CN204867760U - 一种焊接衬垫结构 - Google Patents

一种焊接衬垫结构 Download PDF

Info

Publication number
CN204867760U
CN204867760U CN201520658197.8U CN201520658197U CN204867760U CN 204867760 U CN204867760 U CN 204867760U CN 201520658197 U CN201520658197 U CN 201520658197U CN 204867760 U CN204867760 U CN 204867760U
Authority
CN
China
Prior art keywords
welding
steel bushing
welding backing
spacer block
backing structure
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201520658197.8U
Other languages
English (en)
Inventor
张国栋
张雅芝
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen City Jin Penggui material science and Technology Co Ltd
Original Assignee
Wuhan University WHU
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuhan University WHU filed Critical Wuhan University WHU
Priority to CN201520658197.8U priority Critical patent/CN204867760U/zh
Application granted granted Critical
Publication of CN204867760U publication Critical patent/CN204867760U/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本实用新型提供一种焊接衬垫结构,属于焊接领域。包括若干衬垫块和粘贴胶带,若干衬垫块首尾相连,底面贴装于粘贴胶带上,在引弧端的第一个衬垫块套于与之紧密配合的钢套中,且钢套在焊缝外。钢套的形状根据焊接衬垫块而定。本实用新型解决了现有的陶瓷、石棉等衬垫在单面焊双面成型工艺中,因其导电性不良而带来的引弧困难的问题。钢套不会熔化到焊缝中而影响到焊缝的性能,结构简单,使用方便,生产成本低廉,对于相同形状的焊接衬垫,钢套可以重复使用。

