CN202667571U - 一种用于镁锂合金材料浇铸的保护装置 - Google Patents

一种用于镁锂合金材料浇铸的保护装置 Download PDF

Info

Publication number
CN202667571U
CN202667571U CN 201220398709 CN201220398709U CN202667571U CN 202667571 U CN202667571 U CN 202667571U CN 201220398709 CN201220398709 CN 201220398709 CN 201220398709 U CN201220398709 U CN 201220398709U CN 202667571 U CN202667571 U CN 202667571U
Authority
CN
China
Prior art keywords
ingot mould
lithium alloy
protective device
water
graphite substrate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201220398709
Other languages
English (en)
Inventor
柴东朗
韩百锋
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
XI'AN SIFANG ULTRA-LIGHT MATERIAL Co Ltd
Original Assignee
XI'AN SIFANG ULTRA-LIGHT MATERIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by XI'AN SIFANG ULTRA-LIGHT MATERIAL Co Ltd filed Critical XI'AN SIFANG ULTRA-LIGHT MATERIAL Co Ltd
Priority to CN 201220398709 priority Critical patent/CN202667571U/zh
Application granted granted Critical
Publication of CN202667571U publication Critical patent/CN202667571U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种用于镁锂合金材料浇铸的保护装置,包括有水冷锭模,水冷锭模底部设有石墨衬底,当镁锂合金溶液从上部浇铸到水冷锭模的底部时,石墨衬底石墨衬底导热速度快,迅速将浇点热量散至整个衬底,减小了热量局部积累;由于石墨衬底的缓冲作用,避免了熔液对锭模的直接烧蚀,消除了锭模烧穿的安全隐患;具有安全性高、避免烧蚀水冷锭模特点。

Description

一种用于镁锂合金材料浇铸的保护装置
技术领域
本实用新型属于镁锂合金浇铸技术领域,具体涉及一种用于镁锂合金材料浇铸的保护装置。
背景技术
在镁锂合金浇铸过程中需要水冷冷却,浇铸锭模若全部采用石墨,其缺点在于,石墨强度不够,具有脆性,因此浇铸锭模只能采用金属材料。由于镁锂合金熔液过于活跃,制造浇铸锭模的纯钢材料底部容易被烧蚀。虽然烧蚀速度很慢,但仍然给镁锂合金生产造成了极大地安全隐患;一旦锭模烧蚀烧穿纯钢材料底部,将导致冷却水进入,会造成爆炸等严重后果。由于烧蚀现象极易在熔液浇下与锭模接触的瞬间发生。因为此时在浇点位置热量积累。局部过热无法及时散掉,锭模在烘点被烧蚀。
发明内容
为了克服上述现有技术的不足,本实用新型的目的在于提供一种用于镁锂合金材料浇铸的保护装置,具有安全性高、避免烧蚀水冷锭模特点。
为了实现上述目的,本实用新型采用的技术方案是:一种用于镁锂合金材料浇铸的保护装置,包括有水冷锭模,水冷锭模底部设有石墨衬底。
所述的石墨衬底的厚度为6~10㎜。
所述的石墨衬底的厚度为8㎜。
本实用新型的有益效果是:
本实用新型通过在水冷锭模底加装一层石墨衬底,在镁锂合金材料熔炼铸过程中,防止合金熔液对浇铸锭模进行高温烘蚀及反应,彻底解决烧蚀问题,消除安全隐患。
附图说明
附图1为本实用新型的结构原理图。
具体实施方式
下面结合附图对本实用新型作进一步详细说明。
参见附图1,一种用于镁锂合金材料浇铸的保护装置,包括有水冷锭模1,水冷锭模1底部设有石墨衬底2。
所述的石墨衬底2的厚度为6~10㎜。
所述的石墨衬底2的厚度为8㎜。
本实用新型的工作原理是:
当镁锂合金溶液从上部浇铸到水冷锭模1的底部时,石墨衬底2石墨衬底导热速度快,迅速将浇点热量散至整个衬底,减小了热量局部积累;由于石墨衬底2的缓冲作用,避免了熔液对锭模的直接烧蚀,消除了锭模烧穿的安全隐患;本实用新型也适用于其他需要对浇铸锭模保护的合金的浇铸过程。

Claims (3)

1.一种用于镁锂合金材料浇铸的保护装置,包括有水冷锭模(1),其特征在于,水冷锭模(1)底部设有石墨衬底(2)。
2.根据权利要求1所述的一种用于镁锂合金材料浇铸的保护装置,其特征在于,所述的石墨衬底(2)的厚度为6~10㎜。
3.根据权利要求1所述的一种用于镁锂合金材料浇铸的保护装置,其特征在于,所述的石墨衬底(2)的厚度为8㎜。
CN 201220398709 2012-08-13 2012-08-13 一种用于镁锂合金材料浇铸的保护装置 Expired - Fee Related CN202667571U (zh)