DE60235804D1 - Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen, fehlerreduzierten schweissnaht - Google Patents
Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen, fehlerreduzierten schweissnahtInfo
- Publication number
- DE60235804D1 DE60235804D1 DE60235804T DE60235804T DE60235804D1 DE 60235804 D1 DE60235804 D1 DE 60235804D1 DE 60235804 T DE60235804 T DE 60235804T DE 60235804 T DE60235804 T DE 60235804T DE 60235804 D1 DE60235804 D1 DE 60235804D1
- Authority
- DE
- Germany
- Prior art keywords
- weld
- ductile
- welds
- ductile iron
- pass
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/23—Arc welding or cutting taking account of the properties of the materials to be welded
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/24—Selection of soldering or welding materials proper
- B23K35/30—Selection of soldering or welding materials proper with the principal constituent melting at less than 1550 degrees C
- B23K35/3033—Ni as the principal constituent
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K35/00—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting
- B23K35/22—Rods, electrodes, materials, or media, for use in soldering, welding, or cutting characterised by the composition or nature of the material
- B23K35/38—Selection of media, e.g. special atmospheres for surrounding the working area
- B23K35/383—Selection of media, e.g. special atmospheres for surrounding the working area mainly containing noble gases or nitrogen
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Chemical & Material Sciences (AREA)
- Materials Engineering (AREA)
- Physics & Mathematics (AREA)
- Plasma & Fusion (AREA)
- Arc Welding In General (AREA)
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US09/866,258 US6730876B2 (en) | 2001-05-29 | 2001-05-29 | Highly ductile reduced imperfection weld for ductile iron and method for producing same |
PCT/US2002/016813 WO2002096590A1 (en) | 2001-05-29 | 2002-05-29 | Highly ductile reduced imperfection weld for ductile iron and method for producing same |
Publications (1)
Publication Number | Publication Date |
---|---|
DE60235804D1 true DE60235804D1 (de) | 2010-05-12 |
Family
ID=25347240
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
DE60235804T Expired - Lifetime DE60235804D1 (de) | 2001-05-29 | 2002-05-29 | Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen, fehlerreduzierten schweissnaht |
Country Status (6)
Country | Link |
---|---|
US (1) | US6730876B2 (de) |
EP (1) | EP1390173B1 (de) |
JP (1) | JP2004527381A (de) |
AT (1) | ATE462523T1 (de) |
DE (1) | DE60235804D1 (de) |
WO (1) | WO2002096590A1 (de) |
Families Citing this family (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP4551082B2 (ja) * | 2003-11-21 | 2010-09-22 | 三菱重工業株式会社 | 溶接方法 |
FR2886314B1 (fr) * | 2005-05-26 | 2007-07-20 | Industeel France | Acier pour coques de sous-marins a soudabilite renforcee |
DE102005035585B3 (de) * | 2005-07-29 | 2006-08-10 | Areva Np Gmbh | Verfahren zur Herstellung einer Schweißverbindung sowie Verfahren zur Reparatur einer derartigen Schweißverbindung |
US20080216989A1 (en) * | 2007-03-07 | 2008-09-11 | Behr America Inc. | Weld bead reinforcement of charge air cooler headers and method of making same |
EP2387481B1 (de) * | 2008-12-10 | 2018-03-14 | Boston Scientific Scimed, Inc. | Verfahren zum verbinden von titanlegierung und stahllegierung und medizinisches bauteil mit einer solchen verbindung |
