JP2002028490A5 - - Google Patents

Download PDF

Info

Publication number
JP2002028490A5
JP2002028490A5 JP2000213093A JP2000213093A JP2002028490A5 JP 2002028490 A5 JP2002028490 A5 JP 2002028490A5 JP 2000213093 A JP2000213093 A JP 2000213093A JP 2000213093 A JP2000213093 A JP 2000213093A JP 2002028490 A5 JP2002028490 A5 JP 2002028490A5
Authority
JP
Japan
Prior art keywords
catalyst
foam
metal
ruthenium
nickel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2000213093A
Other languages
English (en)
Japanese (ja)
Other versions
JP4551538B2 (ja
JP2002028490A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2000213093A priority Critical patent/JP4551538B2/ja
Priority claimed from JP2000213093A external-priority patent/JP4551538B2/ja
Publication of JP2002028490A publication Critical patent/JP2002028490A/ja
Publication of JP2002028490A5 publication Critical patent/JP2002028490A5/ja
Application granted granted Critical
Publication of JP4551538B2 publication Critical patent/JP4551538B2/ja
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

JP2000213093A 2000-07-13 2000-07-13 水蒸気改質触媒の製造方法 Expired - Fee Related JP4551538B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2000213093A JP4551538B2 (ja) 2000-07-13 2000-07-13 水蒸気改質触媒の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2000213093A JP4551538B2 (ja) 2000-07-13 2000-07-13 水蒸気改質触媒の製造方法

Publications (3)

Publication Number Publication Date
JP2002028490A JP2002028490A (ja) 2002-01-29
JP2002028490A5 true JP2002028490A5 (enExample) 2007-08-30
JP4551538B2 JP4551538B2 (ja) 2010-09-29

Family

ID=18708904

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2000213093A Expired - Fee Related JP4551538B2 (ja) 2000-07-13 2000-07-13 水蒸気改質触媒の製造方法

Country Status (1)

Country Link
JP (1) JP4551538B2 (enExample)

Families Citing this family (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
BR0001560B1 (pt) 1999-04-09 2010-04-06 Denso Corporation processo para produzir um corpo cerámico-catalisador, e, corpo cerámico-catalisador.
JP4030320B2 (ja) 2001-03-22 2008-01-09 株式会社デンソー セラミック体およびセラミック触媒体
JP4753168B2 (ja) * 2003-11-17 2011-08-24 猛央 山口 炭化水素改質水素製造システム
US7659019B2 (en) * 2005-09-16 2010-02-09 Idatech, Llc Thermally primed hydrogen-producing fuel cell system
JP5811856B2 (ja) * 2011-03-08 2015-11-11 株式会社デンソー 水蒸気改質用触媒及び改質触媒体
JP6903324B2 (ja) * 2017-08-10 2021-07-14 国立研究開発法人物質・材料研究機構 水素製造用触媒、その製造方法、および、それを用いた水素製造装置
JP6980205B2 (ja) * 2017-08-10 2021-12-15 国立研究開発法人物質・材料研究機構 水素製造用触媒及びその製造方法、並びに水素製造装置
US11938471B2 (en) 2018-09-14 2024-03-26 Sumitomo Electric Industries, Ltd. Metal porous body, water vapor reformer including the same, and method for manufacturing metal porous body

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5832001A (ja) * 1981-08-20 1983-02-24 Babcock Hitachi Kk 水素製造装置
US6540975B2 (en) * 1998-07-27 2003-04-01 Battelle Memorial Institute Method and apparatus for obtaining enhanced production rate of thermal chemical reactions
CN1350507A (zh) * 1998-11-05 2002-05-22 Abb拉默斯环球有限公司 含氢气流的生产

Similar Documents

Publication Publication Date Title
Li et al. Ternary PtIrNi catalysts for efficient electrochemical ammonia oxidation
Raghuveer et al. Pd− Co− Mo electrocatalyst for the oxygen reduction reaction in proton exchange membrane fuel cells
Wu et al. Ultrafine Pt nanoparticles and amorphous nickel supported on 3D mesoporous carbon derived from Cu-metal–organic framework for efficient methanol oxidation and nitrophenol reduction
Alia et al. Platinum-coated copper nanowires with high activity for hydrogen oxidation reaction in base
Antolini Palladium in fuel cell catalysis
Sasaki et al. Designing high performance Pt monolayer core–shell electrocatalysts for fuel cells
Chen et al. Geometrically controlled nanoporous PdAu bimetallic catalysts with tunable Pd/Au ratio for direct ethanol fuel cells
Kwon et al. Active methanol oxidation reaction by enhanced CO tolerance on bimetallic Pt/Ir electrocatalysts using electronic and bifunctional effects
CN101781769B (zh) 用于水电解的膜电极及其制备方法
US20060099482A1 (en) Fuel cell electrode
US20070105005A1 (en) Nanostructured core-shell electrocatalysts for fuel cells
EP2664378A2 (en) Metal structure catalyst and preparation method thereof
CN102709574A (zh) 催化剂层、膜电极组件以及电化学电池
Jeong et al. Bimetallic nickel/ruthenium catalysts synthesized by atomic layer deposition for low-temperature direct methanol solid oxide fuel cells
Krishnamurthy et al. First-principles investigation of the formation of Pt nanorafts on a Mo2C support and their catalytic activity for oxygen reduction reaction
CN108479820B (zh) 一种硼氢化钠醇解制氢用块状载体纳米型合金催化剂及其制备方法
CN105449229A (zh) 催化剂层、其制备方法、膜电极组件以及电化学电池
Tarasevich et al. Electrocatalysis of anodic oxidation of ethanol
Solmaz Gold‐supported activated NiZn coatings: hydrogen evolution and corrosion studies
TWI474547B (zh) 電催化觸媒及包含其之燃料電池
JP4551538B2 (ja) 水蒸気改質触媒の製造方法
US7833934B2 (en) Hydrocarbon reforming catalyst, method of preparing the same and fuel processor including the same
Kumaravel et al. DNA-Modified Cobalt Tungsten Oxide Hydroxide Hydrate Nanochains as an Effective Electrocatalyst with Amplified CO Tolerance during Methanol Oxidation
Almeida et al. Influence of the metallic load of Pt/C and Pt0. 6-Ru0. 4/C nanowires on the electrochemical oxidation of methanol in acid medium
CN118308747A (zh) 一种镍钴双金属/介孔石墨烯@泡沫镍复合材料及其制备方法与应用