JP2008169494A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2008169494A5 JP2008169494A5 JP2007001703A JP2007001703A JP2008169494A5 JP 2008169494 A5 JP2008169494 A5 JP 2008169494A5 JP 2007001703 A JP2007001703 A JP 2007001703A JP 2007001703 A JP2007001703 A JP 2007001703A JP 2008169494 A5 JP2008169494 A5 JP 2008169494A5
- Authority
- JP
- Japan
- Prior art keywords
- fabric
- heating
- producing
- carbonized
- temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 239000004744 fabric Substances 0.000 claims 15
- 238000010438 heat treatment Methods 0.000 claims 8
- 239000000835 fiber Substances 0.000 claims 7
- 238000004519 manufacturing process Methods 0.000 claims 6
- 230000001590 oxidative effect Effects 0.000 claims 4
- QVGXLLKOCUKJST-UHFFFAOYSA-N atomic oxygen Chemical compound [O] QVGXLLKOCUKJST-UHFFFAOYSA-N 0.000 claims 3
- 239000001301 oxygen Substances 0.000 claims 3
- 229910052760 oxygen Inorganic materials 0.000 claims 3
- 238000003763 carbonization Methods 0.000 claims 1
- 239000007789 gas Substances 0.000 claims 1
- 239000002994 raw material Substances 0.000 claims 1
- 230000000452 restraining effect Effects 0.000 claims 1
- 238000005979 thermal decomposition reaction Methods 0.000 claims 1
- 239000002759 woven fabric Substances 0.000 claims 1
Priority Applications (3)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2007001703A JP4392434B2 (ja) | 2007-01-09 | 2007-01-09 | 炭素化布帛の製造方法 |
CNA2007800495229A CN101578406A (zh) | 2007-01-09 | 2007-12-28 | 碳化布的制造方法以及由其制得的碳化布 |
PCT/JP2007/075259 WO2008084734A1 (ja) | 2007-01-09 | 2007-12-28 | 炭素化布帛の製造方法およびこれにより得られた炭素化布帛 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2007001703A JP4392434B2 (ja) | 2007-01-09 | 2007-01-09 | 炭素化布帛の製造方法 |
Publications (3)
Publication Number | Publication Date |
---|---|
JP2008169494A JP2008169494A (ja) | 2008-07-24 |
JP2008169494A5 true JP2008169494A5 (enrdf_load_stackoverflow) | 2009-08-06 |
JP4392434B2 JP4392434B2 (ja) | 2010-01-06 |
Family
ID=39608628
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2007001703A Expired - Fee Related JP4392434B2 (ja) | 2007-01-09 | 2007-01-09 | 炭素化布帛の製造方法 |
Country Status (3)
Country | Link |
---|---|
JP (1) | JP4392434B2 (enrdf_load_stackoverflow) |
CN (1) | CN101578406A (enrdf_load_stackoverflow) |
WO (1) | WO2008084734A1 (enrdf_load_stackoverflow) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP4936478B2 (ja) * | 2009-01-14 | 2012-05-23 | 前田 俊克 | 炭素化布帛の製造方法及び炭素化布帛 |
JP6217040B2 (ja) * | 2013-09-05 | 2017-10-25 | 道宇 可児 | 炭化布製造方法 |
KR101565132B1 (ko) | 2015-03-26 | 2015-11-02 | 주식회사 시나프 | 탄화 면직물의 제조공정 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2001234435A (ja) * | 2000-02-25 | 2001-08-31 | Tokai Senko Kk | 炭化セルロース系繊維及び活性炭化セルロース系繊維の連続製造方法及び装置 |
JP2006016699A (ja) * | 2004-06-30 | 2006-01-19 | Le Vert:Kk | 繊維炭及びその製造方法 |
-
2007
- 2007-01-09 JP JP2007001703A patent/JP4392434B2/ja not_active Expired - Fee Related
- 2007-12-28 CN CNA2007800495229A patent/CN101578406A/zh active Pending
- 2007-12-28 WO PCT/JP2007/075259 patent/WO2008084734A1/ja active Application Filing
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP2008169492A5 (enrdf_load_stackoverflow) | ||
WO2008084732A1 (ja) | 炭素化布帛の製造方法およびこれにより得られた炭素化布帛 | |
JP2016505481A5 (enrdf_load_stackoverflow) | ||
JP2018500480A5 (enrdf_load_stackoverflow) | ||
WO2008086475A3 (en) | Wound dressing with controllable permeability | |
CN105683428A (zh) | 活性炭纤维及其制备方法 | |
JP2008169494A5 (enrdf_load_stackoverflow) | ||
WO2013183668A1 (ja) | 触媒を用いた炭素材料の製造方法および炭素材料 | |
CN107215870A (zh) | 一种制备活性炭的方法 | |
WO2008084730A1 (ja) | 炭素化布帛の製造方法およびこれにより得られた炭素化布帛 | |
KR101005115B1 (ko) | 표면에 그라파이트 나노 구조층을 갖는 셀룰로오스 탄화물 구조체의 합성방법 | |
JP2008169493A5 (enrdf_load_stackoverflow) | ||
WO2008084734A1 (ja) | 炭素化布帛の製造方法およびこれにより得られた炭素化布帛 | |
JP4355344B2 (ja) | 炭素化布帛の製造方法およびこれにより得られた炭素化布帛 | |
WO2008084733A1 (ja) | 炭素化布帛の製造方法およびこれにより得られた炭素化布帛 | |
JP2017178635A (ja) | 炭素材料の製造方法 | |
KR20150004309A (ko) | 탄화 폴리에스테르 부직포에 흑연유사구조(석탄화도: 94이상)의 한국산무연탄계분말활성탄(SBET=1,760m2/g이상의 고비표면적)을 퀴놀린가용성 등방성피치바인더에 의해 첨착, 재 탄화를 통해, 새로운 열안정성 흡착필터"a novel thermostable adsorption filter"의 제조방법 | |
KR101456261B1 (ko) | 천연섬유계 탄소 섬유 및 그 제조방법 | |
JP2017020142A5 (ja) | 炭素繊維の製造方法 | |
JO2988B1 (ar) | عمليه لإنتاج الإسمنت أو بدائل له | |
JP2008169495A5 (enrdf_load_stackoverflow) | ||
CN102431995A (zh) | 一种基于煤中精煤族组分制备泡沫炭的方法 | |
JP2012255235A5 (enrdf_load_stackoverflow) | ||
RU2012130021A (ru) | Способ получения активных углей из шихт коксохимического производства | |
JP4392435B2 (ja) | 炭素化布帛の製造方法 |