DE475242C - Process for the production of accumulator plates - Google Patents

Process for the production of accumulator plates

Info

Publication number
DE475242C
DE475242C DEI31296D DEI0031296D DE475242C DE 475242 C DE475242 C DE 475242C DE I31296 D DEI31296 D DE I31296D DE I0031296 D DEI0031296 D DE I0031296D DE 475242 C DE475242 C DE 475242C
Authority
DE
Germany
Prior art keywords
production
lead
plates
accumulator plates
accumulator
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DEI31296D
Other languages
German (de)
Inventor
Dr Georg Kraenglein
Dr Richard Karl Mueller
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
IG Farbenindustrie AG
Original Assignee
IG Farbenindustrie AG
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by IG Farbenindustrie AG filed Critical IG Farbenindustrie AG
Priority to DEI31296D priority Critical patent/DE475242C/en
Application granted granted Critical
Publication of DE475242C publication Critical patent/DE475242C/en
Expired legal-status Critical Current

Description

Verfahren zur Herstellung von Akkumulatorenplatten Die elektrolytische Zerlegung von Bleilegierungen zu porösen Bleiniassen ist bek-annt. Derartighergestellte Elektroden haben jedochkeinenEingang in. diePraxils gefunden.Process for the production of accumulator plates The electrolytic It is well known that lead alloys are broken down into porous lead compounds. Manufactured in this way However, electrodes have not found entry into the practice.

Wie festgestellt wurde, sind s#e praktisch wenig brauchbar, weil sie ungenügende Kapazität und nur geringe Haltbarkeit besitzen und sie sich schon während des Herauslösens des Begleitmetalls deformieren.As has been established, they are of little practical use because they have insufficient capacity and only a short shelf life and they are already during deform the removal of the accompanying metal.

Es wurde nun gefunden, daß Bleile gierungen, welche beispielsweise in ihrer Plattenfo,rm ein Bleigitter bzw. Bleiskelett enthalten, bei der Elektrolyse nicht nur zu wertvollen Kathoden, sondern auch über die Bildun 'g von po-rösem Blei hinaus zu wert vollen Anoden formiert werden können, wenn dafür gesargt wird, daß während der Elektro lyse keine zu hohe Konzentration z. B. an Natriumsulfat entsteht und stets ein gewissier Überschuß an Säure vorhanden ist. Als sehr #iinstig hat sich zudem !eine Stromstärke von etwa 1,2 Amp. pro Quadratdezimeter Oberflaklie. eine Schwefelsäurekonzentration vom spez. Gew. i,io und die Arbeitsweise bei gewöhnlicher Temperatur erwiesen. Arbeitet man dagegen in starken Konzentrationen und mit #,tarken Stromdichten, so findet ein teilweises Herausbröckeln der aktiven Masse statt, und die Elektroden werden minderwertig und unbrauchbar.It has now been found that Bleile governments, which for example in their Plattenfo, rm contain a lead grids or lead skeleton, in electrolysis not only valuable cathode, but also about the Bildun 'g of po-rösem lead out to value full anodes formed can be if it is cured that no too high concentration z. B. sodium sulfate is formed and there is always a certain excess of acid present. A current of around 1.2 amps per square decimeter of surface area has also proven to be very cheap. a sulfuric acid concentration of the spec. Gew. I, io and the operation at ordinary temperature proved. If, on the other hand, one works in strong concentrations and with strong current densities, the active material will partially crumble out, and the electrodes will be inferior and unusable.

Claims (1)

PA T E NI'A N S PR ( 1 CM : Verfahren zur Herstellung von Akku mulatorenplatten aus Blei-Bleileglerungs-Metallen, dadurch gekennzeichnet, daß die Platten in saurer Lösung durch Elektrolyse vom Biegleitmeiall befreit und bei der Hierstel, lung positiver Platten gleichzeitig zu Bleisuperoxyd weiter oxydiert werdenPA T E NI'A N S PR (1 CM: Process for the production of accumulator plates made of lead-lead alloying metals, characterized in that the plates are freed from flexible metal by electrolysis in an acid solution and positive plates are added at the same time Lead peroxide can be further oxidized
DEI31296D 1927-05-25 1927-05-25 Process for the production of accumulator plates Expired DE475242C (en)