CN205734517U - A kind of wear-resistant emery wheel - Google Patents
A kind of wear-resistant emery wheel Download PDFInfo
- Publication number
- CN205734517U CN205734517U CN201620464012.4U CN201620464012U CN205734517U CN 205734517 U CN205734517 U CN 205734517U CN 201620464012 U CN201620464012 U CN 201620464012U CN 205734517 U CN205734517 U CN 205734517U
- Authority
- CN
- China
- Prior art keywords
- chip
- diamond
- mill
- diamond chip
- wear
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
This utility model provides a kind of wear-resistant emery wheel, including chassis, chassis is connected with joint face, joint face is provided with several oval chip-removal hole, joint face is connected with mill, mill is uniformly provided with the first diamond chip and the second diamond chip, first diamond chip and the second diamond chip are disposed on mill, it is provided with water hole on mill between the first diamond chip and the second diamond chip, mill outer ledge is provided with diamond grinding block, diamond grinding block is arranged on the first diamond chip and the second diamond chip both sides, first diamond chip is provided with two the first chip areas, second diamond chip is provided with two the second chip areas, first diamond chip and the second diamond chip upper end are divided into three projections by two the first chip areas and two the second discharge launders respectively.
Description
Technical field
This utility model relates to grinding apparatus field, a kind of wear-resistant emery wheel.
Background technology
Stone material, pottery and metal material etc. can be polished by emery wheel, to part cylindrical components interior or have
Often occur when the part innerside of radian is polished that emery wheel can not adhesive parts completely, it may appear that part is not polished
Arriving, there is the problems such as inadequate, the chip removal poor effect of wear-resistant degree in emery wheel the most of the prior art.
Summary of the invention
In order to solve the problems referred to above this utility model, to provide a kind of chip removal effective, the wear-resistant mill that abrasion resistance properties is high
Wheel.
This utility model is achieved through the following technical solutions in order to achieve the above object:
This utility model is a kind of wear-resistant emery wheel, and including chassis, chassis is connected with joint face, is provided with number on joint face
Individual oval chip-removal hole, joint face is connected with mill, is uniformly provided with the first diamond chip and the second diamond chip on mill, the
One diamond chip and the second diamond chip are disposed on mill, the mill between the first diamond chip and the second diamond chip
Dish is provided with water hole, and mill outer ledge is provided with diamond grinding block, and diamond grinding block is arranged on the first diamond chip and
Two diamond chip both sides, are provided with two the first chip areas on the first diamond chip, are provided with two on the second diamond chip
Two chip areas, two the first chip areas and two the second discharge launders are respectively by the first diamond chip and the second diamond chip upper end etc.
It is divided into three projections.
Further improvement of the utility model is: the height of mill to described first chip area and mill are to the second chip removal
The height of groove is identical.
Further improvement of the utility model is: is arranged on the diamond grinding block of the first diamond chip both sides and is arranged on
The diamond grinding block of the second diamond chip both sides is separated from each other, the thickness of diamond grinding block and the thickness phase of the second diamond chip
With.
Further improvement of the utility model is: joint face and chassis institute angulation are 135 °-165 °.
Further improvement of the utility model is: the width of diamond grinding block and the first diamond chip and the second diamond
The width of the projection on sheet is identical.
The beneficial effects of the utility model are: be arranged on the diamond grinding block of the first diamond chip both sides and be arranged on second
Space is there is, it is ensured that after tank adds water, water can flow between two diamond grinding blocks between the diamond grinding block of diamond chip both sides
Going out, the thickness of the first diamond chip is thicker than the second diamond chip, and object is first polished by the first diamond chip, facilitates user
Finding out the abrasion condition of mill, the second diamond chip and diamond grinding block enhance the wearability of emery wheel simultaneously.
This utility model simple in construction, reasonable in design, not only chip removal is effective, can dispel the heat in time, the most wear-resistant.
Accompanying drawing explanation
Fig. 1 is structural representation of the present utility model.
Fig. 2 is side view.
Wherein: 1-chassis, 2-joint face, 3-chip-removal hole, 4-mill, 5-the first diamond chip, 6-the second diamond chip, 7-
Water hole, 8-diamond grinding block, 9-the first chip area, 10-the second discharge launder.
