IT996202B - Perfezionamento nelle batterie elettriche secondarie con anodo di metallo alcalino allo stato fuso catodo di carbone ed elet trolito di sale allo stato fuso - Google Patents
Perfezionamento nelle batterie elettriche secondarie con anodo di metallo alcalino allo stato fuso catodo di carbone ed elet trolito di sale allo stato fusoInfo
- Publication number
- IT996202B IT996202B IT52741/73A IT5274173A IT996202B IT 996202 B IT996202 B IT 996202B IT 52741/73 A IT52741/73 A IT 52741/73A IT 5274173 A IT5274173 A IT 5274173A IT 996202 B IT996202 B IT 996202B
- Authority
- IT
- Italy
- Prior art keywords
- melted
- elettrolite
- improvement
- alkaline metal
- metal anode
- Prior art date
Links
- OKTJSMMVPCPJKN-UHFFFAOYSA-N Carbon Chemical compound [C] OKTJSMMVPCPJKN-UHFFFAOYSA-N 0.000 title 1
- 229910052799 carbon Inorganic materials 0.000 title 1
- 239000002184 metal Substances 0.000 title 1
- 150000003839 salts Chemical class 0.000 title 1
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/36—Accumulators not provided for in groups H01M10/05-H01M10/34
- H01M10/39—Accumulators not provided for in groups H01M10/05-H01M10/34 working at high temperature
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Secondary Cells (AREA)
- Battery Electrode And Active Subsutance (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US00292281A US3847667A (en) | 1972-09-26 | 1972-09-26 | Alkali metal-porous conductive carbon battery having a molten alkali metal chloraluminate electrolyte |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| IT996202B true IT996202B (it) | 1975-12-10 |
Family
ID=23124000
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| IT52741/73A IT996202B (it) | 1972-09-26 | 1973-09-25 | Perfezionamento nelle batterie elettriche secondarie con anodo di metallo alcalino allo stato fuso catodo di carbone ed elet trolito di sale allo stato fuso |
Country Status (12)
| Country | Link |
|---|---|
| US (1) | US3847667A (it) |
| JP (1) | JPS5233287B2 (it) |
| BE (1) | BE805283A (it) |
| BR (1) | BR7307060D0 (it) |
| CA (1) | CA977824A (it) |
| CH (1) | CH578261A5 (it) |
| DE (1) | DE2348258C3 (it) |
| FR (1) | FR2200643B1 (it) |
| GB (1) | GB1381448A (it) |
| IT (1) | IT996202B (it) |
| NL (1) | NL7313212A (it) |
| SE (1) | SE384100B (it) |
Families Citing this family (25)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3960597A (en) * | 1975-06-09 | 1976-06-01 | Esb Incorporated | Method for fabricating electrochemical cells |
| FR2396234A1 (fr) * | 1977-06-28 | 1979-01-26 | Michelin & Cie | Dispositif comportant un compartiment et un conduit |
| CA1149865A (en) * | 1979-08-22 | 1983-07-12 | Margaretha J. Nolte | Electrolyte for an electrochemical cell, and an electrochemical cell including the electrolyte |
| JPS56105192U (it) * | 1980-01-14 | 1981-08-17 | ||
| ZA828603B (en) * | 1981-12-10 | 1983-09-28 | South African Inventions | Electrochemical cell |
| GB2121597B (en) * | 1982-06-04 | 1986-01-29 | Us Energy | Sodium - sodium nitrate cell |
| US4886715A (en) * | 1987-01-16 | 1989-12-12 | The Dow Chemical Company | Molten membrane electrolyte battery |
| US4859897A (en) * | 1988-04-07 | 1989-08-22 | Frank Massa | Directional waterproof ultrasonic transducer for operating in air |
| US4965146A (en) * | 1988-09-28 | 1990-10-23 | The Dow Chemical Company | Molten membrane electrolyte battery |
| US4929521A (en) * | 1988-09-28 | 1990-05-29 | The Dow Chemical Company | Solid electrolyte battery |
