CN203455253U - 钝化镁脱硫剂中金属镁含量测定装置 - Google Patents
钝化镁脱硫剂中金属镁含量测定装置 Download PDFInfo
- Publication number
- CN203455253U CN203455253U CN201320524210.1U CN201320524210U CN203455253U CN 203455253 U CN203455253 U CN 203455253U CN 201320524210 U CN201320524210 U CN 201320524210U CN 203455253 U CN203455253 U CN 203455253U
- Authority
- CN
- China
- Prior art keywords
- magnesium
- reaction vessel
- desulfurizing agent
- eudiometer
- wireway
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型公开了一种钝化镁脱硫剂中金属镁含量的测定装置。该装置包括设置在固定支架上的反应容器,以及与所述反应容器通过导气管相连接的量气管,反应容器上设置有一个导气管接口和一个反应物料加入口,导气管接口上连接有带橡皮塞的导气管,带橡皮塞的导气管与量气管的上端相连接,量气管下端还连接有敞口水准瓶,反应物料加入口处连接有分液漏斗,量气管和敞口水准瓶中盛有封闭液。该装置结构简单,操作方便,测定结果准确。
Description
技术领域
本实用新型属于分析化学技术领域,具体是指一种钝化镁脱硫剂中金属镁含量测定装置。
背景技术
在炼钢过程中常采用添加脱碳、脱磷、脱硫、脱氧等辅助材料去除有害气体和非金属夹杂物,确保钢材的品质。钝化镁脱硫剂是目前一种最常用的脱硫材料,活性成分为其中的金属镁。由于金属镁是一种相当活泼的金属,在存放过程中极易与空气中的氧气及水分发生化学反应,故常采用化学方法将其表面的金属镁钝化制成钝化镁脱硫剂。钝化镁脱硫剂中镁的存在形态包括金属镁、氧化镁及氟化镁等,其中能起脱硫作用的只有金属镁。因此,应用过程中需要准确测定钝化镁脱硫剂中金属镁的含量。在国家标准GB4374.8-84《镁粉和铝镁合金粉化学分析方法气体容量法测定活性镁及活性铝镁量》通过试样与盐酸反应,其中活性镁置换出等当量的氢气,根据氢气体积计算活性镁的含量。但是该方法中,需要实时测定实验条件下的大气压力和温度,用于准确核算镁的含量,该实施测定的操作大大影响了该方法的测定速度及应用性。
发明内容
本实用新型的目的在于提供一种钝化镁脱硫剂中金属镁含量的测定装置。该装置结构简单,操作方便,测定结果准确。
为实现上述目的,本实用新型的钝化镁脱硫剂中金属镁含量测 定装置,包括设置在固定支架上的反应容器,以及与所述反应容器通过导气管相连接的量气管,其特殊之处在于:所述反应容器上设置有一个导气管接口和一个反应物料加入口,所述导气管接口上连接有带橡皮塞的导气管,所述带橡皮塞的导气管与量气管的上端相连接,所述量气管下端还连接有敞口水准瓶,所述反应物料加入口处连接有分液漏斗,所述量气管和敞口水准瓶中盛有封闭液。
进一步地,所述反应容器外部设置有一个冷却液放置槽,加设此装置后,可以有效控制反应容器中反应物的温度不发生加大幅度的变化,减小检测结构的误差。
再进一步地,所述封闭液为红色的罗丹明溶液。
应用时,连接好装置并对装置检查气密性后,再将待测物从反应物料加入口中加入到反应容器中;打开分液漏斗上的分液阀门,提升水准瓶,将量气管内液面提升到“0”刻度处,关闭分液漏斗上的分液阀门,准确量取一定体积的、且过量的烯酸溶液加至分液漏斗中。打开分液漏斗上的分液阀门,向反应容器中加入足量烯酸使待测物充分反应完全;然后慢慢降低水准瓶高度,直至量气管内液面与水准瓶内液面相平。记录此时量气管中气体的体积读数V即为所产生氢气的体积。
在相同环境下,同时分别采用上述装置将高纯金属镁标样及钝化镁脱硫剂样品作为待测物进行反应,测定得到氢气在量气管5中的体积,通过计算即可得出钝化镁脱硫剂样品中金属镁的含量。
利用本实用新型装置,通过分别测定在相同温度和压力条件下,钝化镁脱硫剂样品和高纯金属镁标样的产气体积,采用简单的比较计算法便可方便求出钝化镁脱硫剂样品中金属镁的含量,而不需要釆用国标GB4374.8-84中所描述的“先测量实验过程中的气压 和温度,再通过查表换算得出样品的产氢气体积,最后求算出样品中金属镁的含量,简化了测量过程,提高了测量精密度和准确度。
附图说明
图1为本实用新型的钝化镁脱硫剂中金属镁含量测定装置的结构示意图。
具体实施方式
下面结合附图和具体实施例对本发明做进一步详细说明。
如图1所示,一种钝化镁脱硫剂中金属镁含量测定装置包括:设置在固定支架1上的反应容器4以及与反应容器4通过导气管相连接的量气管5,反应容器4外部设置有一个冷却液放置槽3,反应容器4上设置有一个导气管接口7和一个反应物料加入口8,导气管接口7上连接有带橡皮塞的导气管9,带橡皮塞的导气管9与量气管5的上端相连接,量气管5下端还连接有敞口水准瓶6,所述反应物料加入口8处连接有分液漏斗2,所述量气管5和敞口水准瓶6中盛有红色的罗丹明溶液作为封闭液。
在相同环境下,先将质量为m10的标准镁放入上述装置进行反应,测定得到生成的气体体积为V1c,再将质量为m20的待测钝化镁脱硫剂放入装置进行反应,计算出生成的气体体积为V2c。
则钝化镁脱硫剂中金属镁的含量WMg为:
Claims (3)
1.一种钝化镁脱硫剂中金属镁含量测定装置,包括设置在固定支架(1)上的反应容器(4),以及与所述反应容器(4)通过导气管相连接的量气管(5),其特征在于:所述反应容器(4)上设置有一个导气管接口(7)和一个反应物料加入口(8),所述导气管接口(7)上连接有带橡皮塞的导气管(9),所述带橡皮塞的导气管(9)与量气管(5)的上端连接,所述量气管(5)下端还连接有敞口水准瓶(6),所述反应物料加入口(8)处连接有分液漏斗(2),所述量气管(5)和敞口水准瓶(6)中盛有封闭液。
2.根据权利要求1所述的钝化镁脱硫剂中金属镁含量测定装置,其特征在于:所述反应容器(4)外部设置有一个冷却液放置槽(3)。
3.根据权利要求1或2所述的钝化镁脱硫剂中金属镁含量测定装置,其特征在于:所述封闭液为红色的罗丹明溶液。