JP2014503693A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2014503693A5 JP2014503693A5 JP2013548891A JP2013548891A JP2014503693A5 JP 2014503693 A5 JP2014503693 A5 JP 2014503693A5 JP 2013548891 A JP2013548891 A JP 2013548891A JP 2013548891 A JP2013548891 A JP 2013548891A JP 2014503693 A5 JP2014503693 A5 JP 2014503693A5
- Authority
- JP
- Japan
- Prior art keywords
- metal object
- anodizing
- voltage
- metal
- anodization
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 238000000034 method Methods 0.000 claims 17
- 239000002184 metal Substances 0.000 claims 13
- 238000007743 anodising Methods 0.000 claims 9
- 238000002048 anodisation reaction Methods 0.000 claims 6
- 238000005259 measurement Methods 0.000 claims 5
- 239000002344 surface layer Substances 0.000 claims 5
- 239000003899 bactericide agent Substances 0.000 claims 4
- 239000003792 electrolyte Substances 0.000 claims 4
- 239000007769 metal material Substances 0.000 claims 2
- 230000003647 oxidation Effects 0.000 claims 2
- 238000007254 oxidation reaction Methods 0.000 claims 2
- 239000003638 chemical reducing agent Substances 0.000 claims 1
- 230000001419 dependent effect Effects 0.000 claims 1
- 229910044991 metal oxide Inorganic materials 0.000 claims 1
- 150000004706 metal oxides Chemical class 0.000 claims 1
- 229910001463 metal phosphate Inorganic materials 0.000 claims 1
- 238000012544 monitoring process Methods 0.000 claims 1
- 238000006722 reduction reaction Methods 0.000 claims 1
Applications Claiming Priority (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| GBGB1100605.3A GB201100605D0 (en) | 2011-01-14 | 2011-01-14 | Metal treatment |
| GB1100605.3 | 2011-01-14 | ||
| GBGB1106733.7A GB201106733D0 (en) | 2011-04-21 | 2011-04-21 | Metal treatment |
| GB1106733.7 | 2011-04-21 | ||
| PCT/GB2012/050068 WO2012095672A2 (en) | 2011-01-14 | 2012-01-13 | Metal treatment |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2014503693A JP2014503693A (ja) | 2014-02-13 |
| JP2014503693A5 true JP2014503693A5 (enExample) | 2015-02-26 |
| JP6130301B2 JP6130301B2 (ja) | 2017-05-17 |
Family
ID=45531884
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2013548891A Active JP6130301B2 (ja) | 2011-01-14 | 2012-01-13 | 金属処理 |
Country Status (4)
| Country | Link |
|---|---|
| US (1) | US9809894B2 (enExample) |
| EP (1) | EP2663671B1 (enExample) |
| JP (1) | JP6130301B2 (enExample) |
| WO (1) | WO2012095672A2 (enExample) |
Families Citing this family (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP5536287B1 (ja) * | 2012-08-06 | 2014-07-02 | 三菱レイヨン株式会社 | モールドの製造方法、および微細凹凸構造を表面に有する成形体の製造方法 |
| GB201508385D0 (en) * | 2015-05-15 | 2015-07-01 | Accentus Medical Ltd | Metal treatment |
| EP3981444A1 (en) | 2017-03-30 | 2022-04-13 | Biomet Manufacturing, LLC | Methods of modifying the porous surface of implants |
| KR102048707B1 (ko) * | 2017-09-29 | 2019-11-27 | (주)알루코 | Al-Mg-Zn 합금 고광택 아노다이징 공법 |
| US11230786B2 (en) * | 2019-06-17 | 2022-01-25 | Nanopec, Inc. | Nano-porous anodic aluminum oxide membrane for healthcare and biotechnology |
| EP4054333A4 (en) | 2019-12-10 | 2024-01-10 | A3 Surface Inc. | ANODIZED BIOCIDAL METAL MATERIAL, METHOD FOR MANUFACTURING THE MATERIAL AND METHOD FOR REACTIVATING THE MATERIAL |
| CA3183538A1 (en) | 2020-07-02 | 2022-01-06 | Mary K. CANTY | Method for optimizing treatment of infected metallic implants by measuring charge transfer |
| EP4397327A4 (en) | 2021-08-31 | 2025-08-13 | Maruemu Works Co Ltd | BIOCOMPATIBLE FILM AND BIOCOMPATIBLE MATERIAL HAVING SAID FILM |
| WO2024089448A1 (en) * | 2022-10-25 | 2024-05-02 | Ecospec Noveltech Pte Ltd | System and method for in-situ formation of barrier coating on metallic article in contact with or exposed to water within a water system |
