Prior art keywords
active material
material layer
electrode active
solid
layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201720793222.2U
Other languages
English (en)
Inventor
程三岗
李宝玉
陈枫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Bogao Yunli Technology Shenzhen Co ltd
Zhongneng Guosheng Power Battery Technology Beijing Co ltd
Original Assignee
In Guosheng Battery Technology (beijing) Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by In Guosheng Battery Technology (beijing) Co Ltd filed Critical In Guosheng Battery Technology (beijing) Co Ltd
Priority to CN201720793222.2U priority Critical patent/CN206976499U/zh
Application granted granted Critical
Publication of CN206976499U publication Critical patent/CN206976499U/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Classifications

    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10Energy storage using batteries
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02PCLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
    • Y02P70/00Climate change mitigation technologies in the production process for final industrial or consumer products
    • Y02P70/50Manufacturing or production processes characterised by the final manufactured product

Landscapes

  • Battery Electrode And Active Subsutance (AREA)
  • Secondary Cells (AREA)

Abstract

本实用新型公开了一种全固态电池,依次包括正极集流体、正极活性物质层、固体电解质层、负极活性物质层和负极集流体,所述固体电解质层处于正极活性物质层和负极活性物质层之间,两侧具有凸起结构,所述正极活性物质层和负极活性物质层具有与所述固体电解质层相匹配的凹槽结构;本实用新型的全固态电池,通过将正负极活性材料层与固体电解质层之间设置成凹凸结构,不但可以增加界面面积,还可以提高界面强度,防止界面处的层层之间发生脱离,粘结更可靠,从而提高固态电池的使用寿命,具有很好的借鉴意义。

Description

一种全固态电池
技术领域
本实用新型涉及电池技术领域,特别涉及一种全固态电池。
背景技术
锂离子电池字实现商业化以来,迅速成为研究热点,与其他二次化学电源相比,锂离子二次电池具有其他能源设备所不具有的优势:工作电压大、能量密度大、循环寿命长、成本低、自放电率低、对环境污染小等,因此成为未来能源领域的首选。目前基于固体电解质的全固态电池已经吸引了越来越多的关注,因此固态电池可以解决有机电解液的安全性问题,并且无机电解质简化了电池的设计,比传统电池更安全、耐用。
现有的固态电池基本都是通过沉积法或溅射法分层压缩而成的,形成的固态电池的相邻层之间具有不足的粘合力,使得截面电阻可能增加,同时,由于在充放电过程中电极活性材料内离子的移动,在层与层之间产生重复的应力,如果相邻层之间粘结力不足,则不能获得足够的界面强度,有可能发生层层之间的脱离等,最终降低电池的容量,缩短电池的寿命。
实用新型内容
本实用新型的目的在于克服现有技术的缺陷,提供一种全固态电池,所述全固态电池的技术方案是这样实现的:
一种全固态电池,依次包括正极集流体、正极活性物质层、固体电解质层、负极活性物质层和负极集流体,所述固体电解质层处于正极活性物质层和负极活性物质层之间,两侧具有凸起结构,所述正极活性物质层和负极活性物质层具有与所述固体电解质层相匹配的凹槽结构。
优选地,所述凸起结构可以是矩形凸起或是燕尾型凸起。
进一步的,所述凸起结构也可以是在正极活性物质层和负极活性物质层上的,所述凹槽结构是在固体电解质层上的。
优选地,所述凸起结构和凹槽结构的厚度为1~200μm。
进一步的优选地,所述凸起结构和凹槽结构的尺寸根据正负极活性物质层、固体电解质层的尺寸确定的。
本实用新型的全固态电池,通过将正负极活性材料层与固体电解质层之间设置成凹凸结构,不但可以增加界面面积,还可以提高界面强度,防止界面处的层层之间发生脱离,粘结更可靠,从而提高固态电池的使用寿命,具有很好的借鉴意义。
附图说明
图1为本实用新型全固态电池的结构示意图;
图2为本实用新型全固态电池的凹凸结构的另一个实施例示意图。
附图标记:1-正极集流体,2-正极活性物质层,3-固态电解质层,4-负极活性物质层,5-负极集流体,6-凸起结构,7-凹槽结构。
具体实施方式
下面结合附图和具体实施例对本实用新型作进一步详细说明。
如图1所示,一种全固态电池,依次包括正极集流体1、正极活性物质层2、固体电解质层3、负极活性物质层4和负极集流体5,所述固体电解质层3处于正极活性物质层2和负极活性物质层4之间,所述固体电解质层3两侧具有凸起结构6,所述正极活性物质层2和负极活性物质层4具有与所述固体电解质层3相匹配的凹槽结构7。
本实用新型的一个实施例,所述凸起结构6为燕尾型凸起。
如图2所示,本实用新型的另一个实施例,所述凸起结构6可以是矩形凸起。
具体实施时,所述凸起结构6也可以是在正极活性物质层2和负极活性物质层4上的,所述凹槽结构7是在固体电解质层3上的。
具体实施时,所述凸起结构6和凹槽结构7的厚度为1~200μm。
具体实施时,所述凸起结构6和凹槽结构7的尺寸根据正极活性物质层2、固体电解质层3和负极活性物质层4的尺寸确定的。
本实用新型的技术内容及技术特征已揭示如上,熟悉本领域的技术人员仍可能基于本实用新型的教示而作出不背离本实用新型实质的替换及修饰,因此,本实用新型保护范围不限于实施例所揭示的内容,也包括各种不背离本实用新型实质的替换及修饰。

