DE923637C - Process for the protective coating of photographic image layers - Google Patents
Process for the protective coating of photographic image layersInfo
- Publication number
- DE923637C DE923637C DEO1119D DEO0001119D DE923637C DE 923637 C DE923637 C DE 923637C DE O1119 D DEO1119 D DE O1119D DE O0001119 D DEO0001119 D DE O0001119D DE 923637 C DE923637 C DE 923637C
- Authority
- DE
- Germany
- Prior art keywords
- image layers
- protective coating
- photographic image
- water
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zur Schutzbeschichtung photographischer Bildschichten Nach dein Patent 896:295 kann i man :die Schutzhe-:schichtung noch nasser photographischer Bildschichten dadurch vornehmen, daß man eiinen teil-@ve;i,se alkalisch-hydrolysierten Zelluloseesber, der nur in einem Gemisch von Azeton-Wasser löslich ist, in einer Lösung auf die nasse photographische Bildschicht aufbringt, die nicht alles zur klaren Löslichkeit ödes verseiften Esters notwendige Wasser enthält. Hierbei ist jedoch als ein gewisser Nachteil zu betrachten, d@aß die photographischen Bildschichten, :die mit einem Lack gleichbleibenden Wassergehalts behandelt werden sollen, auch einen dementsprechend einheitlichen Wassergehalt aufweisen, müssen, damit die Lacke durch zuviel oder zuwenig Wasser nicht zu einem trüben Film auftrocknen.Process for the protective coating of photographic image layers According to Your patent 896: 295 can be: the protective layer: even wet photographic Make image layers by hydrolyzing a partially alkaline hydrolyzed one Cellulose liver, which is only soluble in a mixture of acetone and water, in one Applying solution to the wet photographic image layer, which does not contain anything for clear solubility desolate saponified ester contains necessary water. Here is to be regarded as a certain disadvantage, however, that the photographic image layers, : which should be treated with a varnish of constant water content, too The paints must have a correspondingly uniform water content Do not dry up to a cloudy film with too much or too little water.
Es zeigt sich neun, daß dieser Nachteil erfindungsgemäß vermieden. werden kann und da13 Filme, deren Bildschicht verschiedene Feuch tigkeftsgrade aufweist, völlig transparent lackiert werden können, wenn man dem Lack eine gewisse Menge teilweise alkalisch hydrolysierten Polyvinyl@aze,üats hinzusetzt. Dabei kann das Polyvinyl,azieta@t ziemlich wefgehiend, gegebenenfalls sogar bis zu välliiger Wasserlöslichkeit, abgebaut sein. Man. kann erfindungsgemäß so vorgehen, daß man eine Lösung, die gleichzeitig 7ellulosmster und Polyvinyllazetat enthält, einer alkalischen Vexseifung unterwirft, oder man kann auch der auf @besitimmtengewünschten: Gnad versuiften, Zellulose-Ester-Lösung das für sich allein hydrolysierte Polyvinyllazetat ibzw., falls man vollständig verseift hat, dien. Polyvinylalkohol hinzugeben. Besonders bewährten sich Zusätze von 2 his 2o °/o, bezogen auf den Zelluloseestengehalt des Lackes. Dieser wird dadurch unempfindlicher gegen, den, schwankenden Wassergehalt der Bildschicht.It turns out that this disadvantage is avoided according to the invention. and that films whose image layer has different degrees of moisture Can be painted completely transparent if you add a certain amount of paint partially alkaline hydrolyzed polyvinyl aze, üats added. It can Polyvinyl, azieta @ t quite widespread, possibly even up to completely Water solubility, be dismantled. Man. can proceed according to the invention in such a way that a solution that simultaneously 7 contains cellulose ester and polyvinyl acetate, subjected to an alkaline soap, or you can also choose the one you want on @: Gnad saponify, cellulose ester solution the alone hydrolyzed polyvinyl acetate ibzw., if one completely has saponified, serve. Add polyvinyl alcohol. Additives have proven particularly useful from 2 to 2o%, based on the residual cellulose content of the paint. This becomes through it less sensitive to the fluctuating water content of the image layer.
Claims (1)