CN212613534U - Environment-friendly solid wood floor - Google Patents

Environment-friendly solid wood floor Download PDF

Info

Publication number
CN212613534U
CN212613534U CN202020657723.XU CN202020657723U CN212613534U CN 212613534 U CN212613534 U CN 212613534U CN 202020657723 U CN202020657723 U CN 202020657723U CN 212613534 U CN212613534 U CN 212613534U
Authority
CN
China
Prior art keywords
layer
lacquer
solid wood
environment
paint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN202020657723.XU
Other languages
Chinese (zh)
Inventor
刘帅
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ALL CHINA FEDERATION OF SUPPLY AND MARKETING COOPERATIVES XI'AN INSTITUTE OF RAW LACQUER
Original Assignee
ALL CHINA FEDERATION OF SUPPLY AND MARKETING COOPERATIVES XI'AN INSTITUTE OF RAW LACQUER
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ALL CHINA FEDERATION OF SUPPLY AND MARKETING COOPERATIVES XI'AN INSTITUTE OF RAW LACQUER filed Critical ALL CHINA FEDERATION OF SUPPLY AND MARKETING COOPERATIVES XI'AN INSTITUTE OF RAW LACQUER
Priority to CN202020657723.XU priority Critical patent/CN212613534U/en
Application granted granted Critical
Publication of CN212613534U publication Critical patent/CN212613534U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model relates to a timber apron technical field, concretely relates to environmental protection wood floor. The utility model provides an environmental protection solid wood floor, including the solid board matrix upper surface sets gradually first lacquer sealing layer, first lacquer wood chip layer of caulking, first lacquer grey filling layer, decorative layer and push away the light and wipe the layer clearly, and the solid board matrix lower surface sets gradually second lacquer wood chip layer of caulking, second lacquer grey filling layer, mount cloth and scrape grey coat and raw lacquer spraying layer. The utility model provides an environmental protection solid wood floor can improve hardness, high temperature resistance, corrosion resistance and the antifriction of solid board matrix, has waterproof, dampproofing, thermal-insulated, protection against insects and insulating properties, and the high difficult fish tail of film hardness on solid board matrix surface has greatly reduced later stage maintenance process.

Description

Environment-friendly solid wood floor
Technical Field
The utility model relates to a timber apron technical field, concretely relates to environmental protection wood floor.
Background
At present, with the improvement of living standard of substances, the requirements of people on living environment are more and more strict, the decoration taste is also continuously improved, and the building materials which are beautiful and more healthy and environment-friendly are pursued in decoration. The solid wood floor is a ground decoration material formed by drying and processing natural wood, has the texture of natural growth of the wood, is a poor heat conductor, can play a role of being warm in winter and cool in summer, has the characteristics of comfortable foot feeling and safe use, and is an ideal material for ground decoration of bedrooms, living rooms, study rooms and the like. However, the solid wood floor has poor stability, the indoor environment is too humid or is easy to arch, warp or deform when being dried, and the solid wood floor is frequently waxed and oiled after being paved, otherwise, the gloss of the surface of the floor is quickly lost, the maintenance difficulty is high, and the application of the solid wood floor is restricted.
SUMMERY OF THE UTILITY MODEL
An object of the utility model is to provide an environmental protection solid wood floor, the utility model provides an environmental protection solid wood floor can improve solid wood matrix 1's rigidity, high temperature resistance, corrosion resistance and antifriction, has waterproof, dampproofing, thermal-insulated, protection against insects and insulating properties, and the high difficult fish tail of film hardness on solid wood matrix 1 surface has greatly reduced later stage maintenance process.
In order to realize the purpose of the utility model, the utility model provides a following technical scheme:
the utility model provides an environmental protection solid wood floor, including solid board matrix 1 first paint sealing solid layer 2, first paint bits joint layer 3, first paint ash filling layer 4, decorative layer 5 that solid board matrix 1 upper surface set gradually and push away the light and wipe clear layer 6, and second raw paint sealing solid layer 7, second raw paint bits joint layer 8, second paint ash filling layer 9 that solid board matrix 1 lower surface set gradually, mount cloth and scrape grey layer 10 and raw paint spraying layer 11.
