GB1209083A - Improvements relating to energy storage systems - Google Patents
Improvements relating to energy storage systemsInfo
- Publication number
- GB1209083A GB1209083A GB6063/68A GB606368A GB1209083A GB 1209083 A GB1209083 A GB 1209083A GB 6063/68 A GB6063/68 A GB 6063/68A GB 606368 A GB606368 A GB 606368A GB 1209083 A GB1209083 A GB 1209083A
- Authority
- GB
- United Kingdom
- Prior art keywords
- weight per
- per cent
- metal
- hydrogen
- titanium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/242—Hydrogen storage electrodes
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/36—Selection of substances as active materials, active masses, active liquids
- H01M4/38—Selection of substances as active materials, active masses, active liquids of elements or alloys
- H01M4/383—Hydrogen absorbing alloys
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
- Electrodes For Compound Or Non-Metal Manufacture (AREA)
Priority Applications (5)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB6063/68A GB1209083A (en) | 1968-02-07 | 1968-02-07 | Improvements relating to energy storage systems |
DE19691905453 DE1905453A1 (de) | 1968-02-07 | 1969-02-04 | Speichersystem fuer elektrische Energie |
BE728028D BE728028A (enrdf_load_stackoverflow) | 1968-02-07 | 1969-02-06 | |
FR6902976A FR2001502A1 (fr) | 1968-02-07 | 1969-02-07 | Electrodes pour piles a combustible |
NL6901954A NL6901954A (enrdf_load_stackoverflow) | 1968-02-07 | 1969-02-07 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB6063/68A GB1209083A (en) | 1968-02-07 | 1968-02-07 | Improvements relating to energy storage systems |
Publications (1)
Publication Number | Publication Date |
---|---|
GB1209083A true GB1209083A (en) | 1970-10-14 |
Family
ID=9807753
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB6063/68A Expired GB1209083A (en) | 1968-02-07 | 1968-02-07 | Improvements relating to energy storage systems |
Country Status (5)
Country | Link |
---|---|
BE (1) | BE728028A (enrdf_load_stackoverflow) |
DE (1) | DE1905453A1 (enrdf_load_stackoverflow) |
FR (1) | FR2001502A1 (enrdf_load_stackoverflow) |
GB (1) | GB1209083A (enrdf_load_stackoverflow) |
NL (1) | NL6901954A (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6097550A (ja) * | 1983-11-01 | 1985-05-31 | Matsushita Electric Ind Co Ltd | 蓄電池用陰極 |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4551400A (en) * | 1984-04-18 | 1985-11-05 | Energy Conversion Devices, Inc. | Hydrogen storage materials and methods of sizing and preparing the same for electrochemical applications |
-
1968
- 1968-02-07 GB GB6063/68A patent/GB1209083A/en not_active Expired
-
1969
- 1969-02-04 DE DE19691905453 patent/DE1905453A1/de active Pending
- 1969-02-06 BE BE728028D patent/BE728028A/xx unknown
- 1969-02-07 NL NL6901954A patent/NL6901954A/xx unknown
- 1969-02-07 FR FR6902976A patent/FR2001502A1/fr not_active Withdrawn
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6097550A (ja) * | 1983-11-01 | 1985-05-31 | Matsushita Electric Ind Co Ltd | 蓄電池用陰極 |
Also Published As
Publication number | Publication date |
---|---|
DE1905453A1 (de) | 1969-08-28 |
BE728028A (enrdf_load_stackoverflow) | 1969-08-06 |
FR2001502A1 (fr) | 1969-09-26 |
NL6901954A (enrdf_load_stackoverflow) | 1969-08-11 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB1082568A (en) | Improvements relating to mouldings of carbides | |
GB1245158A (en) | Improvements in nickel-chromium alloys | |
GB1408372A (en) | Nickel base alloys | |
GB1209083A (en) | Improvements relating to energy storage systems | |
GB1260982A (en) | Improvements in or relating to nickel base alloys | |
GB995901A (en) | Double skeleton catalyst electrode, particularly for fuel cells | |
GB1319720A (en) | Alloys for gettering moisture and reactive gases | |
Smith | Effect of hydrogen on nickel and nickel-base alloys | |
GB1092471A (en) | Hydrogen electrodes | |
Jardin et al. | Influence of small additions of carbon on the intergranular brittleness of highly pure molybdenum bicrystals | |
Kolachev | Phase Constitution of Hydrogenation Products of Titanium Alloys | |
Padurets et al. | Reactions of Hydrogen With Some Titanium Alloys and Intermetallic Compounds | |
Pahutová et al. | Creep of Zr-Nb Alloys in the Temperature Range 350-550 C. Pt. 1. Steady-State Creep in a Zr 2. 5 per cent Nb Alloy | |
Ageenkov et al. | Absorption of hydrogen by zirconium alloys at elevated temperatures | |
GORBUNOV et al. | Investigation of the oxidation of VT-14, VT-8, VT-3-1 alloys and of no. 1 experimental alloy in air at 800 to 1200 deg C(Oxidation kinetics and formation of gas saturated layers in titanium alloys in air at high temperatures) | |
GORELIK et al. | Certain features of structural transformations in niobium, tantalum, and the Nb-Mo alloy during local deformation(Elastic stresses during local deformation in Nb-Mo, Ni-Cr, Cu-Al and pure bcc metals, using X ray analysis) | |
Dzhodzhua | The Vacuum Properties of Some Stainless Steels | |
RILEY et al. | Compatibility of Zircaloy-4 and Nb-1 WT percent Zr alloy in hydrogen as a function of temperature(Susceptibility of Zircaloy 4 and niobium base alloy to hydrogen embrittlement at elevated temperature) | |
GB1039828A (en) | Improvements in or relating to fuel cells | |
Nikolaev et al. | Isomer Shifts in Pt 3 Fe Alloys and Stainless Steel Under Pressure | |
Hoffmann et al. | EFFECT OF STEAM IN THE SINTERING GAS ON THE BEHAVIOUR OF METAL POWDERS WITH OXIDE LAYERS ABLE TO BE REDUCED UNDER SINTERING CONDITIONS | |
Peshkov et al. | Creep of titanium alloy OT-4 | |
ESPEVIK et al. | Oxidation of tantalum coated with aluminum and aluminum-chromium alloys(Oxidation of tantalum coated with aluminum and aluminum-chromium alloys at high temperatures and various oxygen pressures, using X-ray diffraction, electron microscopy, etc) | |
ARGENT et al. | The creep of niobium-molybdenum alloys(Creep of high purity Nb-Mo alloys in 800-1300 C range and at 1500-13000 lb/square inch stresses, giving activation energy for creep) | |
Mirotvorskii et al. | High-temperature strength of tungsten wire VT-7 in powder matrices |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PS | Patent sealed | ||
PLNP | Patent lapsed through nonpayment of renewal fees |