FR2440237A1 - Conformation des blocs de fond pour la coulee de metal, notamment de cuivre, par voie electromagnetique - Google Patents
Conformation des blocs de fond pour la coulee de metal, notamment de cuivre, par voie electromagnetiqueInfo
- Publication number
- FR2440237A1 FR2440237A1 FR7920609A FR7920609A FR2440237A1 FR 2440237 A1 FR2440237 A1 FR 2440237A1 FR 7920609 A FR7920609 A FR 7920609A FR 7920609 A FR7920609 A FR 7920609A FR 2440237 A1 FR2440237 A1 FR 2440237A1
- Authority
- FR
- France
- Prior art keywords
- metal
- casting
- lingotier
- electromagnetically
- conformation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
L'INVENTION APPORTE UN BLOC DE FOND DE LINGOTIERE ET UN PROCEDE POUR COMMENCER LA COULEE DANS UNE LINGOTIERE OU LE METAL LIQUIDE EST MAINTENU ENTRE DES LIMITES DEFINIES ET CONFORME PAR UN CHAMP ELECTROMAGNETIQUE PENDANT SA SOLIDIFICATION. SELON L'INVENTION, LE BLOC DE FOND 22 EST EN UNE MATIERE DONT LA RESISTIVITE EST VOISINE DE CELLE DU METAL A COULER, ARRIVANT PAR LE TUBE DE COULEE 16, DE MANIERE A CREER, SUR LE PLAN ELECTRIQUE, DES CONDITIONS SEMBLABLES A CELLES REGNANT PENDANT LA COULEE STABLE. DE PLUS, DANS LA FACE SUPERIEURE DU BLOC DE FOND 22 EST FORME UN CREUX PROFOND 32 QUI RECOIT ET EMPECHE LE DEBORDEMENT DE L'AFFLUX INITIAL DE METAL FONDU AMENE A LA LINGOTIERE 10, COMPRENANT UN INDUCTEUR 11, UN DISTRIBUTEUR 12 D'EAU DE REFROIDISSEMENT ET UN ECRAN AMAGNETIQUE 14.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US95721978A | 1978-11-02 | 1978-11-02 |
Publications (1)
Publication Number | Publication Date |
---|---|
FR2440237A1 true FR2440237A1 (fr) | 1980-05-30 |
Family
ID=25499250
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7920609A Withdrawn FR2440237A1 (fr) | 1978-11-02 | 1979-08-13 | Conformation des blocs de fond pour la coulee de metal, notamment de cuivre, par voie electromagnetique |
Country Status (5)
Country | Link |
---|---|
JP (1) | JPS5564949A (fr) |
DE (1) | DE2944077A1 (fr) |
FR (1) | FR2440237A1 (fr) |
GB (1) | GB2034216B (fr) |
IT (1) | IT1120544B (fr) |
Families Citing this family (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4373571A (en) * | 1980-12-04 | 1983-02-15 | Olin Corporation | Apparatus and process for electromagnetically shaping a molten material within a narrow containment zone |
US4509580A (en) * | 1982-12-09 | 1985-04-09 | Kaiser Aluminum & Chemical Corporation | Bottom block |
FR2570304B1 (fr) * | 1984-09-19 | 1986-11-14 | Cegedur | Procede de reglage du niveau de la ligne de contact de la surface libre du metal avec la lingotiere dans une coulee verticale |
DE4306943C2 (de) * | 1993-03-05 | 1995-05-18 | Vaw Ver Aluminium Werke Ag | Anfahrkopf für eine Vertikal-Stranggießanlage |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2944309A (en) * | 1953-09-04 | 1960-07-12 | Schaaber Otto | Rotary field chill-mold |
FR2092863A1 (en) * | 1970-06-25 | 1972-01-28 | Kuibyshevsky Metallurg | Ingot moulding in continuous and semicontin- - uous metal casting |
-
1979
- 1979-08-10 GB GB7927866A patent/GB2034216B/en not_active Expired
- 1979-08-13 FR FR7920609A patent/FR2440237A1/fr not_active Withdrawn
- 1979-08-27 JP JP10901179A patent/JPS5564949A/ja active Pending
- 1979-08-28 IT IT50114/79A patent/IT1120544B/it active
- 1979-10-31 DE DE19792944077 patent/DE2944077A1/de not_active Withdrawn
