CN2751943Y CN 200420075339 CN200420075339U CN2751943Y CN 2751943 Y CN2751943 Y CN 2751943Y CN 200420075339 CN200420075339 CN 200420075339 CN 200420075339 U CN200420075339 U CN 200420075339U CN 2751943 Y CN2751943 Y CN 2751943Y
Authority
CN
China
Prior art keywords
ball
utility
model
mould
abrading
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200420075339
Other languages
English (en)
Inventor
郭建华
冯祖兴
姚志国
李华
Original Assignee
郭建华
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 郭建华 filed Critical 郭建华
Priority to CN 200420075339 priority Critical patent/CN2751943Y/zh
Application granted granted Critical
Publication of CN2751943Y publication Critical patent/CN2751943Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Milling Processes (AREA)

Abstract

一种等温冷却相型磨球模具,它包括相互扣合的上、下模具本体(1)、(2),所述上、下模具本体(1)、(2)为水平分型结构,环绕其铸造浇道(3)至少设置有四个磨球浇铸型腔(4);所述磨球浇铸型腔(4)的腔壁厚度为均厚结构,且其厚度大于等于磨球浇铸型腔(4)直径的四分之一。由于本实用新型的模具在保证一定保温厚度的前提下采用了等壁厚技术措施,从而确保了金属铸液在成球过程中冷却速度的均匀,这就使得铸造出的磨球的质密度和表面硬度一致性。另外,由于本实用新型的模具从成球原理上更加符合自然规律,相比现有技术更加合理,并可使磨具的使用寿命得以延长,减轻劳动强度,改善工作环境,因此在同等条件下,可使其生产效率、成品率得以大幅度提高。

Description

等温冷却相型磨球模具
(一)技术领域
本实用新型涉及冶金矿山球磨机、建材(水泥)磨机、热电厂磨煤磨机用磨球的生产模具,具体说是涉及一种等温冷却相型磨球模具。
(二)背景技术
冶金矿山用球磨机、水泥建材、电厂等行业用磨机中的磨球多是采用铸造成型的方法制造而成,其形状多为圆形、椭圆形或水滴型等。由于现有技术中的磨球铸造模具中环绕磨球浇铸型腔的腔壁厚度不均,在磨球浇注过程中直接影响到金属浇注液冷却、收缩速度一致性,并会使得金属磨球在成型过程中的冷激效果不同,导致其金属磨球表面硬度、质密度的不同,增加了金属磨球后处理难度,使成品金属磨球的使用寿命降低、生产成本上升、难以适应现在冶金矿山等行业的需要。
(三)发明内容
本实用新型的目的就在于克服上述现有技术中所存在的不足之处而提供一种结构更为合理、且结构简单、制造方便、成品率高的等温冷却相型磨球模具。
本实用新型的目的可通过下述措施来实现:
本实用新型的等温冷却相型磨球模具包括相互扣合的上下模具本体,所述上下模具本体为水平分型结构,环绕其铸造浇道至少设置有四个磨球浇铸型腔;所述磨球浇铸型腔的腔壁厚度为均厚结构,且其厚度大于等于磨球浇铸型腔直径的四分之一。
本实用新型环绕其铸造浇道以均布的方式设置有六个磨球浇铸型腔;在实际生产中可根据具体生产条件将其磨球浇铸型腔设计成八个。
本实用新型与现有技术相比具有以下特点:
1、由于本实用新型的模具在保证一定保温厚度的前提下采用了等壁厚技术措施,从而确保了金属铸液在成球过程中冷却速度的均匀,这就使得铸造出的同等材料的磨球的质密度和表面硬度一致性。
2、由于本实用新型的模具从成球原理上更加符合自然规律,相比现有技术更加合理,并可使磨具的使用寿命得以延长,减轻工人劳动强度,改善工作环境,且在同等条件下,可使其生产效率、成品率得以大幅度提高。
(四)附图说明
图1是本实用新型的主剖图。
图2是下模的俯视图。
(五)具体实施方式
本实用新型以下将结合实施例(附图)作进一步描述:
如图1、2所示,本实用新型的等温冷却相型磨球模具包括相互扣合的上下模具本体1和2,所述上下模具本体1和2为水平分型结构,环绕其铸造浇道3设置有六个磨球浇铸型腔4;所述磨球浇铸型腔4的腔壁厚度为均厚结构,且其厚度大于等于磨球浇铸型腔4直径的四分之一。

