DE642436C - Process for the protection of water-sensitive, unfired leads that are embedded in pencil wood - Google Patents
Process for the protection of water-sensitive, unfired leads that are embedded in pencil woodInfo
- Publication number
- DE642436C DE642436C DEW95557D DEW0095557D DE642436C DE 642436 C DE642436 C DE 642436C DE W95557 D DEW95557 D DE W95557D DE W0095557 D DEW0095557 D DE W0095557D DE 642436 C DE642436 C DE 642436C
- Authority
- DE
- Germany
- Prior art keywords
- mines
- leads
- water
- sensitive
- fat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zum Schutze wasserempfindlicher, ungebrannter Minen, die in Stifthölzer - eingebettet werden Die Erfindung betrifft ein Verfahren zum Schutze wasserempfindlicher, ungebrannter, in Stiftholz einzubettender Minen gegen den festigkeitsvermindernden Einfluß des Wassers (Feuchtigkeit) durch Überziehen der Minen mit Fetten. -Das Verfahren kennzeichnet sich im wesentlichen dadurch, daß die Minen durch ein Bad mit geschmolzenem Fett unter Anwendung eines bekannten Abstreifers, der die Mine allseitig umgibt, hindurchgestoßen werden. Dabei wird Fett, und auch hierin liegt ein Erfindungsmerkmal, von zweckmäßig hohem Schmelzpunkt, z. B. Chlorparaffin mit einem Schmelzpunkt von 12o bis 13o°, verwendet, und der Fettschmelze kann vorteilhaft noch etwas Harz, z. B. Schellack, in Mengen von 1 o bis -5o0/1o, bezogen auf Fett, beigefügt werden.Process for the protection of water-sensitive, unfired mines, the in pencil woods - to be embedded The invention relates to a method for protection water-sensitive, unfired leads to be embedded in pencil wood against the strength-reducing leads Influence of water (moisture) by coating the mines with fats. -The procedure is characterized essentially by the fact that the mines by a bath with molten Grease using a known scraper that surrounds the mine on all sides, be pushed through. This is fat, and this is also a feature of the invention, suitably high melting point, e.g. B. Chlorinated paraffin with a melting point of 12o to 13o °, and the fat melt can advantageously add some resin, z. B. shellac, in amounts of 1 o to -5o0 / 1o, based on fat, are added.
Nach dem neuen Verfahren behandelte Schreib- oder Zeichenminen tragen :einen dünnen, rissefreien Fettfilm, der einen. vorzüglichen Schutzüberzug gegen eindringende Feuchtigkeit bildet, die beim Einleimen der Minen in Holzfassungen nicht vermieden werden kann. Besonders Farb- und Kopierminen, die mit wasserempfindlichen Bindemitteln, z. B. Tragant, hergestellt sind, erleiden durch den beim Einleimen nicht zu vermeidenden Feuchtigkeitseinfluß eine merkliche und sogar meßbare Minderung der Festigkeit, die sich je nach der - Minensorte und Zusammensetzung mehr oder minder stark auswirkt.Carrying writing or drawing leads treated according to the new process : a thin, crack-free film of grease, the one. excellent protective coating against Penetrating moisture forms when the leads are glued into wooden frames cannot be avoided. Especially color and copy leads, those with water-sensitive leads Binders, e.g. B. tragacanth, are produced, suffer from the gluing unavoidable influence of moisture a noticeable and even measurable reduction the strength, which varies depending on the - type of mine and composition more or has less of an effect.
Dieser Übelstand zwingt bisher, bei der Herstellung von Farb- und Kopierminen den Härtegrad der noch nicht eingeleimten Minen höher zu halten, als er nachträglich im Stift sein soll. Durch . das erfindungsgemäße Verfahren kann diese Ausgleichsmaßnahme in Wegfall kommen, und die Minen lassen sich von vornherein in den erforderlichen Härtegraden herstellen, weil der durch das neue Verfahren aufgebrachte Fettüberzug eine Schutzdecke gegen nachteilige Feuchtigkeitseinwirkung für die Minen bildet.So far, this drawback has been compelling in the manufacture of color and Copy leads to keep the hardness of the not yet glued leads higher than it should be in the pen afterwards. By . the inventive method can This compensatory measure will come to an end, and the mines can be closed from the outset Manufacture in the required degrees of hardness because of the new process Applied fat coating provides a protective cover against the adverse effects of moisture for the mines forms.
