CN85106524A - 一种含有腐植酸的新型钻井泥浆处理剂及制备方法 - Google Patents

一种含有腐植酸的新型钻井泥浆处理剂及制备方法 Download PDF

Info

Publication number
CN85106524A
CN85106524A CN 85106524 CN85106524A CN85106524A CN 85106524 A CN85106524 A CN 85106524A CN 85106524 CN85106524 CN 85106524 CN 85106524 A CN85106524 A CN 85106524A CN 85106524 A CN85106524 A CN 85106524A
Authority
CN
China
Prior art keywords
sulfonated
mud
sulfomethylation
sodium
pheno
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN 85106524
Other languages
English (en)
Other versions
CN85106524B (zh
Inventor
杨正宇
刘康德
张德和
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Institute of Chemistry CAS
Original Assignee
Institute of Chemistry CAS
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Institute of Chemistry CAS filed Critical Institute of Chemistry CAS
Priority to CN 85106524 priority Critical patent/CN85106524B/zh
Publication of CN85106524A publication Critical patent/CN85106524A/zh
Publication of CN85106524B publication Critical patent/CN85106524B/zh
Expired legal-status Critical Current

Abstract

一种用高聚物加以改性的腐植酸类钻井泥浆处理剂。该处理剂是由磺甲基酚醛树脂、磺甲基水解聚丙烯腈以及磺甲基腐植酸钠或磺化腐植酸钠所组成。采用简便的制备工艺而不需单独制备上述各个磺甲基化的组份。
加入该处理剂后的一般土泥浆具有耐温、抗盐、抗钙、降失水的特性,尤其在加重泥浆中它的降粘、降静切力效果更显著,适用于深井、超深井、热井和海上油井。

