CN203732356U - 薄壁小径管拉伸试样专用塞头 - Google Patents
薄壁小径管拉伸试样专用塞头 Download PDFInfo
- Publication number
- CN203732356U CN203732356U CN201420103235.9U CN201420103235U CN203732356U CN 203732356 U CN203732356 U CN 203732356U CN 201420103235 U CN201420103235 U CN 201420103235U CN 203732356 U CN203732356 U CN 203732356U
- Authority
- CN
- China
- Prior art keywords
- core
- sleeve
- pipe
- thin
- retainer plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种薄壁小径管拉伸试样专用塞头,其关键技术在于:其包括芯套和芯棒,芯套是经由圆柱形套筒等分而成的三段结构相同的瓣状结构,芯套外径不大于管材内径,芯套一端设有定位轴肩,芯套的中心设有轴向的锥形孔;芯棒呈锥形,芯棒的外圆与锥形孔相匹配,芯棒的长度大于芯套的长度。本实用新型设置了芯套和芯棒,并且芯套为等分而成的三个瓣状结构,在对薄壁小径管进行整管拉伸试验时,在试样两端加装该塞头作为整管拉伸夹持部分,试样拉断后,取出锥形芯棒,芯套便自由脱落,完毕后又可装入其他管材试样继续做拉伸试验,方便拆卸,且塞头坚实牢固,这样就可以大大提高试验的效率以及试验结果的准确性。
Description
技术领域
本实用新型涉及一种拉伸试验用薄壁小径管拉伸试样专用塞头。
背景技术
材料的拉伸试验是材料机械性能试验的基本方法之一,可测定材料的一系列的强度指标和塑性指标,材料的拉伸试验广泛应用于电厂金属材料的长期运行老化评级依据以及金属部件失效分析试验手段。
GB228中针对不同的试样类型规定了相应的试样形状、尺寸及试验方法。电厂金属材料一般都是管材试样,通常管材的拉伸试验采用剖管拉伸和整管拉伸,对于厚壁大径管材一般采用剖管拉伸的方法,而对于薄壁小径管则采用管段试样整管拉伸的方法,允许压扁管段试样两夹持头部或者在试样两端加以塞头,塞头是否合适直接影响了试验的准确性及方便性,而目前没有合适的塞头。
实用新型内容
本实用新型要解决的技术问题是提供一种结构简单、方便拆卸并可重复利用的薄壁小径管拉伸试样专用塞头。
为解决上述技术问题,本实用新型所采取的技术方案是:一种薄壁小径管拉伸试样专用塞头,其关键技术在于:其包括芯套和芯棒,所述芯套是经由圆柱形套筒等分而成的三段结构相同的瓣状结构,所述芯套外径不大于管材内径,所述芯套一端设有定位轴肩,所述芯套的中心设有轴向的锥形孔;
所述芯棒呈锥形,芯棒的外圆与所述锥形孔相匹配,所述芯棒的长度大于芯套的长度。
采用上述技术方案所产生的有益效果在于:本实用新型设置了芯套和芯棒,并且芯套为等分而成的三个瓣状结构,在对薄壁小径管进行整管拉伸试验时,在试样两端加装该塞头作为整管拉伸夹持部分,试样拉断后,取出锥形芯棒,芯套便自由脱落,完毕后又可装入其他管材试样继续做拉伸试验,方便拆卸,且塞头坚实牢固,这样就可以大大提高试验的效率以及试验结果的准确性。
附图说明
图1是本实用新型的使用状态示意图;
图2是圆柱型套筒的示意图;
图3是芯套的示意图;
图4是芯棒的示意图;
其中,1、管材;2、芯套;3、芯棒;4、定位轴肩;5、锥形孔。
具体实施方式
下面结合附图和具体实施方式对本实用新型作进一步详细的说明。
参见附图1-4,本实用新型由芯套2及芯棒3组成,芯套2外径尺寸可根据管材1(即试样)的尺寸大小进行加工,芯套2由一圆柱形套筒三等分而成,芯套2外径小于或等于管材1内径,芯套2一端设有小于管材1壁厚的定位轴肩4,芯套2的内孔车成锥形孔5。芯棒3加工成与锥形孔5相配的锥形。
制作时按照管材试样尺寸加工芯套及芯棒即可,加工好后装入管材1管端,塞紧后即可做拉伸试验,试样拉断后,取出锥形芯棒3,芯套2便自由脱落,完毕后又可装入其他管材试样继续做拉伸试验,如要试验其他不同规格的管材,只要改变芯套外径尺寸即可。本实用新型作为整管拉伸夹持部分使用非常方便。
Claims (1)
1.一种薄壁小径管拉伸试样专用塞头,其特征在于:其包括芯套(2)和芯棒(3),所述芯套(2)是经由圆柱形套筒等分而成的三段结构相同的瓣状结构,所述芯套(2)外径不大于管材(1)内径,所述芯套(2)一端设有定位轴肩(4),所述芯套(2)的中心设有轴向的锥形孔(5);
所述芯棒(3)呈锥形,芯棒(3)的外圆与所述锥形孔(5)相匹配,所述芯棒(3)的长度大于芯套(2)的长度。