CN203103130U - 一种铝电解电容器 - Google Patents
一种铝电解电容器 Download PDFInfo
- Publication number
- CN203103130U CN203103130U CN 201220697326 CN201220697326U CN203103130U CN 203103130 U CN203103130 U CN 203103130U CN 201220697326 CN201220697326 CN 201220697326 CN 201220697326 U CN201220697326 U CN 201220697326U CN 203103130 U CN203103130 U CN 203103130U
- Authority
- CN
- China
- Prior art keywords
- aluminium foil
- electrolytic
- cathode
- aluminium
- negative pole
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种铝电解电容器,其包括铝圆筒和电容器芯包,电容器芯包包括正极铝箔和负极铝箔,正极铝箔和负极铝箔之间装设至少三层电解纸,正极引线和负极引线分别通过固定舌部焊装于相应的正极铝箔和负极铝箔背离电解纸一侧,负极铝箔为腐蚀化成铝箔。正极引线和负极引线采用焊接方式固定于相应的铝箔,不会产生毛刺并避免电解纸被刺穿以及由于毛刺所引起的电容器短路击穿甚至爆炸等缺陷;正极引线和负极引线分别背离电解纸安装,至少三层电解纸叠加的电解纸层能够保证足够的厚度,焊接时所产生的凸起位置很难刺破电解纸层;由腐蚀化成铝箔制备而成的负极铝箔能够承受反向漏电流的冲击。本实用新型具有结构稳定、使用寿命长的优点。
Description
技术领域
本实用新型涉及电容器技术领域,尤其涉及一种铝电解电容器。
背景技术
作为一种重要的电容元器件,铝电解电容器已广泛地应用于电子行业中;其中,铝电解电容器一般包括有正极铝箔、负极铝箔、电解纸、正极引线以及负极引线。
在铝电解电容器生产加工过程中,现有技术普遍采用铆装方式将正极引线和负极引线与相应的正极铝箔以及负极铝箔铆接,电解纸装设于正极铝箔和负极铝箔之间,由于铆装时很容易产生毛刺现象,在将正极铝箔、电解纸以及负极铝箔一起卷绕的过程中,可能会出现毛刺刺穿电解纸或者毛刺尖端在电场作用下放电引起电容器短路击穿、爆炸等缺陷。
另外,现有的铝电解电容器所采用的铝箔一般为普通铝箔,普通铝箔不能承受反向漏电流的冲击,使用寿命短。
发明内容
本实用新型的目的在于针对现有技术的不足而提供一种铝电解电容器,该铝电解电容器能够有效地避免电解纸被毛刺刺穿以及毛刺尖端在电场作用下放电引起电容器短路击穿、爆炸等缺陷,结构稳定且使用寿命长。
为达到上述目的,本实用新型通过以下技术方案来实现。
一种铝电解电容器,包括有铝圆筒以及嵌装于铝圆筒内的电容器芯包,电容器芯包包括有宽度相等的正极铝箔和负极铝箔,正极铝箔和负极铝箔之间装设有至少三层宽度较正极铝箔和负极铝箔的宽度大的电解纸,正极铝箔焊装有正极引线,负极铝箔焊装有负极引线,正极引线和负极引线分别设置有固定舌部,固定舌部分别与相应的正极铝箔和负极铝箔焊接,正极引线的固定舌部位于正极铝箔背离电解纸一侧,负极引线的固定舌部位于负极铝箔背离电解纸一侧;其中,负极铝箔为腐蚀化成铝箔,电解纸的宽度为3mm,正极铝箔和负极铝箔的宽度分别为2.2mm。