Description

本发明属于一种用高聚物加以改性的腐植酸类钻井泥浆处理剂的开发和制备工艺。
泥浆处理剂是钻井工艺中不可缺少的重要组成部份。尤其是同时具有耐高温、抗盐、抗钙、降失水、降粘和降静切力等多种功能的处理剂更为需要。
现有的一种优质泥浆处理剂SCSP是由磺化酚醛树脂和磺化褐煤缩合而成〔1〕。用SCSP所配制的泥浆有较好的耐温性能,但它的抗盐、抗钙能力欠佳。美国MAGCOBAR公司生产的RESINEX是由50%的磺化褐煤和50%的磺甲基酚醛树脂所组成〔2〕。RESINEX是一种耐温抗盐的降失水剂,并具有在高比重泥浆中起着控制失水而不增大泥浆粘度的特殊作用。但该处理剂用于白土(中国、昆山石油器材供应公司经销的改性钠
Figure 85106524_IMG1
土)和安丘土(中国、山东安丘土)配制成的泥浆,经高温老化后的中压失水和高温高压失水仍不理想,它的降粘和降静切力的功能也不明显。
还有一些专利和专著中〔3-7〕曾述及到用磺甲基酚醛树脂、磺化褐煤和水解聚丙烯腈可单独用作泥浆处理剂。
已有的含有磺甲基酚醛树脂成份的处理剂,其中磺甲基酚醛树脂的合成都是按常规的较复杂的合成工艺单独制备的。
本发明的目的是制备出一种多功能的泥浆处理剂。该处理剂具有耐高温、抗盐、抗钙、降失水的优越性能,尤其在高比重泥浆中有降粘及降静切力的特性,可在深井、超深井、热井和海上钻井中使用。
本发明的第二个目的是采用简单的工艺制备含有磺甲基酚醛树脂成份的泥浆处理剂。
本发明是一种含有磺甲基水解聚丙烯腈、磺甲基酚醛树脂和磺甲基腐植酸钠或磺化腐植酸钠和磺甲基腐植酸钠组合物的钻井泥浆处理剂。
其中各自的组份(重量)为:
磺甲基腐植酸钠或磺化腐植酸钠和磺甲基腐植酸钠    0.40-0.75
磺甲基酚醛树脂    0.20-0.55
磺甲基水解聚丙烯腈    0.025-0.50
不同的配比得到的产品性能有所差别。
其制备方法是首先用常规方法从含有腐植酸的泥炭或风化煤或褐煤制取出腐植酸钠。再在100-145℃温度范围内采用一步法制备出磺甲基水解聚丙烯腈、磺甲基酚醛树脂和磺甲基腐植酸钠,并同时组合制得产品,或在100-145℃温度范围内在磺化腐植酸钠存在下采用一步法制备出磺甲基水解聚丙烯腈、磺甲基酚醛树脂和磺甲基腐植酸钠,并同时组合制得产品。磺甲基化反应和组合的时间为1-5小时。
本发明的泥浆处理剂同RESINEX所配制的白土泥浆在相同的条件下用API标准法进行测定和对比,前者的主要性能都优于RESINEX。本发明配制的淡水泥浆经过150℃老化16小时后,测得的中压失水量为RESINEX的63%;高温高压失水量为RESINEX的64%。在饱和盐水条件下经150℃老化16小时后测得的高温高压失水量为RESINEX的72%。经过200℃老化16小时后的高温高压失水量为RESINEX的90%。在加入2%氯化钙的情况下经过200℃老化16小时后测得高温高压失水量为RESINEX的96%。此外,本发明的产品在高
Figure 85106524_IMG2
土的重泥浆中(含有10%的安丘土)还具有降粘、 降静切力的特点,初切力为RESINEX的20%,终切力为RESINEX的35%。这对于打深井或超深井是十分有利的。
本发明所制成的产品经中国华北油田第二勘探公司泥浆站配成含6%安丘土的加重泥浆(比重=1.30)后测得的主要性能指标如下:
Figure 85106524_IMG3
比重(单位:克/厘米3);API=中压失水量(毫升);AV=表观粘度(厘泊);PV=塑性粘度(厘泊);范氏切力(达因/厘米2);HTHP=高温高压失水量(毫升)
**150℃,35大气压测30分钟的失水量
实施例1
用常规的方法从泥炭或风化煤或褐煤制取出腐植酸钠备用。
取腐植酸钠20克、水100毫升、亚硫酸钠12克、水解聚丙烯腈1.1克、苯酚11克、甲醛(36%水溶液)12.7克一次加入反应器内,在100℃加热4小时,蒸去水份得到干燥的产品。
实施例2
取腐植酸钠20克、水100毫升、亚硫酸钠3.5克、亚硫酸氢钠4克、水解聚丙烯腈2.0克、甲醛(36%水溶液)12克、苯酚 6克一次加入反应器中,在130-140℃加热1-4小时,蒸去水份得到干燥的产品。
实施例3
取腐植酸钠20克,加水200毫升、亚硫酸钠4克,加热迴流20分钟以上,再加入亚硫酸钠6克、甲醛(36%水溶液)11.2克、水解聚丙烯腈2.0克、苯酚9克,在100-130℃加热3-5小时,蒸去水份得到干燥的产品。
参考资料
(1)重庆合成化工厂产品说明书
(2)黄汉仁,杨坤鹏,罗平亚编“泥浆工艺原理”,石油工业出版社,(1981)。
(3)捷克专利187,164
(4)英国专利1,363,871
(5)美国专利3,956,140
(6)G.R.Gray    and    H.C.H.Darley,"Composition    and    Properties    of    Oil    Well    Drilling    Fluid",4th    Ed.(1982)
(7)J.McDermott,"Drilling    Mud    and    Fluid    Additives",(1973)
(8)中原石油勘探局泥浆公司科研所测试报告(1985)。

Claims (3)

1、一种含有磺甲基酚醛树脂和磺甲基腐植酸钠或磺化腐植酸钠的钻井泥浆处理剂,其特征在于含有磺甲基水解聚丙烯腈。
2、按权利要求1所说的处理剂,其特征在于各组份的含量(重量)为:
磺甲基酚醛树脂  0.20-0.55
磺甲基腐植酸钠或磺甲基腐植酸钠  0.40-0.75
和磺化腐植酸钠的混合体
磺甲基水解聚丙烯腈  0.025-0.50
3、一种制备权利要求1所说的泥浆处理剂的方法,其特征在于用一步法制得磺甲基酚醛树脂、磺甲基腐植酸钠或磺甲基腐植酸钠和磺化腐植酸钠的混合体、磺甲基水解聚丙烯腈并同时进行组合,磺甲基反应及组合条件是100-145℃,1-5小时。
CN 85106524 1985-08-31 1985-08-31 一种含有腐植酸的新型钻井泥浆处理剂及制备方法 Expired CN85106524B (zh)