GB1174576A - Improvements relating to Methods of Joining Metal in Lead Acid Secondary Electric Batteries - Google Patents
Improvements relating to Methods of Joining Metal in Lead Acid Secondary Electric BatteriesInfo
- Publication number
- GB1174576A GB1174576A GB54878/65A GB5487865A GB1174576A GB 1174576 A GB1174576 A GB 1174576A GB 54878/65 A GB54878/65 A GB 54878/65A GB 5487865 A GB5487865 A GB 5487865A GB 1174576 A GB1174576 A GB 1174576A
- Authority
- GB
- United Kingdom
- Prior art keywords
- lead
- pillar
- grid
- dispersion strengthened
- lugs
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
1,174,576. Welding by pressure. ELECTRIC POWER STORAGE Ltd. 22 Dec., 1966 [24 Dec., 1965], No. 54878/65. Heading B3R. [Also in Division H1] In connecting a metal terminal pillar to a plate grid formed of dispersion strengthened lead for a lead acid secondary electric battery, a joint between the grid and the pillar or between the grid and a metal member which is itself secured to the pillar is effected by cold welding. A grid 10, Fig. 1, formed by extrusion and rolling from dispersion strengthened lead has an integral lug 11 with a tapered end 13 and this end 13 is lapped over a strip of lead alloy 12 also having a tapered end 14 in a die 15. A punch 16 having a working face 17 with semicircular ends and rounded edges is applied to the ends 12, 14 at a pressure of 12,200 p.s.i. to weld them together with 50% reduction. The bulging edges of the joint may be sheared off. The strips of a number of grids are then secured to a pillar by burning. In another embodiment, a number of dispersion strengthened lead grids 20 have integral lugs 21, Fig. 3, and these lugs are arranged in grooves 22 in a lead or lead alloy pillar 23 formed with an integral terminal and the pillar is compressed in a press to cold weld the lugs in the grooves. The materials to which the dispersion strengthened lead is cold welded may be a lead alloy containing tin and selenium or tin, calcium and silver or tin and calcium or it may be pure lead.
Priority Applications (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB54878/65A GB1174576A (en) | 1965-12-24 | 1965-12-24 | Improvements relating to Methods of Joining Metal in Lead Acid Secondary Electric Batteries |
DE19661500715 DE1500715A1 (en) | 1965-12-24 | 1966-12-21 | Method for joining two metal parts |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB54878/65A GB1174576A (en) | 1965-12-24 | 1965-12-24 | Improvements relating to Methods of Joining Metal in Lead Acid Secondary Electric Batteries |
Publications (1)
Publication Number | Publication Date |
---|---|
GB1174576A true GB1174576A (en) | 1969-12-17 |
Family
ID=10472332
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB54878/65A Expired GB1174576A (en) | 1965-12-24 | 1965-12-24 | Improvements relating to Methods of Joining Metal in Lead Acid Secondary Electric Batteries |
Country Status (2)
Country | Link |
---|---|
DE (1) | DE1500715A1 (en) |
GB (1) | GB1174576A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB2371055A (en) * | 2001-01-15 | 2002-07-17 | Innovation And Technology Alum | Anode for electrolysis of aluminium |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4002284A (en) * | 1971-06-29 | 1977-01-11 | Metall-Werk Merkur Gmbh | Method of making a cold welded connection |
-
1965
- 1965-12-24 GB GB54878/65A patent/GB1174576A/en not_active Expired
-
1966
- 1966-12-21 DE DE19661500715 patent/DE1500715A1/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB2371055A (en) * | 2001-01-15 | 2002-07-17 | Innovation And Technology Alum | Anode for electrolysis of aluminium |
Also Published As
Publication number | Publication date |
---|---|
DE1500715A1 (en) | 1969-05-08 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB839090A (en) | Improvements in electrical connections and methods and die-sets for making them | |
IT996202B (en) | IMPROVEMENT IN SECONDARY ELECTRIC BATTERIES WITH MELTED ALKALINE METAL ANODE CARBON CATHODE AND MELTED SALT ELETTROLITE | |
GB1260413A (en) | Sealed electrolytic cells | |
GB1442556A (en) | Zinc electrode and method of making same | |
GB1174576A (en) | Improvements relating to Methods of Joining Metal in Lead Acid Secondary Electric Batteries | |
GB1359747A (en) | Method of electrically connecting a conducting member to a terminal of electric apparatus by means of electric resistance welding | |
GB998580A (en) | Improved resistance welding | |
GB1434003A (en) | Electrical terminals | |
DE1421623B2 (en) | Method of manufacturing a duplex electrode | |
CN211088326U (en) | Sealing element for top cover of lithium ion battery | |
GB1024525A (en) | Improved means for establishing electrical connection with a conductor made of aluminium or an aluminium alloy | |
CN203406363U (en) | Positive lead and soft package lithium ion battery | |
CN215220942U (en) | Battery cover plate negative pole column | |
GB1239147A (en) | ||
GB1114332A (en) | Improvements relating to plate assemblies for multi-cell batteries | |
GB1370777A (en) | Electrodes for electro-chemical cells | |
FR2209634A1 (en) | Current pulse welding of collector rods - with turned down ends to cell end plates by current pulse | |
JPS61133571A (en) | Flat battery | |
JPS5791883A (en) | Production of can | |
JPS61281475A (en) | Manufacture of chargeable electrochemical device | |
JPH0521263Y2 (en) | ||
GB214799A (en) | Improvements in or relating to electric storage batteries | |
GB1185925A (en) | Improvements in or relating to Laminates | |
GB985676A (en) | Improvements in and relating to a method of machining a flanging punch and die | |
JPS5684120A (en) | Manufacture of steel-cored aluminum-covered wire |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PS | Patent sealed [section 19, patents act 1949] | ||
PLNP | Patent lapsed through nonpayment of renewal fees |