Claims (4)

1.一种全固态电池,其特征在于:所述全固态电池依次包括正极集流体、正极活性物质层、固体电解质层、负极活性物质层和负极集流体,所述固体电解质层处于正极活性物质层和负极活性物质层之间,两侧具有凸起结构,所述正极活性物质层和负极活性物质层具有与所述固体电解质层相匹配的凹槽结构。
2.根据权利要求1所述的全固态电池,其特征在于:所述凸起结构是矩形凸起或是燕尾型凸起。
3.根据权利要求1所述的全固态电池,其特征在于:所述凸起结构是在正极活性物质层和负极活性物质层上的,所述凹槽结构是在固体电解质层上的。
4.根据权利要求1~3任一权利要求所述的全固态电池,其特征在于:所述凸起结构和凹槽结构的厚度为1~200μm。
CN201720793222.2U 2017-07-03 2017-07-03 一种全固态电池 Expired - Fee Related CN206976499U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201720793222.2U CN206976499U (zh) 2017-07-03 2017-07-03 一种全固态电池

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201720793222.2U CN206976499U (zh) 2017-07-03 2017-07-03 一种全固态电池

Publications (1)

Publication Number Publication Date
CN206976499U true CN206976499U (zh) 2018-02-06

Family

ID=61406607

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201720793222.2U Expired - Fee Related CN206976499U (zh) 2017-07-03 2017-07-03 一种全固态电池

Country Status (1)

Country Link
CN (1) CN206976499U (zh)

Cited By (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109687032A (zh) * 2018-12-28 2019-04-26 上海纳米技术及应用国家工程研究中心有限公司 一种锂离子电池结构的设计方法
CN110492173A (zh) * 2019-08-20 2019-11-22 成都新柯力化工科技有限公司 一种反阵列结构的固态锂离子电池及制备方法
CN111092254A (zh) * 2018-10-23 2020-05-01 中信国安盟固利动力科技有限公司 一种低界面阻抗高界面相容性全固态电池
CN111293317A (zh) * 2020-02-29 2020-06-16 天津国安盟固利新材料科技股份有限公司 一种可充放固体电池用多功能复合负极片、制备方法及二次电池
CN111312991A (zh) * 2020-02-29 2020-06-19 天津国安盟固利新材料科技股份有限公司 一种可充放固体电池及其制备方法和应用
CN111312992A (zh) * 2020-02-26 2020-06-19 天津国安盟固利新材料科技股份有限公司 二次电池用多功能复合正极片、制备方法及二次电池
CN111326708A (zh) * 2020-02-29 2020-06-23 天津国安盟固利新材料科技股份有限公司 一种可充放固体电池用多功能复合正极片、制备方法及二次电池
CN112086293A (zh) * 2019-06-13 2020-12-15 重庆九环新越新能源科技发展有限公司 全固态超级电容器的导电型复合电极材料
CN112531215A (zh) * 2019-09-17 2021-03-19 拓米(成都)应用技术研究院有限公司 具有超高界面面积的三明治复合结构单元、全固态锂离子电池及其制造方法
CN113054199A (zh) * 2019-12-27 2021-06-29 太阳诱电株式会社 全固体电池及其制造方法