Preferably, the thickness of the solid wood board carcass 1 is 1-3 cm.
Preferably, the thicknesses of the first raw lacquer sealing layer 2 and the second raw lacquer sealing layer 7 are 0.03-0.1 cm independently.
Preferably, the thicknesses of the first raw lacquer wood chip caulking layer 3 and the second raw lacquer wood chip caulking layer 8 are 0.01-0.05 cm independently.
Preferably, the thicknesses of the first paint ash filling layer 4 and the second paint ash filling layer 9 are 0.01-0.05 cm independently.
Preferably, the thickness of the decorative layer 5 is 0.05-0.2 cm.
Preferably, the decorative layer 5 is a layer of a lacquer, an inlay, a layer of a gold tie or a layer of a lacquer.
Preferably, the thickness of the polishing wiping layer 6 is 0.01-0.05 cm.
Preferably, the thickness of the cloth pasting and ash scraping layer 10 is 0.3-0.8 cm.
Preferably, the thickness of the raw lacquer spraying layer 11 is 0.05-0.2 cm.
The utility model provides an environmental protection solid wood floor, including solid board matrix 1 first lacquer sealing layer 2, first lacquer wood bits joint layer 3, first lacquer grey filling layer 4, decorative layer 5 and push away the light clear layer 6 that sets gradually on the solid board matrix 1 upper surface, and second lacquer sealing layer 7, second lacquer wood bits joint layer 8, second lacquer grey filling layer 9, the cloth of mounting of setting gradually scrape grey layer 10 and raw lacquer spraying layer 11 on the solid board matrix 1 lower surface. In the utility model, the basic concepts of natural environmental protection, no volatilization and no public hazard are fully embodied by combining the natural raw lacquer and the natural solid wood, and the market demands of current environmental protection and health are met; the utility model can improve the hardness, high temperature resistance, corrosion resistance, friction resistance, water resistance, moisture resistance, heat insulation, insect prevention and insulation effects of the solid wood board matrix through the arrangement of each coating, and the raw lacquer film has high hardness and is not easy to scratch, thereby greatly reducing the later maintenance procedures; the utility model can improve the beautiful and practical value of the solid wood floor through the arrangement of the decorative layer, can customize the decorative pattern according to the requirement, and is suitable for middle and high grade home decoration and public decoration; additionally, the utility model provides an environmental protection solid wood floor manufacturing process is simple, and the operation degree of difficulty is low, has improved production efficiency.
Drawings
Fig. 1 is a schematic structural view of an environment-friendly solid wood floor provided by the present invention;
the wood board comprises a solid wood board matrix, a first raw paint sealing layer, a first raw paint wood chip joint filling layer, a first paint ash filling layer, a decorative layer, a polishing and cleaning layer, a second raw paint sealing layer, a second raw paint wood chip joint filling layer, a second paint ash filling layer, a cloth-mounted dust scraping layer and a raw paint spraying layer, wherein the solid wood board matrix is 1, the first raw paint sealing layer is 2, the first raw paint wood chip joint filling layer is 3, the first raw paint ash filling layer is 4, the decorative layer is 5, the second raw paint wood chip joint filling layer.
Detailed Description
The utility model provides an environmental protection solid wood floor, including solid board matrix 1 first paint sealing solid layer 2, first paint bits joint layer 3, first paint ash filling layer 4, decorative layer 5 that solid board matrix 1 upper surface set gradually and push away the light and wipe clear layer 6, and second raw paint sealing solid layer 7, second raw paint bits joint layer 8, second paint ash filling layer 9 that solid board matrix 1 lower surface set gradually, mount cloth and scrape grey layer 10 and raw paint spraying layer 11.
The utility model provides an environmental protection solid wood floor includes solid wood board matrix 1. As an embodiment of the present invention, the solid wood board matrix 1 is made of elm, mahogany, teak, mahogany or zizyphus jujube; the solid wood board carcass 1 is dried before use. As an embodiment of the utility model, the thickness of solid board matrix 1 is preferably 1 ~ 3cm, more preferably 2 ~ 2.5 cm.
