DE3475032D1 - Plastic-bonded cadmium electrode - Google Patents

Plastic-bonded cadmium electrode

Info

Publication number
DE3475032D1
DE3475032D1 DE8484402749T DE3475032T DE3475032D1 DE 3475032 D1 DE3475032 D1 DE 3475032D1 DE 8484402749 T DE8484402749 T DE 8484402749T DE 3475032 T DE3475032 T DE 3475032T DE 3475032 D1 DE3475032 D1 DE 3475032D1
Authority
DE
Germany
Prior art keywords
plastic
cadmium electrode
paste
network
electrode
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DE8484402749T
Other languages
German (de)
Inventor
Denis Doniat
Bernard Bugnet
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Societe de Recherches et dApplications Electronchimiques SORAPEC SA
SORAPEC SA
Original Assignee
Societe de Recherches et dApplications Electronchimiques SORAPEC SA
SORAPEC SA
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Societe de Recherches et dApplications Electronchimiques SORAPEC SA, SORAPEC SA filed Critical Societe de Recherches et dApplications Electronchimiques SORAPEC SA
Priority claimed from EP84402749A external-priority patent/EP0185830B2/en
Application granted granted Critical
Publication of DE3475032D1 publication Critical patent/DE3475032D1/en
Expired legal-status Critical Current

Abstract

Plastified Cd electrode for electrochemical generator is mfd. by applying a paste through its complete thickness to a metallic network structure with completely open porosity. The network consists at least superficially of Ni and is 0.5-3 mm. thick. The pore dia. is about 0.7-0.8 mm. The active material introduced into the matrix network is a paste comprising CdO and a plastifier, esp. Teflon (RTM) (PTFE) and an alcohol as diluent.
DE8484402749T 1984-12-28 1984-12-28 Plastic-bonded cadmium electrode Expired DE3475032D1 (en)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
EP84402749A EP0185830B2 (en) 1983-06-29 1984-12-28 Plastic-bonded cadmium electrode

Publications (1)

Publication Number Publication Date
DE3475032D1 true DE3475032D1 (en) 1988-12-08

Family

ID=8192938

Family Applications (1)

Application Number Title Priority Date Filing Date
DE8484402749T Expired DE3475032D1 (en) 1984-12-28 1984-12-28 Plastic-bonded cadmium electrode

Country Status (1)

Country Link
DE (1) DE3475032D1 (en)

Similar Documents

Publication Publication Date Title
DE3277667D1 (en) Method of manufacturing thin electrodes, particularly gas electrodes, for electrochemical devices, and thin electrodes obtained by such a method, the electrodes possibly being provided with current collectors
DE3071723D1 (en) Thin carbon-cloth-based electrocatalytic gas diffusion electrodes, processes, and electrochemical cells comprising the same
FR2430100B1 (en)
GB1524379A (en) Precisely-structured electrochemical cell electrode and method of making same
EP0003851A3 (en) A porous, electrolyte permeable composite diaphragm, electrolytic cell comprising said diaphragm, electrolytic process using said diaphragm and a process for the preparation of said diaphragm
JPS5770448A (en) Enzyme electrode
CA2098606A1 (en) Efficiency enhancement for solid-electrolyte fuel cell
DE3475032D1 (en) Plastic-bonded cadmium electrode
CA1251515A (en) Chromatography system comprising electrode coated with permeable membrane
ES296350U (en) Membrane unit for electrolytic cell.
JPS5616863A (en) Electrode unit
JPS52119579A (en) Method of discharging electrode for electric dust-collector device
DE3063086D1 (en) Process for the production of potassium hydroxide in an electrolytic membrane cell and potassium hydroxide obtained thereby
AU573356B2 (en) Trough electrolysis cell with horizontally disposed electrodes
JPS5535461A (en) Gas diffusing electrode
JPS56102076A (en) Electrode
JPS5711473A (en) Battery
JPS53120783A (en) Preparation of porous material
NL7800522A (en) MEMBRANE FOR AN ELECTROCHEMICAL CELL AND ELECTROLYSIS CELL WITH SUCH MEMBRANE.
JPS56130082A (en) Organic solvent battery
JPS57162259A (en) Pasted lead battery
JPS5411080A (en) Separating support
JPS5679225A (en) Structure of differential pressure gauge
JPS5593672A (en) Manufacturing method of positive electrode active substance for cell
JPS5591566A (en) Manufacture of flat-type cell

Legal Events

Date Code Title Description
8363 Opposition against the patent
8328 Change in the person/name/address of the agent

Free format text: HOFFMEISTER, H., DIPL.-PHYS. DR.RER.NAT., PAT.-ANW., 4400 MUENSTER

8366 Restricted maintained after opposition proceedings
8339 Ceased/non-payment of the annual fee