FR2338775A1 - Razor blade consisting of amorphous alloy - of iron, nickel, chromium, molybdenum, tungsten and metalloids with fluorocarbon polymer coating - Google Patents
Razor blade consisting of amorphous alloy - of iron, nickel, chromium, molybdenum, tungsten and metalloids with fluorocarbon polymer coatingInfo
- Publication number
- FR2338775A1 FR2338775A1 FR7601357A FR7601357A FR2338775A1 FR 2338775 A1 FR2338775 A1 FR 2338775A1 FR 7601357 A FR7601357 A FR 7601357A FR 7601357 A FR7601357 A FR 7601357A FR 2338775 A1 FR2338775 A1 FR 2338775A1
- Authority
- FR
- France
- Prior art keywords
- metalloids
- degrees
- razor blade
- amorphous alloy
- fluorocarbon polymer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Cutting instrument, esp. (safety) razor blade, has strip(s) of amorphous alloy (I) of 60-70 (wt)% Fe-4-10% Ni, 10-20 % Cr, Mo and/or W and 5-15% metalloid(s), pref. P,B,C, Al,S,Si,Ga,Ge,As,Se and/or Te. The cutting edge(s) have a (firmly) adhering coating of a solid fluorocarbon polymer (II), pref. PTFE. MFR. is simple and the quality is better, since embrittlement of NiFe alloys on sintering the (II) coating is avoided. The (II) coating is pref. heated to a temp. of min 330 degrees C to a value above its m.pt. In an example blades produced from an alloy of 68% Fe, 4% Ni,4% Cr,2% Co, 12% Mo and 10% metalloids, with coatings of fluorocarbon telomer and PTFE, were heated rapidly, kept 8-30 min at 345-357 degrees C and chilled. Embrittlement occurred after 30 min at 371 degrees C or over but not at 343 degrees C.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7601357A FR2338775A1 (en) | 1976-01-20 | 1976-01-20 | Razor blade consisting of amorphous alloy - of iron, nickel, chromium, molybdenum, tungsten and metalloids with fluorocarbon polymer coating |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7601357A FR2338775A1 (en) | 1976-01-20 | 1976-01-20 | Razor blade consisting of amorphous alloy - of iron, nickel, chromium, molybdenum, tungsten and metalloids with fluorocarbon polymer coating |
Publications (2)
Publication Number | Publication Date |
---|---|
FR2338775A1 true FR2338775A1 (en) | 1977-08-19 |
FR2338775B1 FR2338775B1 (en) | 1980-06-13 |
Family
ID=9168114
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7601357A Granted FR2338775A1 (en) | 1976-01-20 | 1976-01-20 | Razor blade consisting of amorphous alloy - of iron, nickel, chromium, molybdenum, tungsten and metalloids with fluorocarbon polymer coating |
Country Status (1)
Country | Link |
---|---|
FR (1) | FR2338775A1 (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2376217A1 (en) * | 1976-12-29 | 1978-07-28 | Allied Chem | GLASS METAL ALLOYS WITH IMPROVED MECHANICAL STRENGTH |
EP0096551A2 (en) * | 1982-06-04 | 1983-12-21 | Tsuyoshi Masumoto | Amorphous iron-based alloy excelling in fatigue property |
Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE1024719B (en) * | 1951-04-16 | 1958-02-20 | Carpenter Steel Company | Hot-formable alloys |
FR1398384A (en) * | 1963-06-10 | 1965-05-07 | Eversharp Inc | Razor blade |
FR1492771A (en) * | 1963-10-03 | 1967-08-25 | Wilkinson Sword Ltd | Razor blade and process for its manufacture |
DE1553841A1 (en) * | 1966-03-22 | 1970-02-19 | Wmf Wuerttemberg Metallwaren | Knife blades made from corrosion-resistant austenitic stainless steel alloys |
-
1976
- 1976-01-20 FR FR7601357A patent/FR2338775A1/en active Granted
Patent Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE1024719B (en) * | 1951-04-16 | 1958-02-20 | Carpenter Steel Company | Hot-formable alloys |
FR1398384A (en) * | 1963-06-10 | 1965-05-07 | Eversharp Inc | Razor blade |
FR1492771A (en) * | 1963-10-03 | 1967-08-25 | Wilkinson Sword Ltd | Razor blade and process for its manufacture |
DE1553841A1 (en) * | 1966-03-22 | 1970-02-19 | Wmf Wuerttemberg Metallwaren | Knife blades made from corrosion-resistant austenitic stainless steel alloys |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2376217A1 (en) * | 1976-12-29 | 1978-07-28 | Allied Chem | GLASS METAL ALLOYS WITH IMPROVED MECHANICAL STRENGTH |
EP0096551A2 (en) * | 1982-06-04 | 1983-12-21 | Tsuyoshi Masumoto | Amorphous iron-based alloy excelling in fatigue property |
EP0096551B1 (en) * | 1982-06-04 | 1989-12-13 | Tsuyoshi Masumoto | Amorphous iron-based alloy excelling in fatigue property |
Also Published As
Publication number | Publication date |
---|---|
FR2338775B1 (en) | 1980-06-13 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3900636A (en) | Method of treating cutting edges | |
US3871836A (en) | Cutting blades made of or coated with an amorphous metal | |
US5528833A (en) | Scissors with ceramic coated replaceable cutting blades | |
US4720918A (en) | Razor blades | |
CA2415565A1 (en) | Razor blade and method of manufacture | |
CA1097992A (en) | Amorphous alloy razor blade | |
FR2338775A1 (en) | Razor blade consisting of amorphous alloy - of iron, nickel, chromium, molybdenum, tungsten and metalloids with fluorocarbon polymer coating | |
NL7600406A (en) | Razor blade consisting of amorphous alloy - of iron, nickel, chromium, molybdenum, tungsten and metalloids with fluorocarbon polymer coating | |
US3816920A (en) | Novel cutting edges and processes for making them | |
GB2130955A (en) | Razor blades | |
US3756865A (en) | Razor blades and process for making same | |
GB1350594A (en) | Sharpening cutting edges | |
Williams et al. | The recovery creep of niobium-stabilised austenitic stainless steels | |
SE328220B (en) | ||
IT1206381B (en) | Amorphous alloy strips for razor blades - which are based on nickel or iron, are coated with PTFE, and remain ductile after baking | |
GB360230A (en) | Improvements in and relating to methods of preventing the erosion of metallic objects | |
US1827872A (en) | Fine edged blade | |
US1827870A (en) | Fine edged blade | |
Mordike | Athermal solid solution hardening in niobium alloy single crystals | |
SU1749301A1 (en) | Alloy for blades | |
GB1329984A (en) | Process for making cutting instruments | |
Masui et al. | Hydrogen Permeation Through Iron, Nickel, and Heat-Resistant Alloys at Elevated Temperatures | |
Petrushevskii | The Activities of the Components of Liquid Iron-Nickel-Silicon Alloys | |
GB190423975A (en) | Improvements in the Manufacture of Razors. | |
GB361756A (en) | Improvements in or relating to scissors or like cutting instruments |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
TP | Transmission of property | ||
CD | Change of name or company name | ||
CD | Change of name or company name | ||
ST | Notification of lapse |