CN202764293U - 压延复合的钛-钢-钛复合板 - Google Patents

压延复合的钛-钢-钛复合板 Download PDF

Info

Publication number
CN202764293U
CN202764293U CN201220489187.2U CN201220489187U CN202764293U CN 202764293 U CN202764293 U CN 202764293U CN 201220489187 U CN201220489187 U CN 201220489187U CN 202764293 U CN202764293 U CN 202764293U
Authority
CN
China
Prior art keywords
titanium
steel
composite
calendered
board
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN201220489187.2U
Other languages
English (en)
Inventor
高峰
连敬祥
高景阳
连璐
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
LIAONING HUAYANG NEW GROUP
Original Assignee
LIAONING HUAYANG NEW GROUP
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by LIAONING HUAYANG NEW GROUP filed Critical LIAONING HUAYANG NEW GROUP
Priority to CN201220489187.2U priority Critical patent/CN202764293U/zh
Application granted granted Critical
Publication of CN202764293U publication Critical patent/CN202764293U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

压延复合的钛-钢-钛复合板,是复合金属板,复合金属板有上、中、下三层,上、中、下三层分别是钛层、钢层和钛层。制法是取两块压延复合的钢-钛复合板,把钢板面抛光后相贴合,再用压延复合法把两块压延复合的钢-钛复合板复合在一起。本实用新型是在钢板的两面复合有钛板的压延复合板,钛板可以很薄,复合板的成本较低。钛板具有较高的耐腐蚀性能,中间的钢板层具有较强的导热性和导磁性、价格低廉价,适用在食品、制药、化工等行业和腐蚀性较强的场合及制作锅具使用。

Description

压延复合的钛-钢-钛复合板
技术领域
本实用新型涉及一种金属复合板,特别是一种压延复合的钛-钢-钛复合板。
背景技术
在金属材料中,钛是一种强度高、刚性好、耐各种腐蚀性能极强,特别是钛具有与生物相容性好的特点,在医学上可制成人体内用的医疗器械或代用器官,被称为亲生物金属。工业生产中,在食品、制药、化工等行业和腐蚀性较强的使用场合,需要用钛制作容器和设备,钛的价格昂贵,用钛制作的设备价格很高。钢是国民经济中用量最多的重要材料,钢的强度高、刚性好、导热性好,价格低廉,但钢的耐腐蚀性不是很强,钢制的容器和设备不适用在食品、制药、化工等行业和腐蚀性较强的场合使用。
把钛和钢复合,制成钛-钢复合材料是既能满足食品、制药、化工等行业和腐蚀性较强的场合使用并且价格较为低廉,是一种合理的材料。
用爆炸复合法可以把两种不同的金属板材复合在一起制成复合板材。在用爆炸复合法复合不同的金属板时,相邻金属的接触面间原子互相扩散实现冶金结合,但由于瞬间爆炸的冲击力较大,爆炸复合时相邻金属的接触面会产生的冲击波纹和压坑,为了掩盖冲击波纹和压坑,爆炸复合的金属板要有一定的厚度,否则在下一步的轧制中,会露出相邻金属接触面的波纹和压坑,影响复合板的质量。用爆炸复合法制作的钛-钢复合板中,钛层较厚,也使钛-钢复合板的成本较高。
为了制作成本较低的适用在食品、制药、化工等行业和腐蚀性较强的场合使用的钛-钢复合板,中国专利ZL 2009 1 0010100.1中提出了一种压延复合钛钢复合板的制造方法,该制造方法是把钢板与钛板的一侧表面磨光叠合在一起,排出层间空气,把周边缝隙焊封,再把叠合板加热到其共晶温度,在热轧机上热轧熔接,制成钛层较薄的压延复合钛-钢复合板。
这种压延复合钛-钢复合板的制造方法只能制作在钢板的一面复合钛板的二层复合板,在有些场合需要在钢板的两面都复合钛板的三层复合板。
现有技术中,没有压延复合的钛-钢-钛复合板。
发明内容
本实用新型的目的是为了克服上述不足,提出一种压延复合的钛-钢-钛复合板。
本实用新型是用如下方法实现的。
压延复合的钛-钢-钛复合板是复合金属板,复合金属板有上、中、下三层,上、中、下三层分别是钛层、钢层和钛层。
压延复合的钛-钢-钛复合板的制造方法有如下步骤:
(1)取两块长度和宽度相同的压延复合钛-钢复合板,把压延复合钛-钢复合板的钢板一侧的板面用砂轮打磨、钢刷抛光,得到两块钢板一侧板面抛光的压延复合钛-钢复合板;
(2)把两块钢板一侧板面抛光的压延复合钛-钢复合板的钢板抛光板面相对贴合,得到压延复合钛-钢复合板相叠板;
(3)把压延复合钛-钢复合板相叠板用压力机压合平展,把压延复合钛-钢复合板相叠板的周边用电焊的方法熔封,在四层叠合板的四角分别留出小孔,得到周边熔封的压延复合钛-钢复合板相叠板;
(4)把周边熔封的压延复合钛-钢复合板相叠板加热到共晶温度880℃~900℃,把加热后的周边熔封的压延复合钛-钢复合板相叠板用热轧机压延复合,让变形率是70%~80%,得到钛-钢-钛复合坯板;
(5)把压延复合的钛-钢-钛复合坯板扩散退火,把退火的压延复合的钛-钢-钛复合坯板四边焊缝剪开,把退火的压延复合的钛-钢-钛复合坯板从氧化镁粉隔离剂处分开,得到两块钛-钢-钛复合板。
本实用新型是在钢板的两面都复合有钛板的三层复合板,钛板和钢板之间是压延复合,相邻板之间有过渡层,两侧的钛板可以很薄,节省贵重的金属,使复合板的成本较低。钛板具有较高的耐腐蚀性能,钛是对人体健康和味觉无危害的健康金属,中间的钢板层具有较强的导热性和导磁性、价格低廉价,制成的压延复合的钛-钢-钛三层复合板是适用在食品、制药、化工等行业和腐蚀性较强的场合及制作锅具使用。
下面结合附图,对本实用新型作进一步地说明。
附图说明
图1是根据本实用新型的发明方案提出的一种压延复合的钛-钢-钛复合板的立体局剖示意图。
具体实施方式
图1中,压延复合的钛-钢-钛复合板是复合金属板1,复合金属板有上、中、下三层,上、中、下三层分别是钛层2、钢层3和钛层4。

Claims (1)

1.一种压延复合的钛-钢-钛复合板,是复合金属板,其特征在于:复合金属板有上、中、下三层,上、中、下三层分别是钛层、钢层和钛层。
CN201220489187.2U 2012-09-24 2012-09-24 压延复合的钛-钢-钛复合板 Expired - Lifetime CN202764293U (zh)