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2944309A (en) * | 1953-09-04 | 1960-07-12 | Schaaber Otto | Rotary field chill-mold |
FR2092863A1 (en) * | 1970-06-25 | 1972-01-28 | Kuibyshevsky Metallurg | Ingot moulding in continuous and semicontin- - uous metal casting |
Also Published As
Publication number | Publication date |
---|---|
GB2034216B (en) | 1982-09-22 |
GB2034216A (en) | 1980-06-04 |
JPS5564949A (en) | 1980-05-16 |
DE2944077A1 (de) | 1980-05-14 |
IT7950114A0 (it) | 1979-08-28 |
IT1120544B (it) | 1986-03-26 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5293621A (en) | Production of copper alloy containing graphite | |
Emi | Influence of physical and chemical properties of mold powders on the solidification and occurrence of surface defects of strand cast slabs | |
FR2449498A1 (fr) | Perfectionnement a un appareillage de formation d'une coulee metallique thixotrope par brassage electromagnetique du metal dans le moule, notamment un moule de coulee continue | |
BE807812A (fr) | Dispositif de brassage electromagnetique pour coulee continue d'un metal en fusion | |
FR2440237A1 (fr) | Conformation des blocs de fond pour la coulee de metal, notamment de cuivre, par voie electromagnetique | |
ES455842A1 (es) | Procedimiento de elaboracion de productos metalicos sin de- fectos de superficie, por colada continua centrifuga en una lingotera conductora enfriada. | |
BE861877A (fr) | Procede de coulee continue d'alliages metalliques et lingotiere de coulee continue pour sa mise en oeuvre | |
GB1438186A (en) | Method and apparatus for the continuous casting of killed steel | |
ATE50934T1 (de) | Stranggussverfahren. | |
FR2403850A1 (fr) | Dispositif pour produire un champ electromagnetique tournant a l'interieur du chemin d'appui a rouleaux d'une installation de coulee continue | |
GB1169071A (en) | Improvements relating to Electroslag Ingot Production | |
FR2283438A1 (fr) | Procede pour appliquer une electrode a un analyseur de gaz electrochimique a ceramique | |
JPS577359A (en) | Method and device for production of hollow pipe | |
FR2424084A1 (fr) | Dispositif d'agitation electromagnetique d'une masse coulee en continu en cours de solidification | |
FR2430279A1 (fr) | Procede et dispositif pour la coulee continue ou semi-continue de metaux et d'alliages par voie electromagnetique | |
FR2328529A1 (fr) | Procede d'obtention continue d'un fil de cuivre brillant par laminage d'une ebauche obtenue par coulee continue et installation pour la mise en oeuvre de ce procede | |
CN2420084Y (zh) | 内置式软接触电磁搅拌结晶器 | |
GB1407470A (en) | Casting of killed steel | |
JPS6235565Y2 (fr) | ||
ATE33352T1 (de) | Verfahren zum schleudergiessen von rohren. | |
SU1616766A1 (ru) | Устройство дл сифонной отливки горизонтального слитка | |
SU493291A1 (ru) | Способ автоматического регулировани процесса непрерывной разливки металлов | |
SU1741965A1 (ru) | Способ изготовлени отливок | |
FR2555745B1 (fr) | Procede, moule et dispositif incluant ledit moule pour prelever des echantillons dans un bain de metal en fusion, lequel metal, notamment de la fonte, est cassant a l'etat solidifie | |
FR2349669A1 (fr) | Procede et dispositif pour la fabrication mecanique continue de plaques de demarrage pour l'affinage electrolytique des metaux, en particulier du cuivre |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
RE | Withdrawal of published application |