ES225233A1 - A procedure for the obtaining of glass or chemically resistant glass (Machine-translation by Google Translate, not legally binding)
- Google Patents
A procedure for the obtaining of glass or chemically resistant glass (Machine-translation by Google Translate, not legally binding)
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Schott AG
Original Assignee
Jenaer Glaswerk Schott and Gen
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jenaer Glaswerk Schott and GenfiledCriticalJenaer Glaswerk Schott and Gen
Priority to ES0225233ApriorityCriticalpatent/ES225233A1/en
Publication of ES225233A1publicationCriticalpatent/ES225233A1/en
Process for obtaining glass or chemically resistant glass, characterized by establishing a composition of silicic acid in a proportion of 61-66%, boric acid in amounts ranging between 7-10%, alumina in quantities comprised between 6-10%, oxides of sodium and potassium in amounts between 12-17% and potassium oxide between 3-6%, followed by an amount of barium oxide comprised between 0-10% and zinc, calcium or magnesium oxides in said composition. , only one of these three oxides or in any combination thereof up to a total ranging from 0-5% of the total composition. (Machine-translation by Google Translate, not legally binding)
ES0225233A1955-11-261955-11-26A procedure for the obtaining of glass or chemically resistant glass (Machine-translation by Google Translate, not legally binding)