CN203048855U - 一种低熔点和耐候性的pu热熔膜 - Google Patents
一种低熔点和耐候性的pu热熔膜 Download PDFInfo
- Publication number
- CN203048855U CN203048855U CN 201220392016 CN201220392016U CN203048855U CN 203048855 U CN203048855 U CN 203048855U CN 201220392016 CN201220392016 CN 201220392016 CN 201220392016 U CN201220392016 U CN 201220392016U CN 203048855 U CN203048855 U CN 203048855U
- Authority
- CN
- China
- Prior art keywords
- melting point
- film
- low melting
- hot melting
- polyurethane
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型提供一种低熔点和耐候性的PU热熔膜,该PU热熔膜结构简单,受设备和加工工艺的限制小,易于生产加工,且膜层之间配合合理,利于充分发挥热熔膜的优良性能,可广泛应用于多种面料。为了达到上述目的,本实用新型的技术方案:一种低熔点和耐候性的PU热熔膜,包括离型纸和聚氨酯胶粘层,所述的离型纸和聚氨酯胶粘层依次层状复合。与现有技术相比,本实用新型具有以下优点:本实用新型产品的熔点低,可广泛应用于多种面料中,尤其是对温度敏感的薄面料中。
Description
技术领域
本实用新型涉及热熔膜领域,具体涉及一种低熔点和耐候性的PU热熔膜。
背景技术
热封膜是利用压胶机或者热压机加热,粘贴在面料的接缝处,达到较好密封效果的一种薄膜,被越来越广泛地应用于风雨衣、滑雪衣、帐篷、摩托车雨衣、潜水服、防水鞋、防水袋等防水系列产品中。
传统的服装制造业是采用车缝的方式进行生产的,这种生产方式对车缝技能的要求较高,员工入厂后需要经过较长时间的培训才能掌握车缝技能,即使掌握了车缝技能的员工在工作中也难免会出错,造成残品、次品。
热熔膜黏贴性好,粘贴在面料的接缝处,取代传统的车缝加工,可以有效避免车缝加工的上述不足,被越来越广泛的应用。
目前,应用热熔膜时其粘贴温度在150~200℃之间,在该温度段进行粘贴工作主要存在以下缺点:
1.热熔膜粘贴温度在150~200℃之间,被粘贴的材料易烫损,造成材料的浪费。
2.热熔膜粘贴温度在150~200℃之间,温度高,则增大了胶粘设备的负荷,缩短了胶粘设备的使用寿命。
实用新型内容
针对现有技术的上述不足,本实用新型提供一种低熔点和耐候性的PU热熔膜,该PU热熔膜结构简单,受设备和加工工艺的限制小,易于生产加工,且膜层之间配合合理,利于充分发挥热熔膜的优良性能,可广泛应用于多种面料。
为了达到上述目的,本实用新型的技术方案:一种低熔点和耐候性的PU热熔膜,包括离型纸和聚氨酯胶粘层,所述的离型纸和聚氨酯胶粘层依次层状复合。
所述的一种低熔点和耐候性的PU热熔膜的使用温度为135-145℃。
所述的一种低熔点和耐候性的PU热熔膜的厚度为0.08-0.15mm。
与现有技术相比,本实用新型具有以下优点:
本实用新型产品的熔点低,可广泛应用于多种面料中,尤其是对温度敏感 的薄面料中。
附图说明
图1为本实用新型一种低熔点和耐候性的PU热熔膜的示意图。
其中,1.离型纸;2.聚氨酯胶粘层。
具体实施方式
为了更好地理解本实用新型的技术方案,下面结合本实用新型的具体实施例和附图加以详细的描述,但本实用新型并不限于该实施例。
一种低熔点和耐候性的PU热熔膜,包括离型纸和聚氨酯胶粘层,所述的离型纸和聚氨酯胶粘层依次层状复合。
本实用新型的聚氨酯胶粘层2的材料中,其主成分为聚氨酯,具备聚氨酯的优良性能,同时,聚氨酯层的厚度为0.08-0.15mm,使本实用新型在135-145℃加工温度下粘贴牢固。
本实用新型可应用于服装中的门襟、袖口、下摆、衣领、拉链、口袋、脚口及服装其他部位的粘合装饰,具有遮盖、定型的作用,低温加工,使用方便。
Claims (3)
1.一种低熔点和耐候性的PU热熔膜,其特征在于,包括离型纸和聚氨酯胶粘层,所述的离型纸和聚氨酯胶粘层依次层状复合。
2.根据权利要求1所述的一种低熔点和耐候性的PU热熔膜,其特征在于,其使用温度为135-145℃。
3.根据权利要求1所述的一种低熔点和耐候性的PU热熔膜,其特征在于,其厚度为0.08-0.15mm。