The utility model provides an environmental protection solid wood floor including set up in the first sealed layer 2 of lacquer all the time of solid board matrix 1 upper surface with set up in the sealed layer 7 of lacquer is given birth to the second of solid board matrix 1 lower surface. As an embodiment of the utility model, the raw lacquer sealing layer comprises the raw lacquer, the raw lacquer is the secretion of natural lacquer trees, and as natural plant resin, no toxic and harmful gases such as formaldehyde volatilize, thereby being safer and more environment-friendly; and the raw lacquer sealing layer can improve the high temperature resistance, the corrosion resistance and the friction resistance of the solid wood floor. As an embodiment of the utility model, the thickness of first raw lacquer sealing layer 2 and second raw lacquer sealing layer 7 is independent preferred 0.03 ~ 0.1cm, more preferably 0.05 cm.
The utility model provides an environmental protection solid wood floor including set up in the first lacquer wood chip joint filling layer 3 on 2 surfaces on first lacquer solid layer and set up in the second raw lacquer wood chip joint filling layer 8 on 7 surfaces on second raw lacquer solid layer is used for filling the plank gap. As an embodiment of the present invention, the components of the first raw lacquer wood chip joint filling layer 3 and the second raw lacquer wood chip joint filling layer 8 include wood chips and raw lacquer; the mass ratio of the wood chips to the raw lacquer is preferably 1: 1; the wood chips preferably have a mesh size of 120 meshes. In the embodiment of the utility model, the wood chips with different meshes are respectively selected according to the width, the size and the depth of the gap or the scar furuncle and are filled according to the specific situation in a layered manner. As an embodiment of the utility model, the thickness of first raw lacquer sawdust layer 3 and second raw lacquer sawdust layer 8 of caulking is independent preferred 0.01 ~ 0.05cm, more preferably 0.02 cm.
The utility model provides an environmental protection solid wood floor including set up in the first lacquer grey filling layer 4 on 3 surfaces on first raw lacquer wood bits layer of caulking with set up in the second lacquer grey filling layer 9 on 8 surfaces on second raw lacquer wood bits layer of caulking prevents that solid wood floor from weing. As an embodiment of the present invention, the components of the first paint ash filling layer 4 and the second paint ash filling layer 9 include raw paint and ash; the mass ratio of the raw lacquer to the ash is preferably 6: 4; the ash is preferably brick ash or tile ash; the tile ash is preferably diatomite; the fineness of the ash is preferably 120 mesh. As an embodiment of the utility model, the thickness of first lacquer grey filling layer 4 and second lacquer grey filling layer 9 is independent preferred 0.01 ~ 0.05cm, more preferably 0.02 cm.
The utility model provides an environmental protection solid wood floor including set up in the grey layer 10 is scraped to the mounting cloth on 9 surfaces of second lacquer grey filling layer, can insulate against heat, protection against insects, prevent that timber fracture warp, further improve high temperature resistant, corrosion-resistant, antifriction's performance. As an embodiment of the present invention, the cloth-mounting dust-scraping layer 10 includes a cloth layer and a dust layer disposed on the surface of the cloth layer; the cloth layer is preferably grass cloth; the components of the ash layer preferably comprise raw lacquer, ash and water; the mass ratio of the raw lacquer to the ash to the water is preferably 5:4: 1; the ash is preferably brick ash or tile ash; the tile ash is preferably diatomite; the fineness of the ash is preferably 120 mesh. As an embodiment of the utility model, the thickness of the cloth-mounted ash scraping layer 10 is preferably 0.3-0.8 cm, more preferably 0.5 cm; the thickness of the ash layer is preferably 0.3-0.6 cm, and more preferably 0.5 cm.
The utility model provides an environmental protection solid wood floor including set up in mount cloth and scrape the raw lacquer spraying layer 11 on ash layer 10 surface, can be waterproof, dampproofing. As an example of the present invention, the raw lacquer spraying layer 11 comprises black raw lacquer and peppermint oil; the mass ratio of the black raw lacquer to the mint oil is preferably 7: 3. As an embodiment of the present invention, the thickness of the raw lacquer spraying layer 11 is preferably 0.05-0.2 cm, and more preferably 0.1 cm. The utility model discloses an adopt the raw lacquer spraying technique can improve production efficiency in the embodiment.