Cited By (12)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN111092254A (zh) * 2018-10-23 2020-05-01 中信国安盟固利动力科技有限公司 一种低界面阻抗高界面相容性全固态电池
CN111092254B (zh) * 2018-10-23 2022-05-17 中信国安盟固利动力科技有限公司 一种低界面阻抗高界面相容性全固态电池
CN109687032A (zh) * 2018-12-28 2019-04-26 上海纳米技术及应用国家工程研究中心有限公司 一种锂离子电池结构的设计方法
CN112086293A (zh) * 2019-06-13 2020-12-15 重庆九环新越新能源科技发展有限公司 全固态超级电容器的导电型复合电极材料
CN110492173A (zh) * 2019-08-20 2019-11-22 成都新柯力化工科技有限公司 一种反阵列结构的固态锂离子电池及制备方法
CN112531215A (zh) * 2019-09-17 2021-03-19 拓米(成都)应用技术研究院有限公司 具有超高界面面积的三明治复合结构单元、全固态锂离子电池及其制造方法
CN113054199A (zh) * 2019-12-27 2021-06-29 太阳诱电株式会社 全固体电池及其制造方法
CN111312992A (zh) * 2020-02-26 2020-06-19 天津国安盟固利新材料科技股份有限公司 二次电池用多功能复合正极片、制备方法及二次电池
CN111293317A (zh) * 2020-02-29 2020-06-16 天津国安盟固利新材料科技股份有限公司 一种可充放固体电池用多功能复合负极片、制备方法及二次电池
CN111312991A (zh) * 2020-02-29 2020-06-19 天津国安盟固利新材料科技股份有限公司 一种可充放固体电池及其制备方法和应用
CN111326708A (zh) * 2020-02-29 2020-06-23 天津国安盟固利新材料科技股份有限公司 一种可充放固体电池用多功能复合正极片、制备方法及二次电池
CN111326708B (zh) * 2020-02-29 2023-04-07 天津国安盟固利新材料科技股份有限公司 一种可充放固体电池用多功能复合正极片、制备方法及二次电池

Similar Documents

Publication Publication Date Title
CN206976499U (zh) 一种全固态电池
KR101664244B1 (ko) 전극의 표면에 패턴을 형성하는 방법, 이 방법을 이용해 제조된 전극 및 이 전극을 포함하는 이차전지
CN202495523U (zh) 锂离子电池及其极片
CN106129455A (zh) 锂硫电池
CN105355457A (zh) 锂离子电容器及其化成方法
JP2011204511A (ja) 全固体型リチウムイオン二次電池
CN103427111B (zh) 一种锂离子储能电池及其制造方法
CN206849967U (zh) 一种全固态锂离子电池
CN206947451U (zh) 一种层叠式固态电池
CN206834275U (zh) 一种高倍率锂离子电池
CN108987795A (zh) 一种二次电池的电芯及电芯的制备方法
CN217035901U (zh) 一种内部串联型固态电池及固态电池组
CN204045667U (zh) 一种复合极片制造的电容电池
CN207459090U (zh) 一种锂离子电池
CN201616479U (zh) 多极耳锂离子电池
JP2011034942A (ja) 重畳電界の二次電池と太陽電池
CN206992219U (zh) 一种全固态薄膜锂电池
CN207282663U (zh) 一种全固态电池的充电系统
CN110323483A (zh) 二次电池及其制备方法与包含其的用电装置
US20110310529A1 (en) Electrochemical capacitor and method for manufacturing the same
CN114759184A (zh) 一种锂离子电池正极及锂离子电池的补锂方法
CN102324491A (zh) 叠片锂离子电池用极片以及叠片治具
CN207441882U (zh) 一种层叠式固体电池
CN203150391U (zh) 一种静电电能储存装置
CN203434245U (zh) 一种锂离子储能电池

Legal Events

Date Code Title Description
GR01 Patent grant
GR01 Patent grant
CP01 Change in the name or title of a patent holder
CP01 Change in the name or title of a patent holder

Address after: No. A-1105-044, Floor 10, Building 1, No. 18, Zhongguancun East Road, Haidian District, Beijing 100083

Patentee after: Zhongneng Guosheng power battery technology (Beijing) Co.,Ltd.

Address before: No. A-1105-044, Floor 10, Building 1, No. 18, Zhongguancun East Road, Haidian District, Beijing 100083

Patentee before: ZHONG NENG GUO SHENG BATTERY TECHNOLOGY (BEIJING) CO.,LTD.

TR01 Transfer of patent right
TR01 Transfer of patent right

Effective date of registration: 20221130

Address after: 518100 202-b, Youyi building, 1st lane, Dabao Road, zone 23, Dalang community, Xin'an street, Bao'an District, Shenzhen, Guangdong Province

Patentee after: BOGAO Yunli Technology (Shenzhen) Co.,Ltd.

Address before: No. A-1105-044, Floor 10, Building 1, No. 18, Zhongguancun East Road, Haidian District, Beijing 100083

Patentee before: Zhongneng Guosheng power battery technology (Beijing) Co.,Ltd.

CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20180206