DE645173C - Korrosionsbestaendige Chrom-Nickel-Eisen-Legierung - Google Patents
Korrosionsbestaendige Chrom-Nickel-Eisen-LegierungInfo
- Publication number
- DE645173C DE645173C DEK140425D DEK0140425D DE645173C DE 645173 C DE645173 C DE 645173C DE K140425 D DEK140425 D DE K140425D DE K0140425 D DEK0140425 D DE K0140425D DE 645173 C DE645173 C DE 645173C
- Authority
- DE
- Germany
- Prior art keywords
- nickel
- corrosion
- iron alloy
- resistant chrome
- resistant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Korrosionsbeständige Chrom-Nickel-Eisen-Legierung Zusatz zum Patent 629 759 Gegenstand des Hauptpatents bilden korrosionsbeständige antimonhaltige Chrom-Nickel-Molybdän-Eisen-Legierungen von folgender Zusammensetzungo bis z o1% Kohlenstoff, 1o bis 25%o Chrom, 2o bis 4o% Nickel, @ bis 1oo% Molybdän, o bis 1o% Kupfer, 2 bis 7% Antimon, Rest Eisen.
- Es hat sich gezeigt, daß die im Hauptpatent angegebene hohe Korrosionsbeständigkeit auch bei Antimongehalten von 0,5 bis 2%ö vorhanden ist. Als besonders widerstands fähig, z. B. gegen den Angriff heißer, hochprozentiger Salzsäure, hat sich leine Legierung mit o,o4%oo Kohlenstoff, 13o%`o Chrom, 3o%o Nickel, 5% Molybdän, 5%o Kupfer, 1,5% Antimon, Rest Eisen erwiesen.
Claims (1)
- PATRNTTANSPRUCH Legierung nach dem Hauptpatent 629 759, dadurch gekennzeichnet, daß der Antimongehalt o-,5 bis 201f0 beträgt.