The utility model provides an environmental protection solid wood floor including set up in the decorative layer 5 on 4 surfaces on first lacquer grey filling layer improves solid wood floor's aesthetic property. As an embodiment of the present invention, the decorative layer 5 is a lacquer coating, a paint coating, an inlay layer, a gold-embedded layer, or a carved lacquer layer. In the embodiment of the present invention, when the decorative layer 5 is a paint coating layer, the natural texture of the wood can be highlighted; the components of the paint coating comprise raw lacquer and peppermint oil; the mass ratio of the raw lacquer to the mint oil is preferably 6: 4. When the decorative layer 5 is a plain coat of lacquer, the operation is simple and beautiful, the wood grain is not transparent, and the requirement on the wood grain texture of the solid board matrix 1 is not high; the component of the vegetable lacquer layer comprises raw lacquer and peppermint oil; the mass ratio of the raw lacquer to the mint oil is preferably 8: 2.
As an embodiment of the utility model, the thickness of decorative layer 5 is preferably 0.05 ~ 0.2cm, more preferably 0.1 cm.
The utility model provides an environmental protection solid wood floor including set up in 5 surperficial push away smooth clear layer 6 of wiping on decorative layer to the surface that makes the floor reaches brightly as bright mirror, smooth as the effect of grease. As an embodiment of the present invention, the polishing layer 6 includes a polishing layer disposed on the surface of the decoration layer 5 and an oil layer disposed on the surface of the polishing layer. As an embodiment of the present invention, the component of the light pushing layer is preferably vegetable oil; the constituent of the varnish layer is preferably raw lacquer. As an embodiment of the present invention, the thickness of the polishing wipe layer 6 is preferably 0.01-0.05 cm, and more preferably 0.02 cm.
As an embodiment of the present invention, the present invention provides a method for preparing an environment-friendly solid wood floor, comprising:
(1) selecting a solid wood board carcass 1: thoroughly eliminating dampness and drying elm, and facilitating later-stage production;
(2) dry-grinding a solid wood board carcass 1: dry grinding the solid wood board matrix 1 by using an abrasive belt machine to remove wood thorns and the like on the board, so that the surface of the solid wood board matrix is flat and smooth;
(3) raw lacquer sealing layer: uniformly coating high-quality raw lacquer on two sides of the dry-ground solid wood board matrix 1, wiping redundant raw lacquer on the surface of the board by using cotton cloth after the raw lacquer permeates into the solid wood board matrix 1, putting the board in a shade, and drying to form a first raw lacquer sealing layer 2 and a second raw lacquer sealing layer 7;
(4) raw lacquer wood chip joint filling layer: filling 120-mesh sawdust powder and raw lacquer in a ratio of 1:1, filling gaps or scabs of front and back panels, filling the gaps or scabs layer by layer according to specific conditions, and putting the filled panels into a shady room for drying after each filling to obtain a first raw lacquer sawdust filling layer 3 and a second raw lacquer sawdust filling layer 8;
(5) dry grinding and filling gaps: carrying out dry grinding on the plate obtained in the step (4) by using an abrasive belt machine to remove the redundant joint filling layer, so that the surface of the plate is flat and smooth;
(6) paint ash filling layer: filling pores of the plate with integral paint ash on the front side and the back side, selecting diatomite with ash of 120 meshes, blending raw paint and the diatomite into the paint ash according to the mass ratio of 6:4, filling, and then putting the paint ash into a shade to dry to obtain a first paint ash filling layer 4 and a second paint ash filling layer 9;
(7) dry grinding and filling: carrying out dry grinding on the plate obtained in the step (6) by using an abrasive belt machine to remove redundant paint ash so as to enable the surface of the plate to be flat and smooth;
