CN2436903Y - 一种梯度耐火材料带锚冷却壁 - Google Patents

一种梯度耐火材料带锚冷却壁 Download PDF

Info

Publication number
CN2436903Y
CN2436903Y CN 00221088 CN00221088U CN2436903Y CN 2436903 Y CN2436903 Y CN 2436903Y CN 00221088 CN00221088 CN 00221088 CN 00221088 U CN00221088 U CN 00221088U CN 2436903 Y CN2436903 Y CN 2436903Y
Authority
CN
China
Prior art keywords
cooling wall
refractory material
cooling
utility
model
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 00221088
Other languages
English (en)
Inventor
龙世刚
李家新
孟庆民
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HUADONG METALLURGICAL COLLEGE
Original Assignee
HUADONG METALLURGICAL COLLEGE
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HUADONG METALLURGICAL COLLEGE filed Critical HUADONG METALLURGICAL COLLEGE
Priority to CN 00221088 priority Critical patent/CN2436903Y/zh
Application granted granted Critical
Publication of CN2436903Y publication Critical patent/CN2436903Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种梯度耐火材料带锚冷却壁,它是高炉长寿的重要装备,主要由冷却板、冷却水管、锚刺、导热层、耐磨抗渣层组成。其优点为,(1)冷却壁上带有锚刺不仅能增加传热面积而且能牢牢抓住喷射成型的耐火材料,解决镶砖或捣打耐火材料易脱落的问题。(2)冷却壁已去掉了“”头,冷却均匀,且消除了易破损部位。(3)冷却壁在炉内安装好后进行分层喷射成型,使炉内耐火衬无接缝薄弱环节,整体密封性好。(4)因带锚刺,便于实施喷补。故使用本专利冷却壁可以有效地延长炉龄和改善操作,增加效益。

Description

一种梯度耐火材料带锚冷却壁
本实用新型专利属于高炉炉衬冷却设备技术领域,具体涉及一种梯度耐火材料带锚冷却壁。
目前,一般高炉冷却壁是镶砖或捣打耐火材料于冷却壁热面,但不管用什么方法都存在一个致命的缺陷,耐火材料与冷却壁热膨胀系数差异很大,所以易脱落。高炉投产不久,冷却壁前面砌筑被侵蚀后,镶砖受到热力学,机械力和化学力的作用而迅速脱落或侵蚀。高炉下部某些部位仅几个月就没有砖衬全靠生成渣皮来保护冷却壁,但渣皮与冷却壁的热膨胀系数也相差很大而且不稳定。故冷却壁裸露在炉内受到上述各种破坏作用而开裂、漏水甚至烧穿。
本实用新型的目的在于提供一种使用寿命长易喷补的喷射成型梯度功能带锚冷却壁。
本实用新型梯度耐火材料带锚冷却壁,主要由冷却板1、冷却水管2、锚刺3、导热层4、耐磨抗渣层5组成。锚刺通过浇注或焊接方法固定在冷却板1上。在冷却板1上喷射成型导热层4,在导热层4上喷射成型耐磨抗渣层5。
因为在冷却壁上带有一定的锚刺,喷射一层或多层不同功能的不定形耐火材料,由于这些锚刺牢牢地将喷涂料抓住,使它不易受温度变化而脱落。我们已在研究受补面对喷补层接着强度影响时已得到充分证实。此新型冷却壁无传统冷却壁的“F”字头,消除了破损的薄弱点。而且炉子内型平滑易于顺行。由于热面是耐火材料又有锚刺传热,因此容易形成稳定渣皮从而保护冷却壁使其不易开裂漏水或烧损,延长高炉寿命。新型冷却壁在高炉内喷射成型,无砖缝,炉体整体性能好。由于此冷却壁带有锚刺,因此便于喷补,进一步延长寿命。
同时采用本技术可以根据冷却壁的前面炉衬传热与抗侵蚀功能不同而选用不同的耐火材料,如靠近炉内工作层可选用耐磨耐侵蚀性能好的材料,靠近冷却壁金属面使用导热性好的材料,使其冷却壁的传热和耐侵蚀两功能得到最佳的发挥。
下面结合附图作进一步说明:
图1为本实用新型梯度耐火材料带锚冷却壁结构图。
其中冷却板1是铸铁、铸钢、铸铜或用钢板、铜板焊制而成。冷却水管2是用无缝钢管按一定要求放在铸模中,然后铸造。锚刺3可采用“Y”型或“V”型,其长度为5-35cm,间隔为5-30cm,导热层4的厚度为5-25cm,耐磨抗渣层5的厚度5-50cm。导热层4的耐火材料为导热性好的碳质材料或含SiC的材料,可以较好的传导热量。在导热层4上用耐磨好、抗侵蚀强的耐火材料,如高铝质或刚玉质等构成耐磨抗渣层5。耐火材料的成型方法是喷射成型,即根据需要将不同质地的喷补料分层喷射在带锚刺的冷却板上形成适当的厚度。

Claims (2)

1、一种梯度耐火材料带锚冷却壁,包括冷却板,水管,其特征在于:锚刺(3)通过浇注或焊接的方法固定在冷却板(1)上,在冷却板(1)上喷射成型耐火材料导热层(4),在导热层(4)上喷射成型耐磨抗渣层(5)。
2、根据权利要求1所述的冷却壁,其特征在于:锚剌(3)可采用“Y”型或“V”型,其长度为5-35cm,间隔为5-30cm,导热层(4)的厚度为5-25cm,耐磨抗渣层(5)的厚度为5-50cm。
CN 00221088 2000-07-20 2000-07-20 一种梯度耐火材料带锚冷却壁 Expired - Fee Related CN2436903Y (zh)