| US5194343A (en) * | 1990-10-09 | 1993-03-16 | The United States Of America As Represented By The United States Department Of Energy | Method of electrode fabrication and an electrode for metal chloride battery |
| IT1269906B (it) * | 1993-04-02 | 1997-04-16 | Programme 3 Patent Holding | Cella elettrochimica |
| US6379844B1 (en) * | 2000-01-20 | 2002-04-30 | The United States Of America As Represented By The United States Department Of Energy | Low resistance electrode construction |
| US10020543B2 (en) | 2010-11-05 | 2018-07-10 | Field Upgrading Usa, Inc. | Low temperature battery with molten sodium-FSA electrolyte |
| US10056651B2 (en) | 2010-11-05 | 2018-08-21 | Field Upgrading Usa, Inc. | Low temperature secondary cell with sodium intercalation electrode |
| DE102011002729A1 (de) * | 2011-01-14 | 2012-07-19 | Siemens Aktiengesellschaft | Energiespeicheranordnung |
| US10224577B2 (en) | 2011-11-07 | 2019-03-05 | Field Upgrading Usa, Inc. | Battery charge transfer mechanisms |
| US20140168856A1 (en) * | 2012-12-18 | 2014-06-19 | General Electric Company | Asymmetric electrochemical capacitor positive electrode composition and asymmetric electrochemical capacitor cells and devices comprising same |
| EP3005464B1 (en) | 2013-05-30 | 2020-05-13 | Field Upgrading USA, Inc. | Hybrid molten/solid sodium anode for room/intermediate temperature electric vehicle battery |
| AU2014274717B2 (en) * | 2013-06-06 | 2018-12-13 | Field Upgrading Usa, Inc. | Low viscosity/high conductivity sodium haloaluminate electrolyte |
| JP6476189B2 (ja) | 2013-09-05 | 2019-02-27 | フィールド アップグレーディング ユーエスエー・インク | 高エネルギー効率を有する高温ナトリウム電池 |
| US9537179B2 (en) | 2013-09-25 | 2017-01-03 | Ceramatec, Inc. | Intermediate temperature sodium-metal halide battery |
| CA2983001C (en) * | 2015-04-17 | 2021-07-27 | Field Upgrading Usa, Inc. | Sodium-aluminum battery with sodium ion conductive ceramic separator |
| US10026996B2 (en) * | 2016-04-11 | 2018-07-17 | Dynantis Corp | Molten alkali metal-aluminum secondary battery |
| US12166187B1 (en) | 2024-04-08 | 2024-12-10 | Inlyte Energy, Inc. | Method for improving performance of metal conversion batteries and metal conversion batteries formed therefrom preliminary class |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3382102A (en) * | 1965-09-02 | 1968-05-07 | Gen Electric | Zinc-bromine secondary cell |
| US3404036A (en) * | 1965-10-22 | 1968-10-01 | Ford Motor Co | Energy conversion device comprising a solid crystalline electrolyte and a solid reaction zone separator |
| US3404035A (en) * | 1965-10-22 | 1968-10-01 | Ford Motor Co | Secondary battery employing molten alkali metal reactant |
| US3415687A (en) * | 1966-03-29 | 1968-12-10 | Honeywell Inc | Electric current producing cell |
| US3650834A (en) * | 1970-01-28 | 1972-03-21 | Standard Oil Co Ohio | Aluminum bromide fused salt battery |
| FR2115522A5 (en) * | 1970-11-23 | 1972-07-07 | Accumulateurs Fixes | Sodium-sodium halide cell - using aluminium chloride-sodium halide complexes |
| US3751298A (en) * | 1971-05-21 | 1973-08-07 | Union Carbide Corp | Thermal, rechargeable electrochemical cell having lithium monoaluminide electrode and lithium tetrachloroaluminate electrolyte |
-
1972
- 1972-09-26 US US00292281A patent/US3847667A/en not_active Expired - Lifetime
-
1973
- 1973-09-12 BR BR7060/73A patent/BR7307060D0/pt unknown
- 1973-09-24 GB GB4459573A patent/GB1381448A/en not_active Expired
- 1973-09-25 DE DE2348258A patent/DE2348258C3/de not_active Expired