本实用新型的有益效果为:本实用新型所述的一种铝电解电容器,其包括有铝圆筒和电容器芯包,电容器芯包包括有正极铝箔和负极铝箔,正极铝箔和负极铝箔之间装设有至少三层电解纸,正极引线和负极引线分别通过固定舌部焊装于相应的正极铝箔和负极铝箔,正极引线和负极引线的固定舌部分别背离电解纸,负极铝箔为腐蚀化成铝箔。本实用新型的正极引线和负极引线采用焊接方式固定于相应的正极铝箔和负极铝箔,在相应的正极引线和负极引线焊接过程中不会产生毛刺现象,进而避免了电解纸被刺穿以及由于毛刺所引起的电容器短路击穿甚至爆炸等缺陷;正极引线和负极引线分别背离电解纸安装,至少三层电解纸叠加的电解纸层能够保证足够的厚度,焊接时所产生的凸起位置很难刺破电解纸层;另外,由腐蚀化成铝箔制备而成的负极铝箔能够承受反向漏电流的冲击,使用寿命长。综合上述情况可知,本实用新型具有结构稳定、使用寿命长的优点。
附图说明
下面利用附图来对本实用新型进行进一步的说明,但是附图中的实施例不构成对本实用新型的任何限制。
图1为本实用新型的结构示意图。
1——铝圆筒 2——电容器芯包
3——正极铝箔 4——负极铝箔
5——电解纸 6——正极引线
7——负极引线 8——固定舌部。
具体实施方式
下面结合具体的实施方式来对本实用新型进行说明。
如图1所示,一种铝电解电容器,包括有铝圆筒1以及嵌装于铝圆筒1内的电容器芯包2,电容器芯包2包括有宽度相等的正极铝箔3和负极铝箔4,正极铝箔3和负极铝箔4之间装设有至少三层宽度较正极铝箔3和负极铝箔4的宽度大的电解纸5,正极铝箔3焊装有正极引线6,负极铝箔4焊装有负极引线7,正极引线6和负极引线7分别设置有固定舌部8,固定舌部8分别与相应的正极铝箔3和负极铝箔4焊接,正极引线6的固定舌部8位于正极铝箔3背离电解纸5一侧,负极引线7的固定舌部8位于负极铝箔4背离电解纸5一侧;其中,负极铝箔4为腐蚀化成铝箔,电解纸5的宽度为3mm,正极铝箔3和负极铝箔4的宽度分别为2.2mm。
本实用新型的正极引线6和负极引线7采用焊接方式固定于相应的正极铝箔3和负极铝箔4,在相应的正极引线6和负极引线7焊接过程中不会产生毛刺现象,进而避免了电解纸5被刺穿以及由于毛刺所引起的电容器短路击穿甚至爆炸等缺陷;另外,至少三层电解纸5叠加的电解纸层能够保证足够的厚度,焊接时所产生的凸起位置很难刺破电解纸5层;正极引线6和负极引线7分别背离电解纸5安装。
需进一步解释,由腐蚀化成铝箔制备而成的负极铝箔4能够承受反向漏电流的冲击,进而能够有效地延长本实用新型的使用寿命。
综合上述情况可知,本实用新型具有结构稳定、使用寿命长的优点。
以上内容仅为本实用新型的较佳实施例,对于本领域的普通技术人员,依据本实用新型的思想,在具体实施方式及应用范围上均会有改变之处,本说明书内容不应理解为对本实用新型的限制。
Claims (1)
1.一种铝电解电容器,其特征在于:包括有铝圆筒(1)以及嵌装于铝圆筒(1)内的电容器芯包(2),电容器芯包(2)包括有宽度相等的正极铝箔(3)和负极铝箔(4),正极铝箔(3)和负极铝箔(4)之间装设有至少三层宽度较正极铝箔(3)和负极铝箔(4)的宽度大的电解纸(5),正极铝箔(3)焊装有正极引线(6),负极铝箔(4)焊装有负极引线(7),正极引线(6)和负极引线(7)分别设置有固定舌部(8),固定舌部(8)分别与相应的正极铝箔(3)和负极铝箔(4)焊接,正极引线(6)的固定舌部(8)位于正极铝箔(3)背离电解纸(5)一侧,负极引线(7)的固定舌部(8)位于负极铝箔(4)背离电解纸(5)一侧;其中,正极铝箔(3)和负极铝箔(4)分别为腐蚀化成铝箔,电解纸(5)的宽度为3mm,正极铝箔(3)和负极铝箔(4)的宽度分别为2.2mm。