(8) mounting and scraping the ash layer 10: selecting the ash selected in the step (6), screening out coarse (granularity is 40 meshes), medium (granularity is 80 meshes) and fine (granularity is 120 meshes) for later use by using a sample separation sieve, coating a raw lacquer on the surface of the second lacquer ash filling layer 9, attaching a piece of high-quality grass cloth with proper size onto the solid wood board, and coating the raw lacquer according to the paint 5: ash 4: uniformly mixing ash materials according to the mass ratio of water 1, uniformly coating the mixed paint ash on grass cloth, repeating the step for 3 times according to different mesh numbers of the paint ash, namely coarse, medium and fine paint ash, putting the paint ash into a shady room for drying each time, and obtaining a mounting cloth ash scraping layer 10;
(9) grinding the mounted cloth layer: polishing the solid wood board with multiple layers of grass cloths by 400-mesh abrasive paper, and then polishing the back of the solid wood board smoothly by 800-mesh dry abrasive paper for later use;
(10) raw lacquer spray coating 11: diluting natural peppermint oil and black raw lacquer according to the mass ratio of 3:7, circularly filtering the diluted black raw lacquer for 3 times by using 800-mesh filter cloth, removing fine particles, improving the fineness of the black raw lacquer, finally, filling the filtered black raw lacquer into a high-pressure spray gun, uniformly spraying the black raw lacquer on the surface of a cloth-mounted ash scraping layer 10 by using a 0.09mm atomizing nozzle, putting the cloth-mounted ash scraping layer into a shady room, and drying the cloth-mounted ash scraping layer, wherein the step is repeated for 10 times to obtain a raw lacquer spraying layer 11;
(11) grinding the back surface with water: grinding the solid wood board shaded and dried in the step (10) with 800-mesh sand paper and 1200-mesh sand paper in sequence, wiping off moisture, and naturally drying for later use;
(12) preparing paint wiping: cutting off redundant paint ash left on the side surface of the wood board by using a cutter, namely, mounting a cloth on the lower surface of the solid wood board, scraping an ash layer 10, and then, dry-grinding by using an abrasive belt machine to remove the redundant paint ash so as to enable the surface of the solid wood board to be flat and smooth;
(13) decorative layer 5: firstly, mixing raw lacquer with natural mint oil according to the weight percentage of lacquer 6: diluting and blending the raw lacquer 4 according to the proportion, preparing two groups of clean cotton yarn, dipping the blended raw lacquer by one group of clean cotton yarn, uniformly and thinly wiping the mixed raw lacquer on the surface of the first lacquer ash filling layer 4, slightly waiting for a moment, then wiping the redundant raw lacquer on the surface of the plate by force by using the other group of clean cotton yarn, finally putting the plate into a shady room for drying for later use, repeating the process for 15-20 times, and gradually reducing the proportion of the natural peppermint oil for diluting the raw lacquer each time until the last layer of raw lacquer does not contain the natural peppermint oil, thereby obtaining a lacquer coating;
(14) front grinding: when the paint wiping layer reaches a certain thickness, sequentially grinding with 2000-mesh sand paper and 3000-mesh fine sand paper until the size reaches 5000 meshes, and until the paint layer feels smooth and no grinding mark can be seen from the side surface;
(15) polishing and cleaning layer 6: dipping a little of vegetable oil in cotton, uniformly wiping the cotton on the surface of the decorative layer 5, uniformly spreading flour on the surface of the decorative layer, forcibly pushing and grinding the cotton with a palm or a cotton cloth, wrapping a piece of cotton with the cotton cloth, dipping a little of raw lacquer, forcibly wiping the painted surface, and repeatedly circulating the process for 3 times until the painted surface achieves the effects of brightness like a bright mirror and smoothness like condensation, thereby obtaining the environment-friendly solid wood floor.
The environment-friendly solid wood floor provided by the embodiment uses raw lacquer as main coating, and is matched with the arrangement of each layer of the upper surface and the lower surface of the solid wood board, so that the environment-friendly solid wood floor has higher hardness, high temperature resistance, corrosion resistance and friction resistance, and has the characteristics of water resistance, moisture resistance, heat insulation, insect prevention and insulation.