Family Cites Families (12)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4487666A (en) * | 1984-03-30 | 1984-12-11 | Sprague Electric Company | Electrolytically forming a lot of valve-metal-bodies for use in capacitors |
| JPH0432577A (ja) * | 1990-05-25 | 1992-02-04 | Kobe Steel Ltd | 塗膜密着性及び耐食性に優れた塗装AlまたはAl合金材 |
| JP3335757B2 (ja) * | 1994-03-17 | 2002-10-21 | 株式会社半導体エネルギー研究所 | 陽極酸化方法 |
| JP2000282294A (ja) * | 1999-03-31 | 2000-10-10 | Kobe Steel Ltd | 耐熱割れ性および腐食性に優れた陽極酸化皮膜の形成方法並びに陽極酸化皮膜被覆部材 |
| US20040050709A1 (en) * | 2002-09-17 | 2004-03-18 | The Boeing Company | Accelerated sulfuric acid and boric sulfuric acid anodize process |
| US7033466B2 (en) * | 2002-09-27 | 2006-04-25 | United Technologies Corporation | Electrochemical stripping using single loop control |
| US20050045482A1 (en) * | 2003-08-25 | 2005-03-03 | Storms Edmund K. | Electrolytic heat source |
| JP2005287985A (ja) * | 2004-04-05 | 2005-10-20 | Gha:Kk | 炎症/臭い抑制部材及びその製造方法並びにこれを用いた義体及びギブス |
| US20090292346A1 (en) * | 2005-03-31 | 2009-11-26 | St. Jude Medical Ab | Porous Niobium Oxide as Electrode Material and Manufacturing Process |
| DE102007026086B4 (de) * | 2007-06-04 | 2009-03-05 | Fraunhofer-Gesellschaft zur Förderung der angewandten Forschung e.V. | Verfahren zur Ausbildung einer dielektrischen Dünnschicht auf einem Titansubstrat, mit dem Verfahren hergestelltes Titansubstrat mit Dünnschicht sowie seine Verwendung |
| AU2008306596B2 (en) * | 2007-10-03 | 2013-04-04 | Accentus Plc | Method of manufacturing metal with biocidal properties |
| CN102449207B (zh) * | 2009-03-30 | 2015-05-27 | 阿山特斯医疗有限公司 | 金属处理 |
-
2012
- 2012-01-13 EP EP12701260.7A patent/EP2663671B1/en active Active
- 2012-01-13 JP JP2013548891A patent/JP6130301B2/ja active Active
- 2012-01-13 US US13/979,459 patent/US9809894B2/en active Active
- 2012-01-13 WO PCT/GB2012/050068 patent/WO2012095672A2/en not_active Ceased
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2014503693A5 (enExample) | ||
| JP2012522135A5 (enExample) | ||
| Çapraz et al. | Factors controlling stress generation during the initial growth of porous anodic aluminum oxide | |
| JP2013506304A5 (enExample) | ||
| TW201339370A (zh) | 金屬工件之陽極氧化染色方法 | |
| JP2012522136A5 (enExample) | ||
| JP2014060231A (ja) | 固体電解コンデンサの製造方法 | |
| CN107904644A (zh) | 一种制备金属钨表面纳米多孔活性层的方法 | |
| JP2016145383A5 (enExample) | ||
| CN109632916A (zh) | 一种测定增材制造钛合金表面钝化膜稳定性的方法 | |
| WO2012095672A3 (en) | Metal treatment | |
| CN101798702A (zh) | 一种钛及钛合金电化学抛光的电解液及其表面抛光方法 | |
| Kim et al. | Superhydrophobic nanostructures based on porous alumina | |
| Mohsen et al. | Improvement in corrosion resistance of commercial pure titanium for the enhancement of its biocompatibility | |
| Kollender et al. | Direct observation of metal dissolution during anodization of niobium | |
| SG11201804099RA (en) | Electrochemical measurement method, electrochemical measurement device and transducer | |
| Nguyen et al. | Formation behavior of nanoporous anodic aluminum oxide films in hot glycerol/phosphate electrolyte | |
| Metikoš-Huković et al. | EIS-in situ characterization of anodic films on antimony and lead–antimony alloys | |
| Rodrigues et al. | Voltammetric and ellipsometric studies of films formed on 304 stainless steel in sulphuric acid solution without and with benzotriazole | |
| JP2015520646A5 (enExample) | ||
| JP2009299188A5 (enExample) | ||
| KR101565523B1 (ko) | 고내식성 아노다이징 표면처리방법 | |
| RO130771A2 (ro) | Procedeu de îmbunătăţire a aderenţei filmelor de polipirol prin ancore de polimeri bio-inspiraţi de tip polidopamină | |
| Mišković et al. | Influence of fluoride concentration and pH value on the corrosion behaviour of iron | |
| KR101291310B1 (ko) | 알루미늄 산화물 박막이 부착된 금속 전극을 이용한 미생물 측정 방법 |