CN2541703Y - 镀有强化金属层的铜管 - Google Patents

镀有强化金属层的铜管 Download PDF

Info

Publication number
CN2541703Y
CN2541703Y CN 02232179 CN02232179U CN2541703Y CN 2541703 Y CN2541703 Y CN 2541703Y CN 02232179 CN02232179 CN 02232179 CN 02232179 U CN02232179 U CN 02232179U CN 2541703 Y CN2541703 Y CN 2541703Y
Authority
CN
China
Prior art keywords
copper pipe
metal layer
copper
strengened
plated
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 02232179
Other languages
English (en)
Inventor
裴国喜
赵松奇
杨士英
Original Assignee
裴国喜
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 裴国喜 filed Critical 裴国喜
Priority to CN 02232179 priority Critical patent/CN2541703Y/zh
Application granted granted Critical
Publication of CN2541703Y publication Critical patent/CN2541703Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种镀有强化金属层的铜管。在铜管内壁镀一层镍、铬、铁或其它金属,热处理后,铜管与镀层之间形成一复合的强化金属层。在不影响铜管热交换性能的前提下,可大幅度提高铜管的耐腐蚀性能和抗冲刷性能。

Description

镀有强化金属层的铜管
所属技术领域
本实用新型涉及一种复合铜管。
背景技术
目前,市场流通的铜管大部分未作内表面处理而直接用于不同工况,当用于冷热交换器时,裸露的铜管内表面与不同酸性且流动的冷却水长时间接触,铜管就会受到腐蚀和水中各种固体颗粒的冲刷磨损,影响铜管使用寿命,特别是黄铜管在脱锌后会很快被腐蚀穿孔而报废。现时,应用在各种冷热交换器中的铜管,也有采用硫酸亚铁镀膜来保护铜管内表面。硫酸亚铁镀取的膜是一种碱式氧化铁膜,该膜层在偏酸性水中易被腐蚀,抗冲刷性能也差;由于碱式氧化物膜,是一种热的不良导体,导热性能差,影响铜管的热交换性能。
发明内容
为克服现有铜管没有保护层易受腐蚀易被冲刷磨损、碱式氧化物膜不耐腐蚀及抗冲刷性能的不足,本实用新型的目的是提供一种镀有强化金属层的铜管,该铜管不仅可以大幅度提高其耐腐蚀性能和抗冲刷性能,而且不影响热交换性能。
本实用新型解决其技术问题所采用的技术方案是:利用电化学镀或化学镀方法,在铜管内表面镀一层镍、铬、铁或其它金属层。其步骤是首先将铜管内表面酸洗活化,然后将所选镀液在铜管内孔中流动若干分钟,最后在200℃-400℃范围内进行热处理,使铜与所镀金属材料相互扩散,使之形成本实用新型所指的铜管内表面金属强化层。
本实用新型的有益效果是,该铜管具有优异的耐腐蚀性能和抗冲刷性能,且不影响铜管的导热性。这样就可以满足在不同工况下的工艺要求,并能有效地延长铜管的使用寿命,节省有限的铜资源,提高企业效益。
附图说明
图1是镀有强化金属层的铜管示意图。
图中1.铜管,2.铜与所镀金属的相互扩散层,3.镀层金属。
具体实施方式
先将铜管内表面用盐酸进行酸洗活化,而后用水冲洗,然后将镀液通过铜管内孔若干分钟,再用水冲洗干净,最后将这种铜管放置于200-400℃的温度中进行热处理,即可得到镀有强化金属层的铜管。

Claims (1)

1.一种镀有强化金属层的铜管,在铜管内壁是一强化金属层,其特征是:铜管内壁与镀层之间是铜与镀层金属材料相互扩散的复合金属层,复合金属层外是所镀金属层。
CN 02232179 2002-04-10 2002-04-10 镀有强化金属层的铜管 Expired - Fee Related CN2541703Y (zh)