-31 2022-11-04 西安交通大学 一种宽温域自润滑涂层的喷涂材料、制备方法、及其应用
DE102022204689A1 (de) * 2022-05-13 2023-11-16 ADMOS Gleitlager GmbH Verfahren zur Herstellung eines Getriebeelements mit einer als Gleitlager fungierenden Oberfläche
CN115780794B (zh) * 2022-10-26 2024-08-06 合肥工业大学 一种低成本细晶粒自润滑合金材料及其制备方法
JP7540105B1 (ja) 2023-02-07 2024-08-26 住友化学株式会社 プロピレン樹脂組成物及び成形体
JP7466742B1 (ja) 2023-05-29 2024-04-12 住友化学株式会社 プロピレン系樹脂組成物
CN117107185A (zh) * 2023-08-11 2023-11-24 中国第一汽车股份有限公司 一种抗氢脆、自润滑的车用轴瓦涂层及制备方法

Family Cites Families (12)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH06264079A (ja) * 1993-03-10 1994-09-20 Nippon Carbon Co Ltd 摺動材料並びにその製造方法
JPH08332562A (ja) * 1995-06-08 1996-12-17 Toyota Motor Corp 摺動用部材の製造方法
JPH10204569A (ja) * 1997-01-16 1998-08-04 Ofic Co 自己潤滑複合材及びそれを用いた複合表面処理方法
JPH11347787A (ja) * 1998-06-08 1999-12-21 Ofic Co Ni−C系溶接材料
JP2000170924A (ja) 1998-12-01 2000-06-23 Eagle Ind Co Ltd 摺動材
JP4179740B2 (ja) 2000-08-31 2008-11-12 株式会社クボタ 耐食性・耐摩耗性に優れた排水用ポンプの羽根軸の摺動部材
DE60332705D1 (de) 2002-01-18 2010-07-08 Riken Kk Kolbenring mit spritzbeschichtung
JP2007016262A (ja) 2005-07-06 2007-01-25 Nissan Motor Co Ltd カーボンナノチューブ含有複合材及びその製造方法
DE102005059544A1 (de) 2005-12-13 2007-06-14 Ecka Granulate Gmbh & Co. Kg Sn-haltige hochbelastbare Materialzusammensetzung; Verfahren zur Herstellung einer hochbelastbaren Beschichtung und deren Verwendung
JP4860320B2 (ja) 2006-03-30 2012-01-25 株式会社小松製作所 耐摩耗粒子及び耐摩耗構造部材
US9272358B2 (en) 2012-07-19 2016-03-01 Lincoln Global, Inc. Hot-wire consumable to provide self-lubricating weld or clad
CN104278268B (zh) 2013-07-10 2018-04-20 上海宝钢工业技术服务有限公司 锌锅辊轴套和衬套保护涂层的制备方法

Similar Documents

Publication Publication Date Title
JP2019218606A5 (enExample)
JP6675370B2 (ja) 肉盛合金および肉盛部材
Nurminen et al. Microstructure and properties of hard and wear resistant MMC coatings deposited by laser cladding
Fan et al. Microstructure change caused by (Cr, Fe) 23C6 carbides in high chromium Fe–Cr–C hardfacing alloys
CN107151751B (zh) 耐磨性铜基合金
Mokgalaka et al. NiTi Intermetallic Surface Coatings by Laser Metal Deposition for Improving Wear Properties of Ti‐6Al‐4V Substrates
JP7297279B2 (ja) 肉盛層、肉盛層を有する機械部品、及び肉盛層の形成方法
US11717889B2 (en) Multi-metallic articles of manufacture
JP7018603B2 (ja) クラッド層の製造方法
Ferreira et al. Microstructure and properties of nickel-based C276 alloy coatings by PTA on AISI 316L and API 5L X70 steel substrates
US20170284466A1 (en) Plain bearing or part thereof, method for producing same and use of a cucrzr alloy as a plain bearing material
Günther et al. Influence of processing conditions on the degradation kinetics of fused tungsten carbides in hardfacing
US20050142026A1 (en) Ductile cobalt-based Laves phase alloys
US3340049A (en) Copper base alloy
JP7168331B2 (ja) 銅基合金
D'Oliveira et al. Coatings enrichment by carbide dissolution
RU2542922C2 (ru) Порошковая композиционная смесь для лазерной наплавки на металлическую подложку
WO2019189532A1 (ja) 耐摩耗性部品
JP2005305449A (ja) 熱間加工用工具
CN113195759B (zh) 耐腐蚀和耐磨镍基合金
Bober Composite coatings deposited by plasma transfer–characteristics and formation
Uluköy Pulsed metall inert gas (MIG) welding and its effects on the microstructure and element distribution of an aluminum matrix reinforced with SiC composite material: Die Auswirkung von Metallinertgas (MIG)‐Impulsschweißen auf die Mikrostruktur und die Elementverteilung eines Verbundwerkstoffs aus mit SiC verstärktem Aluminium
JP6474887B2 (ja) シリンダロッド
JPH0813116A (ja) 金属部品の表面処理方法
Fauchais et al. Plasma-transferred arc