CN203490964U - 一种太阳能电动车电机用漆包铝线 - Google Patents

一种太阳能电动车电机用漆包铝线 Download PDF

Info

Publication number
CN203490964U
CN203490964U CN201320502083.5U CN201320502083U CN203490964U CN 203490964 U CN203490964 U CN 203490964U CN 201320502083 U CN201320502083 U CN 201320502083U CN 203490964 U CN203490964 U CN 203490964U
Authority
CN
China
Prior art keywords
layer
coated
coating
electric car
enamel insulated
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201320502083.5U
Other languages
English (en)
Inventor
尹先国
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhongshan Xincheng enamelled wire Co., Ltd.
Original Assignee
GANZHOU SUNJINN SPECIAL ENAMELLED WIRE Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GANZHOU SUNJINN SPECIAL ENAMELLED WIRE Co Ltd filed Critical GANZHOU SUNJINN SPECIAL ENAMELLED WIRE Co Ltd
Priority to CN201320502083.5U priority Critical patent/CN203490964U/zh
Application granted granted Critical
Publication of CN203490964U publication Critical patent/CN203490964U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型提供一种太阳能电动车电机用漆包铝线,包括铝芯、绝缘漆层、屏蔽层、耐热涂层,其中在铝芯的外表面涂覆有绝缘漆层,绝缘漆层为聚酯亚胺层,在绝缘漆层上涂覆有屏蔽层,所述的屏蔽层是有机涂层,有机涂层是掺有钛、硅、锑、铬的固态金属化合物,在屏蔽层外涂覆有耐热层,耐热层为聚酰胺酰亚胺层。本实用新型在绝缘漆层与耐热涂层中间加了一层屏蔽层,这种带屏蔽层的漆包铝线具有耐电晕性能,电机绕组耐局部放电,可以延长太阳能汽车电机使用寿命,同时用铝芯导体代替铜,制造成本也相对较低一些。

Description

一种太阳能电动车电机用漆包铝线
技术领域
本实用新型涉及一种漆包线,尤其涉及一种太阳能电动车电机用漆包铝线。 
背景技术
目前,在太阳能电动车的电机上都会用到漆包线,而太阳能电动车的电机长时间在高温下工作会产生电晕,从而会破坏漆包线的漆膜,继而降低了漆包线的使用寿命,这就要求漆包线的耐电晕性能要较好。但是,目前漆包线大多数以铜为导体,加工工艺复杂,缺少屏蔽效果,不耐局部放电,耐电晕性能也不理想。 
发明内容
为了使在太阳能电动车电机上使用的漆包线具有较好的耐电晕性能,本实用新型提供一种一种太阳能电动车电机用漆包铝线。 
本实用新型的目的是通过以下方案实现的:一种太阳能电动车电机用漆包铝线,包括铝芯、绝缘漆层、屏蔽层、耐热涂层,其中在铝芯的外表面涂覆有绝缘漆层,绝缘漆层为聚酯亚胺层,在绝缘漆层上涂布有屏蔽层,所述的屏蔽层是有机涂层,有机涂层是掺有钛、硅、锑、铬的固态金属化合物,在屏蔽层外涂覆有耐热层,耐热层为聚酰胺酰亚胺层。 
本实用新型的有益效果是:在绝缘漆层与耐热涂层中间加了一层屏蔽层,这种带屏蔽层的漆包铝线具有耐电晕性能,电机绕组耐局部放电,可以延长太阳能汽车电机使用寿命,同时用铝芯导体代替铜,制造成本也相对较低一些。 
附图说明
图1为本实用新型的结构示意图。 
具体实施方式
下面结合附图对本实用新型做进一步的说明。 
本实用新型的技术方案是:一种太阳能电动车电机用漆包铝线,包括铝芯1、绝缘漆层2、屏蔽层3、耐热涂层4,其中在铝芯1的外表面涂覆有绝缘漆层2,绝缘漆层2为聚酯酰亚胺层,在绝缘漆层2上涂布有屏蔽层3,所述的屏蔽层3是有机涂层,在屏蔽层3外涂覆有耐热涂层4,耐热涂层4为聚酰胺酰亚胺层。 

Claims (1)

1.一种太阳能电动车电机用漆包铝线,包括绝缘漆层、耐热涂层、其特征在于:还包括铝芯、屏蔽层,其中在铝芯的外表面涂覆有绝缘漆层,绝缘漆层为聚酯亚胺层,在绝缘漆层上涂覆有屏蔽层,所述的屏蔽层是有机涂层,在屏蔽层外涂覆有耐热层,耐热层为聚酰胺酰亚胺层。
CN201320502083.5U 2013-08-17 2013-08-17 一种太阳能电动车电机用漆包铝线 Expired - Fee Related CN203490964U (zh)