Prior art keywords
feeding
titanium
branch pipes
titanium sponge
feeding device
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201220460222
Other languages
English (en)
Inventor
张金宝
付永
满茂德
王中启
王世达
景超
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chaoyang Jinda Titanium Industry Co., Ltd.
Original Assignee
CHAOYANG JINDA TITANIUM CO LTD
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHAOYANG JINDA TITANIUM CO LTD filed Critical CHAOYANG JINDA TITANIUM CO LTD
Priority to CN 201220460222 priority Critical patent/CN202786386U/zh
Application granted granted Critical
Publication of CN202786386U publication Critical patent/CN202786386U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Manufacture And Refinement Of Metals (AREA)

Abstract

本实用新型提供一种生产海绵钛的加料装置,以解决现有技术中反应器中心部位海绵钛因温度过高而烧结所带来的一系列问题。本实用新型的加料装置包括加料主管和加料支管,四氯化钛由加料主管进入,由加料支管喷出,加料支管焊接在加料主管上,支管数量为2-6个,直径和长度相同,各支管之间的夹角相同,各支管与主管的夹角为100-160°。该装置可使四氯化钛分散进入反应器,避免集中于中心部位,加快了散热速度,便于提高加料速度,提高了生产效率,另外可以改善钛坨结构,更加利于蒸馏,可缩短蒸馏时间,保证了海绵钛的质量。

Description

一种生产海绵钛的加料装置
技术领域
本实用新型涉及一种有色金属冶炼领域,具体涉及一种用于生产海绵钛的加料装置。
背景技术
镁还原法一直是工业生产海绵钛的主要方法,还原过程是海绵钛生产过程中的关键环节之一。在镁法生产海绵钛的过程中,用金属镁还原四氯化钛制得海绵钛,四氯化钛是通过一根加料管直接加入反应器内,使之与其中的液体金属镁发生反应,反应器内的温度可达800-900℃。四氯化钛进入反应器内,大部分会发生气化与反应器内熔融的镁和镁蒸汽迅速发生反应,生成海绵钛。但当四氯化钛加入的速度较快且集中于反应液面的中间时,有一部分液体的四氯化钛未能气化,会在反应器中心部位与金属镁发生剧烈的反应,使反应液面中心温度不断升高,最高可达1200℃。此部位海绵钛因温度过高而烧结,会造成海绵钛的坨心致密,不易破碎,难以达到产品指标所规定的粒度。生成的海绵钛毛细孔被堵塞,氯化物无法分离,造成钛坨中心产品含氯较高,海绵钛的坨心产品致密,使残存的金属镁及氯化镁等杂质难以去除,严重影响产品质量。另外用户使用这种海绵钛钛块,在熔炼过程不易熔化,产生掉块现象,造成钛锭的局部缺陷。
发明内容
本实用新型的目的在于提供一种生产海绵钛的加料装置,以解决现有技术中反应器中心部位海绵钛因温度过高而烧结所带来的一系列问题。
为实现上述目的,本实用新型采取的技术方案是将反应器内的单一的四氯化钛加料管改为带支管式的加料装置,该装置包括加料主管和加料支管,四氯化钛由加料主管进入,由加料支管喷出。多个加料支管焊接在加料主管上,支管数量为2-6个,直径大小相同,直径为20-50mm,长度为100-400mm,各支管之间的夹角相同,各支管与主管的夹角为100-160°,该角度可根据实际情况调整,支管数量也可根据加料速度和反应器直径大小进行选择。 
本实用新型所述的加料装置,可使四氯化钛分散进入反应器,避免集中于中心部位,克服了现有技术中四氯化钛在反应器中心部位与金属镁剧烈反应,影响海绵钛质量的难题,以及由于钛的导热性差,导致熔体温度过高、造成海绵钛的Fe含量偏高的问题,通过所述加料装置能够降低海绵钛中的铁含量。
本实用新型所述的加料装置提高了散热速度,便于提高加料速度,提高生产效率,缩短生产周期。另外通过所述加料装置,可以改善钛坨结构,更有利于蒸馏,可缩短蒸馏时间,进一步降低电耗,保证了海绵钛的质量。。
附图说明
图1为生产海绵钛的加料装置的示意图。
图2为生产海绵钛的加料系统的示意图。
其中,1是加料主管,2是加料管支管,3是支管之间的角度,4是蒸馏通道,5是大盖,6是反应器。
具体实施方式
实施例1,加料主管焊接两个支管,直径25mm,各支管之间的夹角相同,各支管与加料主管之间的夹角为120°,各支管长度为200mm。
实施例2,加料主管焊接三个支管,直径25mm,各支管之间的夹角相同,各支管与加料主管之间的夹角为135°,各支管长度为250mm。
最后应说明的是:显然,上述实例仅仅是为清楚地说明本实用新型所作的举例,而并非对实施方式的限定。对于所属领域的技术人员来说,在上述说明的基础上还可以做出其它不同形式的变化和变动。这里无需也无法对所有的实施方式予以穷举。而由此所引伸的显而易见的变化或变动仍处于本实用新型的保护范围之中。