Description

一种焊接衬垫结构
技术领域
本实用新型涉及一种焊接衬垫结构,属于焊接技术领域。
背景技术
在对工件进行单面焊双面成型焊接时,为了防止焊缝熔融金属液从焊缝底部流失或烧穿,需要焊接衬垫使焊缝根部熔融金属强制成型。焊接衬垫结构一般包括若干衬垫块和粘贴胶带,
将若干块焊接衬垫块首尾相连,将底面贴装在粘贴胶带上,再由粘贴胶带固定在工件焊缝下。使用的衬垫体材料有陶瓷、石棉、玻璃纤维、金属等,其中陶瓷是目前使用最多的焊接衬垫材料,陶质衬垫熔点适宜,电弧热使衬垫成形槽表面发生部分熔化,对焊缝金属起润滑作用,使焊道背面成形良好,且耐吸潮性好,位置适应性强。
申请号为201210479952.7的发明提供一种特别适用于高效埋弧单面焊的高效埋弧焊焊接衬垫,衬垫材料为陶瓷,其特征在衬垫上表面设有一层与焊接衬垫大小相配的玻璃纤维带,优点是保证高温的熔化焊缝金属不致泄露,从而避免了焊瘤缺陷的产生,保证了焊缝的焊趾整齐美观,提高焊接速度。上述发明的衬垫材料为陶瓷,焊接方法为自动或半自动焊,未考虑到由于陶瓷不导电,自动焊接时焊丝引弧较困难,降低焊接速度的问题。
申请号为201020286349.3的实用新型考虑到了由于陶瓷衬垫不导电易出现电弧熄灭的问题,提供一种粘贴式陶瓷焊接衬垫,其特征在于衬垫的凹槽内设置有与其形状相匹配的金属条,金属条的高度等于或小于所述凹槽的深度优点由于金属条的导电性,从而保证焊接时不会出现电弧熄灭,由于金属条在焊接完成后已成为焊缝的一部分,不存在取出问题,结构非常简单且加工成本很低。上述发明在衬垫的凹槽内设置有金属条,当金属条的高度小于凹槽的深度时,金属条在凹槽内会松动,不易定位,影响背面焊缝成型,且容易从衬垫脱落,使用不方便;若金属条的厚度等于凹槽,在正常焊接电弧热的作用下不能完全熔化而成为焊缝的一部分,会使焊缝不能成型,出现未焊透、焊瘤、夹渣和焊缝外面缺欠等焊接缺陷,得到的焊接接头达不到力学性能要求;若将整个金属条熔化,则需要的焊接热很高,得到的焊接接头影响区晶粒粗大,且金属条的成分未知,熔于焊缝中影响焊缝机械性能。
实用新型内容
针对现有技术存在的问题,本实用新型提供一种引弧容易、使用方便的焊接衬垫结构。
为解决上述技术问题,本实用新型采用如下技术方案。
一种焊接衬垫结构,包括若干衬垫块和粘贴胶带,若干衬垫块首尾相连,底面贴装于粘贴胶带上,在引弧端的第一个衬垫块套于与之紧密配合的钢套中,且钢套在焊缝外。
所述钢套壁厚为0.1-0.3mm。
所述钢套的深度即衬垫块伸入其中的长度按焊丝引弧活动范围而定,要保证钢套在焊缝外,一般为8-12mm。
所述钢套采用低碳钢制成,塑韧性较好,容易加工成配合各种焊接衬垫使用的形状。
所述衬垫块材料为陶瓷、石棉、玻璃纤维等一切用于焊接衬垫中不导电的材料。
与现有技术相比,本实用新型具有以下优点和有益效果:
1、本实用新型当衬垫块为陶瓷、石棉等不导电的材料,焊接引弧较困难时,通过钢套使焊丝易于引弧,保证焊接过程的顺利进行,提高生产效率。
2、本实用新型的钢套仅套在位于引弧端的第一个衬垫块的首端,钢套仅用于引弧,钢套套在衬垫块的部分伸出焊缝外,焊接电弧热不需要用来熔化钢套,钢套的成分不影响焊缝的性能,焊缝不会因为钢套出现各种焊接缺陷。
3、本实用新型结构简单,使用方便,生产成本低廉,对于相同形状的焊接衬垫,钢套可以重复使用,节约资源;且钢套可加工成各种形状,从而适用于各种形状的焊接衬垫,实用性强。
附图说明
图1为本实用新型的钢套结构简图。
图2为本实用新型的结构示意图。
其中,1—钢套,2—衬垫块,3—粘贴胶带。
具体实施方式
下面结合附图所示的实施例对本实用新型作进一步说明。
如图2所示,本实用新型所示的焊接衬垫结构,包括若干衬垫块2和粘贴胶带3,若干衬垫块2首尾相连,底面贴装于粘贴胶带3上,在引弧端的第一个衬垫块2套于与之紧密配合的钢套1中。
钢套1材料为塑韧性较好的低碳钢,壁厚为0.1-0.3mm;钢套1是按照衬垫块2的形状制成的,钢套的深度设置为10mm。
在使用本实用新型焊接衬垫结构对工件进行焊接时,在引弧端,将钢套1套于第一个衬垫块2的首端,钢套1伸出焊缝外部,伸出的距离为钢套的深度为10mm;将多块衬垫块互相连接成条状,底部平面用粘贴胶带3固定连接,粘贴胶带3采用铝箔胶带;使用衬垫块2两侧的固定粘贴胶带将衬垫块固定在工件的接头背面。
在对工件进行焊接时,钢套1使焊丝引弧容易,保证了焊接过程的顺利进行,且钢套仅用于引弧,未熔化到焊缝中去,不会影响焊缝的性能,从而形成良好的焊接接头,提高生产效率。
最后应当说明的是,以上实施例仅用以说明本实用新型的技术方案,钢套1的形状是根据衬垫块2的形状制成。本实用新型中的钢套可加工成各种形状,从而适用于各种形状的焊接衬垫块,结构简单,使用方便,实用性强,生产成本低廉;对于相同形状的焊接衬垫,钢套可以重复使用,节约资源。

Claims (6)

1.一种焊接衬垫结构,其特征在于:包括若干衬垫块(2)和粘贴胶带(3),若干衬垫块(2)首尾相连,底面贴装于粘贴胶带(3)上,在引弧端的第一个衬垫块(2)套于与之紧密配合的钢套(1)中,且钢套(1)在焊缝外。
2.根据权利要求1所述的焊接衬垫结构,其特征在于:钢套(1)壁厚为0.1-0.3mm。
3.根据权利要求1所述的焊接衬垫结构,其特征在于:所述钢套(1)的深度为8-12mm。
4.根据权利要求1所述的焊接衬垫结构,其特征在于:钢套(1)采用低碳钢制成。
5.根据权利要求1所述的焊接衬垫结构,其特征在于:钢套(1)的形状按照衬垫块的形状制成。
6.根据权利要求1所述的焊接衬垫结构,其特征在于:所述衬垫块材料为陶瓷、石棉或玻璃纤维。
CN201520658197.8U 2015-08-28 2015-08-28 一种焊接衬垫结构 Expired - Fee Related CN204867760U (zh)