CN206799426U - 一种曲边的3d玻璃热压成型设备的加热模组 - Google Patents
一种曲边的3d玻璃热压成型设备的加热模组 Download PDFInfo
- Publication number
- CN206799426U CN206799426U CN201720574495.8U CN201720574495U CN206799426U CN 206799426 U CN206799426 U CN 206799426U CN 201720574495 U CN201720574495 U CN 201720574495U CN 206799426 U CN206799426 U CN 206799426U
- Authority
- CN
- China
- Prior art keywords
- installing plate
- heat block
- press forming
- hole
- water service
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种曲边的3D玻璃热压成型设备的加热模组,包括:安装板、通水管、加热块、加热管、底板、隔热板,所述的安装板为热压成型设备的活动模具安装板,安装板内部开有U型水平通孔,所述的通水管固接在安装板上,且通水管与安装板的水平通孔连接,所述的加热块上端面通过隔热板连接在安装板的下端面,加热块上均匀开有多个安装孔,所述的加热管固接在加热块的安装孔内,所述的底板固接在加热块的下端面,所述的底板为钨钢材料制成,所述的安装板内部水平通孔平行设置有多条。本实用新型具有结构简单、形变量小、使用效果好等优点。
Description
技术领域
本实用新型涉及玻璃热压成型设备技术领域,具体为一种曲边的3D玻璃热压成型设备的加热模组。
背景技术
传统的热弯设备的加热模组是用钢质的钢板开孔,并且加装加热管,达到升温加热的目的,然而在实际的生产中,钢板每天从常温到800℃左右高温之间变化,导致钢板受热胀冷缩以及高温而轻微形变,导致钢板表面与受加工的石墨模具表面接触不平整,从而使得受热不均匀,这直接导致被加工工件玻璃的受热不均,最终导致压制出来的玻璃产品产品有缺陷。
实用新型内容
本实用新型的目的在于提供一种曲边的3D玻璃热压成型设备的加热模组,以解决上述背景技术中提出的问题。
为实现上述目的,本实用新型提供如下技术方案:一种曲边的3D玻璃热压成型设备的加热模组,包括:安装板、通水管、加热块、加热管、底板、隔热板,所述的安装板为热压成型设备的活动模具安装板,安装板内部开有U型水平通孔,所述的通水管固接在安装板上,且通水管与安装板的水平通孔连接,所述的加热块上端面通过隔热板连接在安装板的下端面,加热块上均匀开有多个安装孔,所述的加热管固接在加热块的安装孔内,所述的底板固接在加热块的下端面。
进一步的,所述的底板为钨钢材料制成。
进一步的,所述的安装板内部水平通孔平行设置有多条。
与现有技术相比,本实用新型的有益效果是:
1.结构简单、造价低廉;
2.形变量小、使用效果好。
本实用新型具有结构简单、形变量小、使用效果好等优点。
附图说明
图1为本实用新型整体结构示意图;
图中:1-安装板;2-通水管;3-加热块;4-加热管;5-底板;6-隔热板。
具体实施方式
下面将结合本实用新型实施例中的附图,对本实用新型实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本实用新型一部分实施例,而不是全部的实施例。基于本实用新型中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本实用新型保护的范围。
请参阅图1,本实用新型提供了一种曲边的3D玻璃热压成型设备的加热模组,包括:安装板1、通水管2、加热块3、加热管4、底板5、隔热板6,所述的安装板1为热压成型设备的活动模具安装板,安装板1内部开有U型水平通孔,所述的通水管2固接在安装板1上,且通水管2与安装板1的水平通孔连接,所述的加热块3上端面通过隔热板6连接在安装板1的下端面,加热块3上均匀开有多个安装孔,所述的加热管4固接在加热块3的安装孔内,所述的底板5固接在加热块3的下端面。
进一步的,所述的底板5为钨钢材料制成。利用钨钢材料在高温以及常温不断变化的情况下,不会形变的物理特性;
进一步的,所述的安装板1内部水平通孔平行设置有多条。增大冷却水的流量,提高冷却的效果。
工作原理:本实用新型提供了一种曲边的3D玻璃热压成型设备的加热模组,在现有的设备上做出改进,采用钨钢材料制成的底板5,其优势在于利用钨钢材料在高温以及常温不断变化的情况下,不会形变的物理特性,从而解决加热模组因高温而变形的问题,从而保证了产品的质量。
尽管已经示出和描述了本实用新型的实施例,对于本领域的普通技术人员而言,可以理解在不脱离本实用新型的原理和精神的情况下可以对这些实施例进行多种变化、修改、替换和变型,本实用新型的范围由所附权利要求及其等同物限定。
Claims (3)
1.一种曲边的3D玻璃热压成型设备的加热模组,包括:安装板(1)、通水管(2)、加热块(3)、加热管(4)、底板(5)、隔热板(6),其特征在于:所述的安装板(1)为热压成型设备的活动模具安装板,安装板(1)内部开有U型水平通孔,所述的通水管(2)固接在安装板(1)上,且通水管(2)与安装板(1)的水平通孔连接,所述的加热块(3)上端面通过隔热板(6)连接在安装板(1)的下端面,加热块(3)上均匀开有多个安装孔,所述的加热管(4)固接在加热块(3)的安装孔内,所述的底板(5)固接在加热块(3)的下端面。
2.根据权利要求1所述的一种曲边的3D玻璃热压成型设备的加热模组,其特征在于:所述的底板(5)为钨钢材料制成。
3.根据权利要求1所述的一种曲边的3D玻璃热压成型设备的加热模组,其特征在于:所述的安装板(1)内部水平通孔平行设置有多条。