As another embodiment of the present invention, the preparation method of the environment-friendly solid wood floor provided by the present invention is as follows:
(1) selecting a solid wood board carcass 1: thoroughly eliminating dampness and drying the solid wood board matrix, and facilitating later-stage manufacture;
(2) dry-grinding a solid wood board carcass 1: dry grinding the solid wood board matrix 1 by using an abrasive belt machine to remove wood thorns and the like on the board, so that the surface of the solid wood board matrix is flat and smooth;
(3) raw lacquer sealing layer: uniformly coating high-quality raw lacquer on two sides of the dry-ground solid wood board matrix 1, wiping redundant raw lacquer on the surface of the board by using cotton cloth after the raw lacquer permeates into the solid wood board matrix 1, putting the board in a shade, and drying to form a first raw lacquer sealing layer 2 and a second raw lacquer sealing layer 7;
(4) raw lacquer wood chip joint filling layer: filling 120-mesh sawdust powder and raw lacquer in a ratio of 1:1, filling gaps or scabs of front and back panels, filling the gaps or scabs layer by layer according to specific conditions, and putting the filled panels into a shady room for drying after each filling to obtain a first raw lacquer sawdust filling layer 3 and a second raw lacquer sawdust filling layer 8;
(5) dry grinding and filling gaps: carrying out dry grinding on the plate obtained in the step (4) by using an abrasive belt machine to remove the redundant joint filling layer, so that the surface of the plate is flat and smooth;
(6) paint ash filling layer: filling pores of the plate with integral paint ash on the front side and the back side, selecting diatomite with ash of 120 meshes, blending raw paint and the diatomite into paint ash according to the mass ratio of 6:4, filling, and then putting the paint ash into a shady room for drying to obtain a first paint ash filling layer 4 and a second paint ash filling layer 9;
(7) dry grinding and filling: carrying out dry grinding on the plate obtained in the step (6) by using an abrasive belt machine to remove redundant paint ash so as to enable the surface of the plate to be flat and smooth;
(8) mounting and scraping the ash layer 10: selecting the ash selected in the step (6), screening out coarse (granularity is 40 meshes), medium (granularity is 80 meshes) and fine (granularity is 120 meshes) for later use by using a sample separation sieve, coating a raw lacquer on the surface of the second lacquer ash filling layer 9, attaching a piece of high-quality grass cloth with proper size onto the solid wood board, and coating the raw lacquer according to the paint 5: ash 4: uniformly mixing ash materials according to the mass ratio of water 1, uniformly coating the mixed paint ash on grass cloth, repeating the step for 3 times according to different mesh numbers of the paint ash, namely coarse, medium and fine paint ash, putting the paint ash into a shady room for drying each time, and obtaining a mounting cloth ash scraping layer 10;
(9) grinding the mounted cloth layer: polishing the solid wood board with multiple layers of grass cloths by 400-mesh abrasive paper, and then polishing the back of the solid wood board smoothly by 800-mesh dry abrasive paper for later use;
(10) raw lacquer spray coating 11: diluting natural peppermint oil and black raw lacquer according to the mass ratio of 3:7, circularly filtering the diluted black raw lacquer for 3 times by using 800-mesh filter cloth, removing fine particles, improving the fineness of the black raw lacquer, finally, filling the filtered black raw lacquer into a high-pressure spray gun, uniformly spraying the black raw lacquer on the surface of a cloth-mounted ash scraping layer 10 by using a 0.09mm atomizing nozzle, putting the cloth-mounted ash scraping layer into a shady room, and drying the cloth-mounted ash scraping layer, wherein the step is repeated for 10 times to obtain a raw lacquer spraying layer 11;
(11) grinding the back surface with water: grinding the solid wood board shaded and dried in the step (10) with 800-mesh sand paper and 1200-mesh sand paper in sequence, wiping off moisture, and naturally drying for later use;
(12) preparing paint wiping: cutting off redundant paint ash left on the side surface of the wood board by using a cutter, namely, mounting a cloth on the lower surface of the solid wood board, scraping an ash layer 10, and then, dry-grinding by using an abrasive belt machine to remove the redundant paint ash so as to enable the surface of the solid wood board to be flat and smooth;