Claims (2)

1、一种等温冷却相型磨球模具,它包括相互扣合的上、下模具本体(1)、(2),其特征在于:所述上、下模具本体(1)、(2)为水平分型结构,环绕其铸造浇道(3)至少设置有四个磨球浇铸型腔(4);所述磨球浇铸型腔(4)的腔壁厚度为均厚结构,且其厚度大于等于磨球浇铸型腔(4)直径的四分之一。
2、根据权利要求1所述的等温冷却相型磨球模具,其特征在于:环绕其铸造浇道(3)以均布的方式设置有六个磨球浇铸型腔(4)。
CN 200420075339 2004-12-08 2004-12-08 等温冷却相型磨球模具 Expired - Fee Related CN2751943Y (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 200420075339 CN2751943Y (zh) 2004-12-08 2004-12-08 等温冷却相型磨球模具

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 200420075339 CN2751943Y (zh) 2004-12-08 2004-12-08 等温冷却相型磨球模具

Publications (1)

Publication Number Publication Date
CN2751943Y true CN2751943Y (zh) 2006-01-18

Family

ID=35913359

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 200420075339 Expired - Fee Related CN2751943Y (zh) 2004-12-08 2004-12-08 等温冷却相型磨球模具

Country Status (1)

Country Link
CN (1) CN2751943Y (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110814296A (zh) * 2019-11-18 2020-02-21 安徽省宁国市宁沪钢球有限公司 一种用于铸造磨球的快速冷却式模具

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110814296A (zh) * 2019-11-18 2020-02-21 安徽省宁国市宁沪钢球有限公司 一种用于铸造磨球的快速冷却式模具

Similar Documents

Publication Publication Date Title
CN207480859U (zh) 石墨坩埚静压烧结易脱模模具
CN2751943Y (zh) 等温冷却相型磨球模具
CN206780770U (zh) 一种塑料模具冷却装置
CN209189634U (zh) 一种冷作钣金加工用模具
CN208408592U (zh) 一种便于清洁冷却液的冲钻模具
CN204381339U (zh) 真空铸造冰箱内胆模具用上箱
CN201940571U (zh) 新型金属液引流槽
CN208680184U (zh) 一种桥梁支座板的成形装置
CN2723161Y (zh) 围棋制坯成型冲模
CN206779463U (zh) 一种分解式加压烧结用石墨模具
CN204711147U (zh) 一种气压式压铸模具
CN206633317U (zh) 一种分型面分类加工的注塑模具
CN2392626Y (zh) 一种金属球的铸造模具
CN211333780U (zh) 人造金刚石生产用坩埚压制模具
CN208322010U (zh) 一种不锈钢餐台底盘模具
CN202387835U (zh) 一种新型模具
CN216226526U (zh) 一种模具冲头的冷却结构
CN204486493U (zh) 一种锌基合金挤压模具
CN203804156U (zh) 一种制作工字钢的模具
CN209832759U (zh) 一种具有冷却效果好的模具
CN211248223U (zh) 一种耐磨损铜套铸造模具
CN213729270U (zh) 一种汽车配件加工用铸造模具
CN204584266U (zh) 一种用于粉末冶金件产品的阴模
CN219074298U (zh) 一种湿型砂铸造用缸盖浇注系统
CN213918827U (zh) 一种可以快速成形且脱模方便的方形石墨坩埚用成形模具

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C19 Lapse of patent right due to non-payment of the annual fee
CF01 Termination of patent right due to non-payment of annual fee