Detailed description of the invention
In order to strengthen understanding of the present utility model, below in conjunction with drawings and Examples, this utility model is made further
Detailed description, this embodiment be only used for explain this utility model, to protection domain of the present utility model constitute limit.
As shown in Figure 1-2, this utility model is a kind of wear-resistant emery wheel, and including chassis 1, chassis 1 is connected with joint face 2,
Being provided with several oval chip-removal hole 3 on joint face 2, joint face 2 is connected with mill 4, is uniformly provided with the first Buddha's warrior attendant on mill 4
Flag 5 and the second diamond chip 6, the first diamond chip 5 and the second diamond chip 6 are disposed on mill 4, at the first Buddha's warrior attendant
Mill 4 between flag 5 and the second diamond chip 6 is provided with water hole 7, and mill 4 outer ledge is provided with diamond grinding block 8,
Diamond grinding block 8 is arranged on the first diamond chip 5 and the second diamond chip 6 both sides, is provided with two on the first diamond chip 5
One chip area 9, is provided with two the second chip areas 10, two the first chip areas 9 and two second excretions on the second diamond chip 6
First diamond chip 5 and the second diamond chip 6 upper end are divided into three projections by groove 10 respectively, and the first diamond chip is than the second gold medal
Hard rock sheet is thick, and the first diamond chip 5 is first treated polishing object and polished, after the first diamond chip 5 is worn in use
When the thickness of thickness and the second diamond chip 6 is identical, first diamond chip the 5, second diamond chip 6 and diamond grinding block 8 are simultaneously
Treating polishing object to polish, mill 4 is connected with chassis 1 by joint face 2, makes mill 4 can treat polishing by side
Object carries out curve polishing, and diamond grinding block 8 also add the length at polishing effective to object position, mill 4 side simultaneously, increases
Added the service life of mill 4, diamond grinding block 8 width identical with the width of projection, it is to avoid impact the first Buddha's warrior attendant is set
First chip area 9 of flag 5 and the second chip area 10 being arranged on the second diamond chip 6 carry out chip removal, and mill is to first row
The height of bits groove 9 is identical with the height of mill the 4 to the second chip area 10, it is ensured that the first diamond chip 5 first chip removal upon wear
The chip removal function of groove 9 is unaffected.
This utility model simple in construction, reasonable in design, not only chip removal is effective, can dispel the heat in time, the most wear-resistant.
Claims (5)
1. a wear-resistant emery wheel, including chassis (1), it is characterised in that: described chassis (1) is connected with joint face (2), described
Joint face (2) is provided with several oval chip-removal hole (3), and described joint face (2) is connected with mill (4), on described mill (4)
It is uniformly provided with the first diamond chip (5) and the second diamond chip (6), described first diamond chip (5) and described second diamond
Sheet (6) is disposed on described mill (4), between described first diamond chip (5) and described second diamond chip (6)
Described mill (4) is provided with water hole (7), and described mill (4) outer ledge is provided with diamond grinding block (8), described diamond
Abrading block (8) is arranged on described first diamond chip (5) and described second diamond chip (6) both sides, at described first diamond chip
(5) it is provided with two the first chip areas (9), described second diamond chip (6) is provided with two the second chip areas (10), two
Described first chip area (9) and two described second discharge launders (10) are respectively by described first diamond chip (5) and described second
Diamond chip (6) upper end is divided into three projections.
A kind of wear-resistant emery wheel, it is characterised in that: described mill (4) arrives described first chip area
(9) height is identical with the height of described mill (4) to described second chip area (10).
A kind of wear-resistant emery wheel, it is characterised in that: it is arranged on described first diamond chip (5) two
The described diamond grinding block (8) of side and the described diamond grinding block (8) being arranged on described second diamond chip (6) both sides mutually divide
From, the thickness of described diamond grinding block (8) is identical with the thickness of described second diamond chip (9).
A kind of wear-resistant emery wheel, it is characterised in that: described joint face (2) and described chassis (1) institute
Angulation is 135 °-165 °.
A kind of wear-resistant emery wheel, it is characterised in that: the width of described diamond grinding block (8) and institute
State the first diamond chip (5) identical with the width of the described projection on described second diamond chip (6).