Claims (3)

1.一种生产海绵钛的加料装置,其特征在于:该装置包括加料主管(1)和加料支管(2),四氯化钛由加料主管(1)进入,由加料支管(2)喷出。
2.根据权利要求1所述的加料装置,其特征在于所述加料支管(2)焊接在加料主管(1)上,加料支管(2)的数量为2-6个,并且直径和长度均相同,直径为20-50mm,长度为100-400mm。
3.根据权利要求1所述的加料装置,其特征在于所述加料支管(2)之间的夹角相同,所述各加料支管(2)与加料主管(1)之间的夹角为100-160°。
CN 201220460222 2012-09-11 2012-09-11 一种生产海绵钛的加料装置 Expired - Fee Related CN202786386U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201220460222 CN202786386U (zh) 2012-09-11 2012-09-11 一种生产海绵钛的加料装置

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201220460222 CN202786386U (zh) 2012-09-11 2012-09-11 一种生产海绵钛的加料装置

Publications (1)

Publication Number Publication Date
CN202786386U true CN202786386U (zh) 2013-03-13

Family

ID=47813687

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201220460222 Expired - Fee Related CN202786386U (zh) 2012-09-11 2012-09-11 一种生产海绵钛的加料装置

Country Status (1)

Country Link
CN (1) CN202786386U (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN113462908A (zh) * 2021-07-09 2021-10-01 攀钢集团攀枝花钢铁研究院有限公司 一种海绵钛生产反应器及加料方法
CN113718119A (zh) * 2021-09-22 2021-11-30 攀钢集团研究院有限公司 加料管及布料装置
CN116536530A (zh) * 2023-06-19 2023-08-04 遵义钛业股份有限公司 一种生产海绵钛的加料系统

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN113462908A (zh) * 2021-07-09 2021-10-01 攀钢集团攀枝花钢铁研究院有限公司 一种海绵钛生产反应器及加料方法
CN113718119A (zh) * 2021-09-22 2021-11-30 攀钢集团研究院有限公司 加料管及布料装置
CN116536530A (zh) * 2023-06-19 2023-08-04 遵义钛业股份有限公司 一种生产海绵钛的加料系统

Similar Documents

Publication Publication Date Title
CN104032151B (zh) 一种tc4钛合金铸锭的eb冷床炉熔炼方法
CN202786386U (zh) 一种生产海绵钛的加料装置
CN104209526A (zh) 一种微细球形钛合金粉体的制备方法
CN107119199A (zh) 一种低杂质含量钛粉的生产装置及其生产方法
CN202786384U (zh) 一种生产海绵钛的i型炉多点加料装置
CN200974862Y (zh) 一种镁法生产海绵钛的四氯化钛气化装置
CN103773968A (zh) 采用三相联合实现铝熔体除气除渣的方法及系统
CN212504027U (zh) 一种制备四氯化钛的装置
CN202705438U (zh) 用于镁热法海绵钛生产的四氯化钛加料管
CN202272940U (zh) 一种用于制取海绵钛的气化加料装置
CN107199218A (zh) 氧化反应器除疤装置及除疤方法
CN101607345A (zh) 一种降低钛合金搅拌摩擦焊工艺中搅拌头磨损的方法
CN102676879A (zh) 一种用于湿法炼锌锑盐净化除钴的合金锌粉及其制备方法
CN202492377U (zh) 催化剂级三氧化二锑制备装置
CN102330010B (zh) 一种铋包芯线
CN103343227A (zh) 一种净化海绵钛生产中熔融镁的方法及设备
CN104551455B (zh) 一种-70℃低温钢焊条
CN103627847A (zh) 用于稀土钢生产的镧铈混合稀土铁合金
CN208234814U (zh) 二腈熔融提纯一体化装置
CN202517020U (zh) 一种新型上引连铸炉
CN206872910U (zh) 一种低杂质含量钛粉的生产装置
CN203768433U (zh) 一种镁法生产海绵钛的四氯化钛均匀布料装置
CN103555884A (zh) 钙包芯线和使用该钙包芯线对钢水进行钙处理的方法
CN201729668U (zh) 一种无水氯化铝生产装置
CN205675979U (zh) 一种金属溶液吊运装置

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: CHAOYANG JINDA TITANIUM INDUSTRY CO., LTD.

Free format text: FORMER OWNER: CHAOYANG JINDA TITANIUM CO., LTD.

Effective date: 20131108

C41 Transfer of patent application or patent right or utility model
TR01 Transfer of patent right

Effective date of registration: 20131108

Address after: 122000 No. 4, Longshan street, 788, Liaoning, Chaoyang City

Patentee after: Chaoyang Jinda Titanium Industry Co., Ltd.

Address before: 122000 No. four, Longshan street, Twin Towers District, Liaoning, Chaoyang City province 788

Patentee before: Chaoyang Jinda Titanium Co.,Ltd.

CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20130313

Termination date: 20150911

EXPY Termination of patent right or utility model