JP2011219874A - 化粧板用原紙の製造方法 - Google Patents

化粧板用原紙の製造方法 Download PDF

Info

Publication number
JP2011219874A
JP2011219874A JP2010086468A JP2010086468A JP2011219874A JP 2011219874 A JP2011219874 A JP 2011219874A JP 2010086468 A JP2010086468 A JP 2010086468A JP 2010086468 A JP2010086468 A JP 2010086468A JP 2011219874 A JP2011219874 A JP 2011219874A
Authority
JP
Japan
Prior art keywords
wet paper
wet
strength agent
paper strength
paper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2010086468A
Other languages
English (en)
Japanese (ja)
Other versions
JP2011219874A5 (enExample
Inventor
Yuki Tamagawa
祐基 玉川
Yoshiyuki Terajima
良幸 寺島
Masahiko Shibuya
昌彦 渋谷
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kohjin Holdings Co Ltd
Kohjin Co
Original Assignee
Kohjin Holdings Co Ltd
Kohjin Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kohjin Holdings Co Ltd, Kohjin Co filed Critical Kohjin Holdings Co Ltd
Priority to JP2010086468A priority Critical patent/JP2011219874A/ja
Publication of JP2011219874A publication Critical patent/JP2011219874A/ja
Publication of JP2011219874A5 publication Critical patent/JP2011219874A5/ja
Pending legal-status Critical Current

Links

Landscapes

  • Paper (AREA)
JP2010086468A 2010-04-02 2010-04-02 化粧板用原紙の製造方法 Pending JP2011219874A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2010086468A JP2011219874A (ja) 2010-04-02 2010-04-02 化粧板用原紙の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2010086468A JP2011219874A (ja) 2010-04-02 2010-04-02 化粧板用原紙の製造方法

Publications (2)

Publication Number Publication Date
JP2011219874A true JP2011219874A (ja) 2011-11-04
JP2011219874A5 JP2011219874A5 (enExample) 2012-02-09

Family

ID=45037198

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2010086468A Pending JP2011219874A (ja) 2010-04-02 2010-04-02 化粧板用原紙の製造方法

Country Status (1)

Country Link
JP (1) JP2011219874A (enExample)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103866639A (zh) * 2014-02-28 2014-06-18 苏州恒康新材料有限公司 一种用于造纸的湿强剂及其制备方法
JP2015059292A (ja) * 2013-09-20 2015-03-30 王子ホールディングス株式会社 化粧板原紙
CN105507076A (zh) * 2014-09-22 2016-04-20 丹阳市华兴纸箱有限公司 一种湿强剂及其制备工艺
CN105887552A (zh) * 2014-12-01 2016-08-24 富阳市金枫纸业有限公司 一种起皱的彩色牙科纸围巾用纸的制造方法
CN106968118A (zh) * 2017-03-09 2017-07-21 河南林泉环保科技有限公司 一种废纸制造的育果袋纸及其零排放生产方法
JP2017172077A (ja) * 2016-03-24 2017-09-28 北越紀州製紙株式会社 紙の製造方法
WO2019143519A1 (en) 2018-01-16 2019-07-25 Solenis Technologies, L.P. Process for making paper with improved filler retention and opacity while maintaining wet tensile strength

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2015059292A (ja) * 2013-09-20 2015-03-30 王子ホールディングス株式会社 化粧板原紙
CN103866639A (zh) * 2014-02-28 2014-06-18 苏州恒康新材料有限公司 一种用于造纸的湿强剂及其制备方法
CN105507076A (zh) * 2014-09-22 2016-04-20 丹阳市华兴纸箱有限公司 一种湿强剂及其制备工艺
CN105887552A (zh) * 2014-12-01 2016-08-24 富阳市金枫纸业有限公司 一种起皱的彩色牙科纸围巾用纸的制造方法
JP2017172077A (ja) * 2016-03-24 2017-09-28 北越紀州製紙株式会社 紙の製造方法
CN106968118A (zh) * 2017-03-09 2017-07-21 河南林泉环保科技有限公司 一种废纸制造的育果袋纸及其零排放生产方法
WO2019143519A1 (en) 2018-01-16 2019-07-25 Solenis Technologies, L.P. Process for making paper with improved filler retention and opacity while maintaining wet tensile strength
US10975524B2 (en) 2018-01-16 2021-04-13 Solenis Technologies, L.P. Process for making paper with improved filler retention and opacity while maintaining wet tensile strength

Similar Documents

Publication Publication Date Title
EP3071751B1 (en) Method for increasing paper strength
JP2011219874A (ja) 化粧板用原紙の製造方法
EP3768892B1 (en) Method for manufacturing a multi-layered paperboard, multi-layered paperboard and composition for use in multi-layered paperboard manufacturing
FI121121B (fi) Vesipitoisia alkyylidiketeenidispersioita ja niiden käyttö paperin liima-aineena
CA3038853C (en) A method for increasing dimensional stability of a paper or a board product
WO2021074879A1 (en) Mfc composition with phosphorylated cellulose fibers
KR20070112162A (ko) 종이 제조에 사용하기 위한 첨가제계 및 그의 사용방법
US8118976B2 (en) Process for the production of a cellulosic product
NZ230427A (en) Process for dewatering cellulose pulp on a wire
FI3899136T3 (fi) Prosessi paperin tai pahvin tuottamiseksi ja sen tuote
JP6176918B2 (ja) 包装材
CN113661290A (zh) 使用金属螯合物和合成阳离子聚合物提高纸强度
US20030127210A1 (en) Sizing paper by wet-end addition of water dispersibility polyester
CN103384742A (zh) 生产纸制品的方法
JP6791067B2 (ja) 熱転写紙用原紙および熱転写紙
Bhardwaj et al. Chitosan as wet-end additive for papermaking using mixed hardwood pulp
EP3458646B1 (en) Treatment system for making of paper
JP2021195663A (ja) 紙の製造方法
JP4268583B2 (ja) 中性新聞印刷用紙の製造方法
AU761790B2 (en) Silica-acid colloid blend in a microparticle system used in papermaking
EP2239370B1 (en) Dry and wet strength improvement of paper products with cationic tannin
KR0181507B1 (ko) 내유지 및 그의 제조 방법
WO2018060002A1 (en) A method for increasing dimensional stability of a paper or a board product
JP6189026B2 (ja) 印刷用紙
JP6927403B1 (ja) 紙の製造方法

Legal Events

Date Code Title Description
A711 Notification of change in applicant

Free format text: JAPANESE INTERMEDIATE CODE: A712

Effective date: 20110930

A521 Written amendment

Free format text: JAPANESE INTERMEDIATE CODE: A523

Effective date: 20111214