An sich ist es bekannt, Einzelminen mit Vaseline oder öl einzureiben; doch stellt diese Maßnahme eine Erschwerung des Fabrikationsvorganges dar; eine solche ölschicht besitzt außerdem keinen mechanischen Widerstand und wird auch beim Einpressen der Mine in die Hölzer leicht verletzt und abgerieben, so daß ein geschlossener, feuchtigkeitsabweisender Schutzüberzug nicht vorhanden ist. Dieser wird auch nicht erreicht durch die ebenfalls bekannte Maßnahme, die Minen blockartig gebündelt in geschmolzenes Fett zu tauchen und dieses dann durch Zentrifugieren oder Abtropfenlassen wieder zu entfernen. Die Mine wird hierbei zwar in sich präpariert, zeigt aber nicht den schützenden Fettfilm bzw. Außenüberzug.It is known per se to rub single leads with petroleum jelly or oil; but this measure makes the manufacturing process more difficult; one In addition, such an oil layer has no mechanical resistance and is also used in Pressing the lead into the wood slightly injured and rubbed off, so that a closed, moisture-repellent protective coating is not available. This one won't either achieved by the also known measure, the mines bundled in blocks in dip the melted fat and then centrifuge or drain it to remove again. The mine is prepared in itself, but does not show the protective grease film or outer coating.
Man .hat auch schon versucht, zerfließliche
Minen
vor Einbettung in das Holz mit einem Wachsüberzug zu versehen; doch ist diese Maßnahme
wirtschaftlich,#L4cht tragbar.,,
Man kann aber einen einwandfreien dichten und wirklich gegen Feuchtigkeit schützenden dünnen Fettüberzug auf den Minen herstellen, wenn man diese nach dem neuen Verfahren durch ein Bad mit geschmolzenem Fett hindurchstößt, aus dem die Minen durch .einen an sich bekannten Abstreifer, der die Mine allseitig umgibt, hinaustreten.But you can have a perfect seal and really against moisture Make a protective thin layer of fat on the leads, if you have them after the new method penetrates through a bath of molten fat, from which the Mines by. A known scraper that surrounds the mine on all sides, step out.
Dadurch erfolgt das reine Oberflächenfetten der Minen im rasch fortlaufenden Arbeitsgang, und es wird durch die mechanische Einwirkung des Abstreifers ein dichter Fettüberzug erreicht, der die Minen auch wirklich gegen Feuchtigkeitseinflüsse schützt und unempfindlich macht.As a result, the pure surface greasing of the mines takes place in a rapidly progressing manner Operation, and the mechanical action of the scraper makes it a tight one A grease coating that really protects the leads against the effects of moisture and makes it insensitive.
Um irrige Auffassungen auszuschließen, sei ausdrücklich darauf hingewiesen, daß das beanspruchte Verfahren nicht zu einem den Schreibcharakter der Minen verändernden Fetten dient, sondern lediglich zum überziehen der Minen auf der Oberfläche mit einem dichten, feuchtigkeitsabweisenden Fettfilm. Es können sowohl unpräparierte wie präparierte Minen mit gleich gutem Erfolg nach dem neuen Verfahren behandelt werden.In order to rule out erroneous views, it is expressly pointed out that that the claimed method does not lead to a change in the writing character of the mines Fats is used, but only to coat the mines on the surface with a dense, moisture-repellent grease film. It can be both unprepared treated like prepared mines with equally good success according to the new method will.
Bei genügend hohem Schmelzpunkt des Fettes erstarrt der Schutzüberzug auf den Minen sofort nach dem Verlassen des Bades, und die - Mine kann ohne Verletzung der Schutzschicht und ohne Gefahr -des Zusamenklebens sofort aufgefangen werden, so die. fortlaufende mechanische Durchbfettung der Minen in rascher Arbeits-;r Durchgangsfolge erfolgen kann.If the melting point of the fat is high enough, the protective coating solidifies on the mines immediately after leaving the bath, and the - mine can be used without injury the protective layer and without the risk of sticking together are caught immediately, so that. Continuous mechanical greasing of the mines in rapid working sequence can be done.
Die mechanischen Eigenschaften des Fettüberzuges kann man erhöhen, indem man der Fettmasse etwas Harz zusetzt, wodurch der Überzug eine erhöhte Zähigkeit erlangt.The mechanical properties of the fat coating can be increased, by adding some resin to the fat mass, which increases the toughness of the coating attained.
Das neue Durchstoßfettungsverfahren sichert ein durchwegs gleichmäßiges Fabrikat von dauernd gleichbleibendem Qualitätswert, der sich auch bei langer Lagerung der Stifte nicht mindert, da auch der Einfluß der Luftfeuchtigkeit auf ein Mindestmaß zurückgedrängt ist.The new push-through lubrication process ensures a consistently uniform Product of consistently constant quality value, which is also retained for long periods of time the pencil does not diminish, since the influence of the air humidity is also kept to a minimum is pushed back.
Claims (1)