DE102010031890B3 (de) * | 2010-07-21 | 2011-11-10 | Benteler Automobiltechnik Gmbh | Verfahren zum Herstellen einer stoffschlüssigen Verbindung und Hohlprofilverbindung |
US10974349B2 (en) * | 2010-12-17 | 2021-04-13 | Magna Powertrain, Inc. | Method for gas metal arc welding (GMAW) of nitrided steel components using cored welding wire |
US9126287B2 (en) * | 2012-03-12 | 2015-09-08 | Siemens Energy, Inc. | Advanced pass progression for build-up welding |
ITMI20131271A1 (it) * | 2013-07-29 | 2015-01-30 | D G Weld S R L | Metodo per il rivestimento in materiale metallico di corpi in ghisa sferoidale e piani per stampi per macchine della pressofusione di alluminio realizzato con tale metodo |
CN114669839A (zh) * | 2022-03-29 | 2022-06-28 | 岭澳核电有限公司 | 焊缝修补方法 |
Family Cites Families (25)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US1589017A (en) | 1918-10-11 | 1926-06-15 | John C Lincoln | Method and means for electric-arc welding |
US2547872A (en) | 1948-01-31 | 1951-04-03 | Stacey Brothers Gas Constructi | Welding torch |
US2900490A (en) | 1958-06-24 | 1959-08-18 | Int Nickel Co | Coated electrode for welding cast iron |
US2995815A (en) * | 1959-03-13 | 1961-08-15 | Int Nickel Co | Welding rod and method of making and welding with same |
US3253950A (en) * | 1962-05-01 | 1966-05-31 | Eutectic Welding Alloys | Flux-coated welding electrode |
US3328557A (en) * | 1964-01-09 | 1967-06-27 | Eutectic Welding Alloys | Nickel arc welding electrode |
US3301997A (en) | 1965-02-15 | 1967-01-31 | Canada Iron Foundries Ltd | Method of welding ductile iron |
US3555239A (en) | 1966-11-16 | 1971-01-12 | William J Kerth | Welding machine with digital pulse control |
US3581053A (en) | 1967-12-05 | 1971-05-25 | Union Carbide Corp | Synchro-arc metal transfer |
US3803381A (en) | 1971-12-22 | 1974-04-09 | Dover Corp | Arc welding gun |
US3851143A (en) | 1972-03-29 | 1974-11-26 | Int Nickel Co | Weld rod |
US3851142A (en) | 1972-03-29 | 1974-11-26 | Int Nickel Co | Weld rod containing manganese |
US3778588A (en) | 1972-03-29 | 1973-12-11 | Int Nickel Co | Self-shielding cored wire to weld cast iron |
SU492394A1 (ru) | 1973-07-19 | 1975-11-25 | Ордена Ленина И Ордена Трудового Красного Знамени Институт Электросварки Им.Е.О.Патона | Сварочна проволока |
FR2251399B1 (de) | 1973-11-20 | 1978-12-01 | Pont A Mousson | |
US4087673A (en) | 1976-06-11 | 1978-05-02 | Weld Mold Company | Method of welding and electrode therefore |
DE2759836C2 (de) * | 1976-08-27 | 1983-05-05 | Mitsubishi Denki K.K., Tokyo | Verfahren zum Lichtbogen-Verbindungsschweißen |
US4534793A (en) | 1979-09-19 | 1985-08-13 | Research Corporation | Cast iron welding materials and method |
US4624706A (en) * | 1985-07-02 | 1986-11-25 | Inco Alloys International, Inc. | Weld wire from extruded nickel containing powder |
US5242759A (en) * | 1991-05-21 | 1993-09-07 | Cook Incorporated | Joint, a laminate, and a method of preparing a nickel-titanium alloy member surface for bonding to another layer of metal |
FR2742368B1 (fr) * | 1995-12-18 | 1998-03-06 | Framatome Sa | Procede de raccordement par soudage heterogene bout a bout de deux pieces de natures differentes et utilisations |
FR2742369B1 (fr) | 1995-12-18 | 1998-03-06 | Framatome Sa | Procede de raccordement par soudage heterogene de deux pieces et utilisation |