- 1973-09-25 JP JP48107873A patent/JPS5233287B2/ja not_active Expired
- 1973-09-25 CH CH1372673A patent/CH578261A5/xx not_active IP Right Cessation
- 1973-09-25 IT IT52741/73A patent/IT996202B/it active
- 1973-09-25 CA CA181,895A patent/CA977824A/en not_active Expired
- 1973-09-25 FR FR7334343A patent/FR2200643B1/fr not_active Expired
- 1973-09-25 BE BE136019A patent/BE805283A/xx unknown
- 1973-09-25 SE SE7313067A patent/SE384100B/xx unknown
- 1973-09-25 NL NL7313212A patent/NL7313212A/xx not_active Application Discontinuation
Also Published As
| Publication number | Publication date |
|---|---|
| BR7307060D0 (pt) | 1974-07-11 |
| GB1381448A (en) | 1975-01-22 |
| JPS5233287B2 (it) | 1977-08-27 |
| CH578261A5 (it) | 1976-07-30 |
| FR2200643A1 (it) | 1974-04-19 |
| BE805283A (fr) | 1974-03-25 |
| US3847667A (en) | 1974-11-12 |
| CA977824A (en) | 1975-11-11 |
| DE2348258C3 (de) | 1980-06-19 |
| NL7313212A (it) | 1974-03-28 |
| DE2348258A1 (de) | 1974-03-28 |
| JPS4970141A (it) | 1974-07-06 |
| SE384100B (sv) | 1976-04-12 |
| DE2348258B2 (de) | 1979-09-27 |
| FR2200643B1 (it) | 1978-01-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| IT996202B (it) | Perfezionamento nelle batterie elettriche secondarie con anodo di metallo alcalino allo stato fuso catodo di carbone ed elet trolito di sale allo stato fuso | |
| JPS5566873A (en) | Battery containing alkaline metal anode* solid cathode and chloroborane and*or chlorocarborane electrolyte | |
| IT1096587B (it) | Batterie reversibili con anodi di metallo alcalino,catodi di calcogenuro e contenenti elettroliti a base di composti poliarilmetallici di metalli alcalini | |
| GB1533116A (en) | Electric batteries | |
| ES451238A1 (es) | Mejoras introducidas en una pila electroquimica. | |
| CA961092A (en) | Electrochemical cell with molten lithium anode and molten selenium cathode | |
| IT1125375B (it) | Catodo per cella di elettrolisi allo stato fuso | |
| CA1003036A (en) | Solid-state battery with anode of light metal and electrolyte containing iodine | |
| IT1066316B (it) | Perfezionamento nelle celle elettrochimiche in particolare batterie zinco ossido di argento | |
| SE404463B (sv) | Galvanisk cell innefattande en zinkanod, en mangandioxidkatod och en alkalisk elektrolyt | |
| JPS5233036A (en) | Battery having anode made of strongly positive metal and nonnaqueous electrolyte | |
| JPS5265798A (en) | Electrolytic cell equipped with vertical anode and cathode and method operating thereof | |
| GB1131458A (en) | Storage battery | |
| BG28429A3 (bg) | Положителен електрод за оловни акумулатори | |
| GB1065059A (en) | Improvements relating to storage battery electrodes | |
| JPS5221623A (en) | Galvanic battery having anode composed of light metal* nonnaqueous electrolyte and metal oxide cathode | |
| IT1058006B (it) | Perfezionamento nelle pile elettriche con elettrolita alcalino e procedimento di fabbricazione | |
| GB1047821A (en) | Improvements in or relating to batteries | |
| GB981405A (en) | Improvements in electric accumulators | |
| GB1251223A (it) | ||
| GB544770A (en) | Improvements in electric storage batteries | |
| GB971351A (en) | High power output primary battery | |
| GB1200418A (en) | Electric currrent producing cell | |
| GB1028548A (en) | Improvements in or relating to electric batteries | |
| IT1148799B (it) | Composizione di sali fusi utilizzabile come elettrolita anodico negli accumulatori ad allumina alcalina ed elettrodo negativo di metallo alcalino |