JP2018092139A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2018092139A5 JP2018092139A5 JP2017202917A JP2017202917A JP2018092139A5 JP 2018092139 A5 JP2018092139 A5 JP 2018092139A5 JP 2017202917 A JP2017202917 A JP 2017202917A JP 2017202917 A JP2017202917 A JP 2017202917A JP 2018092139 A5 JP2018092139 A5 JP 2018092139A5
- Authority
- JP
- Japan
- Prior art keywords
- toner
- particles
- fine particles
- resin
- toner according
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Description
本発明は、トナー粒子を有するトナーであって、
該トナー粒子が、
結着樹脂を含有するトナー母粒子、及び、
該トナー母粒子の表面に形成された、樹脂Aを含有する被覆層を有し、
該樹脂Aの弾性率Ea及び該結着樹脂の弾性率Ebが、下記式を満たし、
0.5≦(Ea/Eb)×100[%] ≦ 50.0
該トナー粒子にカンチレバーの先端に球状SiO2が付いたプローブを3μNで押し込んだ際の該トナー粒子の付着力ATが、500nN以上であることを特徴とするトナーに関する。
The present invention is a toner having toner particles.
The toner particles,
Toner mother particles containing a binder resin and
It has a coating layer containing resin A formed on the surface of the toner matrix particles , and has a coating layer containing resin A.
The elastic modulus Ea of the resin A and the elastic modulus Eb of the binder resin satisfy the following formulas.
0.5 ≤ (Ea / Eb) x 100 [%] ≤ 50.0
The present invention relates to a toner characterized in that the adhesive force AT of the toner particles when a probe having a spherical SiO 2 attached to the tip of a cantilever is pushed into the toner particles with 3 μN is 500 nN or more.
Claims (7)
該トナー粒子が、
結着樹脂を含有するトナー母粒子、及び、
該トナー母粒子の表面に形成された、樹脂Aを含有する被覆層を有し、
該樹脂Aの弾性率Ea及び該結着樹脂の弾性率Ebが、下記式を満たし、
0.5≦(Ea/Eb)×100[%]≦50.0
該トナー粒子にカンチレバーの先端に球状SiO2が付いたプローブを3μNで押し込んだ際の該トナー粒子の付着力ATが、500nN以上である
ことを特徴とするトナー。 A toner having a preparative toner particles,
The toner particles,
Toner mother particles containing a binder resin and
It has a coating layer containing resin A formed on the surface of the toner matrix particles , and has a coating layer containing resin A.
The elastic modulus Ea of the resin A and the elastic modulus Eb of the binder resin satisfy the following formulas.
0.5 ≤ (Ea / Eb) x 100 [%] ≤ 50.0
A toner characterized in that the adhesive force AT of the toner particles when a probe having a spherical SiO 2 attached to the tip of a cantilever is pushed into the toner particles with 3 μN is 500 nN or more.
前記トナー粒子の表面に微粒子が存在し、
該微粒子が、下記の規定(i)及び(ii)を満たす
請求項1〜3のいずれか1項に記載のトナー。
(i)該微粒子の個数平均粒子径が0.090μm以上である。
(ii)該微粒子による前記トナー粒子に対する被覆率C(%)が下記式(1)を満たす。
(式(1)中、DTは前記トナー粒子の個数平均粒子径(D1)(μm)を表し、DEは該微粒子の個数平均粒子径(D1)(μm)を表す。) The AT is 600 nN or more,
Fine particles are present on the surface of the previous Symbol toner particles,
The toner according to any one of claims 1 to 3 , wherein the fine particles satisfy the following provisions ( i) and ( ii).
( I) The number average particle diameter of the fine particles is 0.090 μm or more .
( Ii) The coverage C (%) of the fine particles on the toner particles satisfies the following formula (1) .
(In the formula (1), DT represents the number average particle diameter (D1) (μm) of the toner particles, and DE represents the number average particle diameter (D1) (μm) of the fine particles.)
、相対湿度80%の環境下に1時間放置した際、前記微粒子の質量変化率を、前記微粒子の比表面積で除した値(質量変化率/比表面積)が、0.055%・g/mWhen left for 1 hour in an environment with a relative humidity of 80%, the value obtained by dividing the mass change rate of the fine particles by the specific surface area of the fine particles (mass change rate / specific surface area) is 0.055% · g / m. 22 以下である請求項4に記載のトナー。The toner according to claim 4, which is as follows.