CN2269300Y - 造纸机用陶瓷涂层真空吸水箱面板 - Google Patents

造纸机用陶瓷涂层真空吸水箱面板 Download PDF

Info

Publication number
CN2269300Y
CN2269300Y CN 96239845 CN96239845U CN2269300Y CN 2269300 Y CN2269300 Y CN 2269300Y CN 96239845 CN96239845 CN 96239845 CN 96239845 U CN96239845 U CN 96239845U CN 2269300 Y CN2269300 Y CN 2269300Y
Authority
CN
China
Prior art keywords
suction
ceramic
paper machine
face plates
panel
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 96239845
Other languages
English (en)
Inventor
潘牧
张汉平
罗志平
周少华
邱凤襄
潘庆鸿
邵刚勤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hanyang Hubei Paper Mill
Wuhan Polytechnic University
Original Assignee
Hanyang Hubei Paper Mill
Wuhan Polytechnic University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hanyang Hubei Paper Mill, Wuhan Polytechnic University filed Critical Hanyang Hubei Paper Mill
Priority to CN 96239845 priority Critical patent/CN2269300Y/zh
Application granted granted Critical
Publication of CN2269300Y publication Critical patent/CN2269300Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

造纸机用陶瓷涂层真空吸水箱面板,是在金属基板上开吸水孔,其上再喷涂过渡粘结层、陶瓷层。本吸水箱面板硬度高、摩擦系数低、耐磨、耐腐蚀、使用寿命长、对聚酯网磨损小。本实用新型能一次性制备大规格面板,加工容易、成本低,而且当陶瓷涂层磨损后,还可重新喷涂涂层后重用。

Description

造纸机用陶瓷涂层真空吸水箱面板
本实用新型涉及一种造纸机用吸水箱部件。
真空吸水箱是在低真空的条件下,将湿纸页固定于聚脂网面上,利用负压将湿纸页部分的水分抽走的脱水元件。目前吸水箱面板材料有木材、橡胶、低压聚乙烯、超高分子聚乙烯、陶瓷等。陶瓷块吸水箱面板由于具有耐磨、耐腐蚀、摩擦系数小、节能、对聚脂网磨损小等优点,而成为现代高速造纸机用最佳吸水箱面板,但是因大型陶瓷件成型、烧结、加工均很困难,致使价格昂贵。现有的高分子聚乙烯面板上镶嵌陶瓷条,虽可降低成本,但在加工和使用过程中难以保证其表面的平整度,故对聚脂网磨损大,使网的使用寿命短。
本实用新型的目的是针对上述吸水箱面板所存在的不足,旨在设计一种硬度高、摩擦系数低、耐磨、耐腐蚀、对聚脂网磨损小,使用寿命长的真空吸水箱面板。
下面参照附图详述本实用新型。
图1本实用新型主视图。
图2本实用新型侧视图。
本实用新型的目的实现方式为,造纸机用陶瓷涂层真空吸水箱面板,是在金属基板1上开有吸水孔2,基板上有喷涂过渡粘结层3,喷涂陶瓷层4。
参照附图,根据造纸机吸水箱的规格,按所需要的尺寸和结构形式加工出金属基板1,金属基板可为铸铁板、钢板或铝合金板。在基板上开吸水孔2,吸水孔按需要可加工为圆形或长条形或组合形。
采用等离子喷涂工艺在有吸水孔的金属基板上喷涂一层过渡粘结层3,过渡粘结层采用镍铝合金材料,其中Al含量3-20%,其余为镍。再在过渡粘结层上喷涂陶瓷涂层4,陶瓷涂层材料可为纯氧化铝陶瓷或氧化铝—氧化钛复合陶瓷。复合陶瓷的重量%含量为TiO2 1-50,SiO2 0.1-0.5,Mgo 0-0.2,Ca0-0.1,Fe2O3 0-0.3其余为Al2O43。而后对陶瓷涂层表面磨削加工到所需的光洁度和平直度。
本吸水箱面板硬度高、摩擦系数低、耐磨、耐腐蚀、使用寿命长、对聚脂网磨损小。本实用新型能一次性制备大规格面板、加工容易、成本低,而且当陶瓷涂层磨损后,还可重新喷涂涂层后使用。
下面举出本实用新型一实施例:
基板1为H30铸铁基板,规格为2300cm×295cm×50cm,板上纵向均匀开长条形孔2。过渡粘结层Ni含5%,其余为Al,厚度0.1mm,陶瓷涂层材料Al2O3-13%FiO2,厚度0.6mm。陶瓷涂层表面磨削加工达平直度1.6丝/m。
本实用新型与其他材料面板的主要性能指标见下表。
面板材料    密度(g/cm3)   硬度   孔隙率   摩擦系数     平直度   光洁度
陶瓷涂层     4.02  HRA80.8     2.5%     0.09     1.6丝/m
陶瓷     3.895  1900(威氏)    0.06-0.1     △7
超高分子聚乙烯     0.12     1.6丝/m  △3~△4
从表中可见,本实用新型较之其他面板性能优越,是理想的吸水箱面板。

Claims (5)

1、造纸机用陶瓷涂层真空吸水箱面板,其特征在于金属其板(1)上开有吸水孔(2),其板上有喷涂过渡粘结层(3),喷涂陶瓷层(4)。
2、根据权利要求1所述的吸水箱面板,其特征在于吸水孔(2)可为圆形、长条形或组合形。
3、根据权利要求1所述的吸水箱面板,其特征在于金属基板(1)可为铸铁板、钢板或铝合金板。
4、根据权利要求1所述的吸水箱面板,其特征在于过渡粘结层为镍铝合金层,其铝含量为3-20%。
5、根据权利要求1所述的吸水箱面板,其特征在于陶瓷涂层(4)为氧化物陶瓷或氧化铝—氧化钛复合陶瓷层。
CN 96239845 1996-12-10 1996-12-10 造纸机用陶瓷涂层真空吸水箱面板 Expired - Fee Related CN2269300Y (zh)