CN2618025Y - 环保型复合钢铜管 - Google Patents

环保型复合钢铜管 Download PDF

Info

Publication number
CN2618025Y
CN2618025Y CN 03234396 CN03234396U CN2618025Y CN 2618025 Y CN2618025 Y CN 2618025Y CN 03234396 CN03234396 CN 03234396 CN 03234396 U CN03234396 U CN 03234396U CN 2618025 Y CN2618025 Y CN 2618025Y
Authority
CN
China
Prior art keywords
utility
model
copper pipe
poor
performance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 03234396
Other languages
English (en)
Inventor
岳成平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CHENGDU DITUO PIPE SCIENCE AND TECHNOLOGY DEVELOPMENT Co Ltd
Original Assignee
CHENGDU DITUO PIPE SCIENCE AND TECHNOLOGY DEVELOPMENT Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHENGDU DITUO PIPE SCIENCE AND TECHNOLOGY DEVELOPMENT Co Ltd filed Critical CHENGDU DITUO PIPE SCIENCE AND TECHNOLOGY DEVELOPMENT Co Ltd
Priority to CN 03234396 priority Critical patent/CN2618025Y/zh
Application granted granted Critical
Publication of CN2618025Y publication Critical patent/CN2618025Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种民用建筑管材,确切的说是一种环保型复合钢铜管,旨在克服现有环保型管材存在的耐温性能差、刚度低、穿墙、暗埋性能差等缺陷。本实用新型采用作为内层的铜管(1)与作为外层的碳素钢管(2)经紧密复合而成。本实用新型由于采用以上结构,因此具有其耐压强度高,耐温性能好,无着火隐患,在-50℃~450℃范围内可长期稳定工作,其穿墙、暗埋性能均可靠、无水污染等突出优点。

Description

环保型复合钢铜管
技术领域
本实用新型涉及一种民用建筑管材,确切的说是一种环保型复合钢铜管。
背景技术
随着人们对生活用水品质要求的提高,在建筑业迫切需要一种管水不被污染的环保型管材,镀锌有缝钢管被禁止使用后,铝塑复合管、钢塑复合管以纯塑料管相继涌入市场。这些作为环保型产品还不尽人意,主要问题是耐温性能较差,铝塑管、纯塑料管由于刚度低,其穿墙、暗埋性能差,在实际应用中达不到满意的效果。
发明内容
本实用新型旨在克服现有环保型管材存在的上述缺陷,提供一种耐压强度高、耐温性能好,放火、穿墙、暗埋可靠、无污染、成本低的环保型复合钢铜管。
为解决上述技术问题,本实用新型采用的技术方案如下:
一种环保型复合钢铜管,其特征在于:包括碳素钢管层和与其紧密复合的铜管层。
所述钢铜管,其内层为铜管,紧密复合的外层为碳素钢管。
所述钢铜管口径为15~300mm;铜管壁厚为0.3~1mm,碳素钢管壁厚为1~3mm。
本实用新型由于采用以上结构,使其具有如下优点:
由于复合管内外层采用铜管和钢管配合,因此其耐压强度高,耐温性能好,无着火隐患,在-50℃~450℃范围内可长期稳定工作,其穿墙、暗埋性能均可靠,这是铝塑管、钢塑管、纯塑料管无法比拟的。
附图说明
图1为本实用新型结构及管材制作方法示意图
图中标记:1、铜管层,2、碳素钢管层,3为拉挤机缩径口环
具体实施方式
本实用新型采用作为内层的铜管1与作为外层的碳素钢管2,经紧密复合而成。
本实用新型可按如下方法制造:将检验合格的铜管1套装在碳素钢管2内,放在拉挤机工作位上,管子在拉挤机的牵引下,被机上的缩径口环3约束,强制性地将外层碳素钢管2的直径缩小,不但使其内层铜管1与外层碳素钢管2的初始套管间隙消失,还要使他们产生过盈配合,致使外层碳素钢管2与内层铜管1牢固地结合成一个整体。
本实用新型可制作口径15~300mm的薄壁复合钢铜管;铜管1壁厚为0.3~1mm,碳素钢管2壁厚为1~3mm,耐压强度:2.5Mpa,耐温性:-50℃~450℃,使用寿命为25年以上。

Claims (4)

1、一种环保型复合钢铜管,其特征在于:包括碳素钢管层(2)和与其紧密复合的铜管层(1)。
2、根据权利要求1所述的一种环保型复合钢铜管,其特征在于:其内层为铜管(1),紧密复合的外层为碳素钢管(2)。
3、根据权利要求1或2所述的一种环保型复合钢铜管,其特征在于:该钢铜管口径为15~300mm。
4、根据权利要求3所述的一种环保型复合钢铜管,其特征在于:铜管(1)壁厚为0.3~1mm,碳素钢管(2)壁厚为1~3mm。
CN 03234396 2003-05-16 2003-05-16 环保型复合钢铜管 Expired - Fee Related CN2618025Y (zh)