(13) decorative layer 5: mixing the natural mint oil for the colored raw lacquer according to the ratio of lacquer 8: diluting and blending the oil 2 in proportion, filtering the mixture for 3 times by using a filter cloth with 1200 meshes left and right in a dust-free room to remove fine particles and improve the fineness of the colored raw lacquer, then dipping a proper amount of the colored raw lacquer by using a special hairbrush for a lacquer process, uniformly and thinly brushing the colored raw lacquer on a solid wood plate, removing the fine particles on the lacquer surface by using a fine needle, and finally putting the solid wood plate into a shady room for standby, wherein the process is circulated for 10 times to obtain a vegetarian decorative lacquer layer;
(14) grinding a lacquer coat: when the lacquer layer of the lacquer with the lacquer is up to a certain thickness, sequentially grinding with 2000-mesh abrasive paper and 3000-mesh fine abrasive paper until the size of the lacquer layer is 5000 meshes with water until the hand feeling of the lacquer layer is smooth and no grinding mark can be seen from the side surface, if the lacquer surface has granular feel or is not flat, continuously painting with the lacquer with the method in the step (13) until the lacquer layer is smooth;
(15) polishing and cleaning layer 6: dipping a little of vegetable oil in cotton, uniformly wiping the cotton on the surface of the decorative layer 5, uniformly spreading flour on the surface of the decorative layer, forcibly pushing and grinding the cotton with a palm or a cotton cloth, wrapping a piece of cotton with the cotton cloth, dipping a little of raw lacquer, forcibly wiping the painted surface, and repeatedly circulating the process for 3 times until the painted surface achieves the effects of brightness like a bright mirror and smoothness like condensation, thereby obtaining the environment-friendly solid wood floor.
The environment-friendly solid wood floor provided by the embodiment has higher hardness, high temperature resistance, corrosion resistance and friction resistance, and has the characteristics of water resistance, moisture resistance, heat insulation, insect prevention and insulation.
The foregoing is only a preferred embodiment of the present invention, and it should be noted that, for those skilled in the art, a plurality of modifications and decorations can be made without departing from the principle of the present invention, and these modifications and decorations should also be regarded as the protection scope of the present invention.

Claims (10)

1. The utility model provides an environmental protection solid wood floor, includes solid board matrix (1) first lacquer sealing layer (2), first lacquer sawdust joint layer (3), first lacquer ash filling layer (4), decorative layer (5) that solid board matrix (1) upper surface set gradually and push away smooth clean layer (6), and second lacquer wood flour joint layer (8), second lacquer ash filling layer (9), mount cloth and scrape grey layer (10) and raw lacquer spraying layer (11) that solid board matrix (1) lower surface set gradually.
2. The environment-friendly solid wood floor as claimed in claim 1, wherein the solid wood carcass (1) has a thickness of 1-3 cm.
3. The environment-friendly solid wood flooring according to claim 1, wherein the first green paint sealing layer (2) and the second green paint sealing layer (7) independently have a thickness of 0.03-0.1 cm.
4. The environment-friendly solid wood floor as claimed in claim 1, wherein the thickness of the first green paint wood chip joint layer (3) and the second green paint wood chip joint layer (8) is 0.01-0.05 cm independently.
5. The environment-friendly solid wood flooring according to claim 1, wherein the first paint ash filling layer (4) and the second paint ash filling layer (9) have a thickness of 0.01-0.05 cm independently.
6. The environment-friendly solid wood flooring according to claim 1, wherein the decorative layer (5) has a thickness of 0.05-0.2 cm.
7. The environment-friendly solid wood flooring according to claim 1 or 6, wherein the decorative layer (5) is a layer of a lacquer, an inlay layer, a layer of a bronzing or a layer of a lacquer carving.
8. The environment-friendly solid wood flooring according to claim 1, wherein the thickness of the polishing wipe layer (6) is 0.01-0.05 cm.
9. The environment-friendly solid wood floor as claimed in claim 1, wherein the thickness of the cloth-mounted dust scraping layer (10) is 0.3-0.8 cm.
10. The environment-friendly solid wood flooring according to claim 1, wherein the raw lacquer sprayed layer (11) has a thickness of 0.05 to 0.2 cm.
CN202020657723.XU 2020-04-26 2020-04-26 Environment-friendly solid wood floor Expired - Fee Related CN212613534U (en)