CN2804537Y - 外镀锌管 - Google Patents

外镀锌管 Download PDF

Info

Publication number
CN2804537Y
CN2804537Y CN 200520025218 CN200520025218U CN2804537Y CN 2804537 Y CN2804537 Y CN 2804537Y CN 200520025218 CN200520025218 CN 200520025218 CN 200520025218 U CN200520025218 U CN 200520025218U CN 2804537 Y CN2804537 Y CN 2804537Y
Authority
CN
China
Prior art keywords
utility
model
zinc
pipe
wall
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200520025218
Other languages
English (en)
Inventor
左树清
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200520025218 priority Critical patent/CN2804537Y/zh
Application granted granted Critical
Publication of CN2804537Y publication Critical patent/CN2804537Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种简便,价格低廉的外镀锌管。本实用新型外镀锌管,包括管体外壁和管体内壁,在所述管体外壁设置一层镀锌层。本实用新型管体仅设置外壁镀锌层,可以有效的节约资源,大幅降低成本;本实用新型可用于制作各种自来水管线,煤气管线或其它管线附件。

Description

外镀锌管
技术领域
本实用新型属于一种流体输送管线及其管线制品,可用于制作各种自来水管线,煤气管线或其它管线附件。
背景技术
现在自来水管和管道煤气管或各种流体输送管线,为了防腐多采用外表面和内表面镀锌处理,以此延长管子的使用寿命,然而由于自来水中存在着杂质特别是工业用水中大量的存在着含酸性的物质,以及煤气中合有的大量硫化物质对管内壁的腐蚀相当严重,以至镀锌管的内镀锌仍抵挡不住这些杂质的腐蚀,所以现在的各种管道往往出现蚀穿现象都是因管内壁腐蚀所造成的,而且管内壁的腐蚀极易造成饮用自来水的二次污染,影响人体的身体健康;内壁易生锈、易滋生细菌和微生物等有害杂质,容易堆积水垢、使水流堵塞;当镀锌层接触水分后,会因化学反应而产生一层白锈(白浊),对人体十分有害;最使人担忧的是,自来水在管道输送中容易被“二次污染”,所以现在很多厂家加强对管内壁的防腐处理。可是在内壁镀锌层上再次做防腐处理不仅易造成防腐层的剥落,而且也造成锌资源的浪费,达不到延长管子使用寿命的目的。
实用新型内容
本实用新型的所要解决的技术问题是克服现有技术中存在的不足,提供一种简便,价格低廉的外镀锌管。
本实用新型外镀锌管,通过以下技术方案予以实现,包括管体外壁和管体内壁,在所述管体外壁设置一层镀锌层。
本实用新型所述管体内壁设置有涂塑防腐层,管体涂塑防腐层为改性环氧树脂粉末。
本实用新型所述管体内壁设置有衬塑防腐层,管体涂塑防腐层为热溶胶的聚乙烯。
本实用新型与现有技术相比较具有如下有益效果:
1.管体仅设置外壁镀锌层,可以有效的节约资源,相同管体节约锌原料近三分之二的用量,从而降低了产品的成本。
2.管体内壁不设置镀锌层,不仅可以降低成本,而且可以增加后续进行防腐处理层的附着力。现有技术中内镀锌层的存在在很大程度上影响后续防腐处理层的附着,使防腐层容易剥落,从而影响管体的使用寿命。
附图说明
图1是本实用新型剖面结构示意图。
具体实施方式
下面结合附图对本实用新型做进一步描述。
如图1所示,管体包括管体外壁1和管体内壁2,在管体外壁上设置一层镀锌层3,根据不同使用场所的需要,本实用新型还可以在管体内壁设置防腐层。其中防腐层可采用涂塑防腐层,即使用改性环氧树脂粉末;也可以采用衬塑防腐层,即使用热溶胶的聚乙烯。
现有热镀锌钢管生产工艺流程基本如下:1.除锈,即将待镀锌的钢管浸泡于一定浓度的酸溶液中一段时间,以清除钢管内外表面的锈蚀;2.清洗,即以清水将钢管上的酸溶液清洗干净;3.沾药液,即将清洗后的钢管浸泡在氯化锌溶剂中一定时间,让溶剂通过和铁反应粘附在管壁上;4.烘干,将沾好药液的钢管表面的水分子去除;5.镀锌,即将经前述工序处理后的钢管置于一定温度的锌液中一定时间,将锌镀在钢管的内外表面上;6.外吹,即用压缩空气将钢管外表面的残留锌液及浮物吹干净:7.内吹,用压缩空气将管子内表面的残留锌液及浮物吹干净;8.冷却,将镀好锌的钢管置于冷却水槽中冷至常温。为实现本实用新型可采用在除锈、清洗,即在酸洗和水洗工序前将管体密封,保证内管壁不接触任何溶液,然后在沾药液(浸溶液)工序后再将密封解除,最后得到本实用新型。

Claims (3)

1.一种外镀锌管,包括管体外壁和管体内壁,其特征是,在所述管体外壁设置一层镀锌层。
2.根据权利要求1所述的外镀锌管,其特征是,所述管体内壁设置有涂塑防腐层。
3.根据权利要求1所述的外镀锌管,其特征是,所述管体内壁设置有衬塑防腐层。
CN 200520025218 2005-01-28 2005-01-28 外镀锌管 Expired - Fee Related CN2804537Y (zh)