US5915743A (en) | 1997-06-30 | 1999-06-29 | The Boeing Company | Metal spray tool repair system |
US6335512B1 (en) * | 1999-07-13 | 2002-01-01 | General Electric Company | X-ray device comprising a crack resistant weld |
US6308882B1 (en) * | 1999-09-13 | 2001-10-30 | Dana Corporation | Method for joining ductile iron and steel |
-
2001
- 2001-05-29 US US09/866,258 patent/US6730876B2/en not_active Expired - Lifetime
-
2002
- 2002-05-29 JP JP2002593092A patent/JP2004527381A/ja active Pending
- 2002-05-29 DE DE60235804T patent/DE60235804D1/de not_active Expired - Lifetime
- 2002-05-29 WO PCT/US2002/016813 patent/WO2002096590A1/en active Application Filing
- 2002-05-29 AT AT02737228T patent/ATE462523T1/de not_active IP Right Cessation
- 2002-05-29 EP EP02737228A patent/EP1390173B1/de not_active Expired - Lifetime
Also Published As
Publication number | Publication date |
---|---|
EP1390173A4 (de) | 2008-02-27 |
WO2002096590A1 (en) | 2002-12-05 |
EP1390173A1 (de) | 2004-02-25 |
US6730876B2 (en) | 2004-05-04 |
ATE462523T1 (de) | 2010-04-15 |
EP1390173B1 (de) | 2010-03-31 |
JP2004527381A (ja) | 2004-09-09 |
US20020179583A1 (en) | 2002-12-05 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US9821401B2 (en) | High toughness weld metals with superior ductile tearing resistance | |
JP4800628B2 (ja) | フェライト鋼のレーザー/アークハイブリッド溶接方法 | |
US20180169799A1 (en) | High Strength Weld Metal for Demanding Structural Applications | |
DeRuntz | Assessing the benefits of surface tension transfer® welding to industry | |
EP2911825B1 (de) | Zusammengesetzter schweissdraht und verfahren zur herstellung | |
Costanza et al. | Weldability of austenitic stainless steel by metal arc welding with different shielding gas | |
MX2013000376A (es) | Metodo de soldeo hibrido con arco electrico/laser para partes de acero aluminizado utilizando elementos gammagenos y un gas que contiene mendo del 10% de nitrogeno u oxigeno. | |
Torbati et al. | Optimization procedures for GMAW of bimetal pipes | |
US20070108174A1 (en) | Gas-less process and system for girth welding in high strength applications | |
Kumar et al. | Experimental investigation and optimization of TIG welding parameters on aluminum 6061 alloy using firefly algorithm | |
CN112171016A (zh) | 一种奥氏体不锈钢nbg焊接工艺 | |
DE60235804D1 (de) | Verfahren zum schweissen zwei werkstücke aus duktilem eisen zur herstellung einer hochduktilen, fehlerreduzierten schweissnaht | |
Ikram et al. | Investigation of single pass welding of thick AH36 steel plates in a square groove butt joint configuration during AC-GMAW | |
JP2016526486A (ja) | 厚肉ワークピースにおける高破壊靱性の溶接部 | |
KR20140010107A (ko) | 니켈 함량이 높은 강철의 용접용 플럭스-코어드 와이어 | |
JP2008000808A (ja) | 低温靭性、耐低温割れ性、および全姿勢溶接時のビード形状が良好な高強度溶接金属 | |
Maruyama | Arc welding technology for dissimilar joints | |
CN108213661A (zh) | 一种机器人双丝垂直立焊高强钢构件的焊接方法 | |
JPH03281089A (ja) | 高降伏強さ用改良溶着合金およびその溶着方法 | |
JP2006026651A (ja) | ステンレス鋼溶接用シールドガス | |
Houldcroft | Welding process developments and future trends | |
US20090212023A1 (en) | Welding Processes | |
US20230405707A1 (en) | Laser additive manufacturing and welding with hydrogen shield gas | |
Muniraju et al. | Litrature survey on on gas metal arc welding process | |
Singh et al. | Study Different Graded Electrode’s Influence Over Tensile Strength Of Tig Welded 5083 Al-Alloy |
Legal Events