JP2005076074A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2005076074A5 JP2005076074A5 JP2003306966A JP2003306966A JP2005076074A5 JP 2005076074 A5 JP2005076074 A5 JP 2005076074A5 JP 2003306966 A JP2003306966 A JP 2003306966A JP 2003306966 A JP2003306966 A JP 2003306966A JP 2005076074 A5 JP2005076074 A5 JP 2005076074A5
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (3)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2003306966A JP4276031B2 (ja) | 2003-08-29 | 2003-08-29 | チタン化合物被覆ニッケル粉末およびこれを用いた導電ペースト |
PCT/JP2004/010799 WO2005021189A1 (ja) | 2003-08-29 | 2004-07-29 | チタン化合物被覆ニッケル粉末およびこれを用いた導電ペースト |
TW093125687A TWI241227B (en) | 2003-08-29 | 2004-08-27 | Nickel powder coated with titanium compound and conductive paste containing the nickel powder |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2003306966A JP4276031B2 (ja) | 2003-08-29 | 2003-08-29 | チタン化合物被覆ニッケル粉末およびこれを用いた導電ペースト |
Publications (3)
Publication Number | Publication Date |
---|---|
JP2005076074A JP2005076074A (ja) | 2005-03-24 |
JP2005076074A5 true JP2005076074A5 (ja) | 2006-05-25 |
JP4276031B2 JP4276031B2 (ja) | 2009-06-10 |
Family
ID=34269413
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2003306966A Expired - Lifetime JP4276031B2 (ja) | 2003-08-29 | 2003-08-29 | チタン化合物被覆ニッケル粉末およびこれを用いた導電ペースト |
Country Status (3)
Country | Link |
---|---|
JP (1) | JP4276031B2 (ja) |
TW (1) | TWI241227B (ja) |
WO (1) | WO2005021189A1 (ja) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP6512734B2 (ja) * | 2014-01-15 | 2019-05-15 | 日本化学工業株式会社 | 被覆導電性粉体、被覆導電性粉体の製造方法、被覆導電性粉体を含む導電性接着剤及び接着構造体 |
JP6395196B2 (ja) * | 2017-07-20 | 2018-09-26 | 日本化学工業株式会社 | 被覆導電性粉体、被覆導電性粉体の製造方法、被覆導電性粉体を含む導電性接着剤及び接着構造体 |
JP6469817B2 (ja) * | 2017-11-07 | 2019-02-13 | 日本化学工業株式会社 | 被覆導電性粉体、被覆導電性粉体の製造方法、被覆導電性粉体を含む導電性接着剤及び接着構造体 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP4076107B2 (ja) * | 1999-03-31 | 2008-04-16 | 三井金属鉱業株式会社 | 複合ニッケル微粉末の製造方法 |
JP2992270B2 (ja) * | 1998-05-29 | 1999-12-20 | 三井金属鉱業株式会社 | 複合ニッケル微粉末及びその製造方法 |
-
2003
- 2003-08-29 JP JP2003306966A patent/JP4276031B2/ja not_active Expired - Lifetime
-
2004
- 2004-07-29 WO PCT/JP2004/010799 patent/WO2005021189A1/ja active Application Filing