CN202662711U - 一种镍氢电池负极湿法拉浆用模具 - Google Patents
一种镍氢电池负极湿法拉浆用模具 Download PDFInfo
- Publication number
- CN202662711U CN202662711U CN2012202723092U CN201220272309U CN202662711U CN 202662711 U CN202662711 U CN 202662711U CN 2012202723092 U CN2012202723092 U CN 2012202723092U CN 201220272309 U CN201220272309 U CN 201220272309U CN 202662711 U CN202662711 U CN 202662711U
- Authority
- CN
- China
- Prior art keywords
- nickel
- metal hydride
- thickness
- pulling
- mold
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型属于镍氢电池技术领域,提供一种镍氢电池负极湿法拉浆用模具。这种镍氢电池负极湿法拉浆用模具,包括相对设置的上下模板,上下模板的相对位置处分别设有凹槽,上下模板的凹槽底部之间距离与负极片主体部分的厚度相当,上下模板之间的距离小于负极片主体部分的厚度。根据本实用新型的镍氢电池负极湿法拉浆用模具,采用一步即可制作出尾部较主体部分厚度小的负极片,节省电池极芯占用的空间,降低高容量电池开发难度及制作难度,有利于电池成品率的提高,同时可以使活性物质更好的粘附于负极基体,同时减少活性物质的用量,节约成本。
Description
技术领域
本实用新型涉及镍氢电池,尤其涉及一种镍氢电池负极湿法拉浆用模具。
背景技术
镍氢负极极片通常为横截面为长方形二侧均匀涂覆活性物质,或极片尾部在涂覆好后再进行去除基体一侧的活性物质,拉浆模具通常为平板型模具,但存在以下几点缺点:1,活性物质被均匀分配于的整个负极基体,前端单位面积活性物质与与正极配对的N/P值未增加,电池的过充性能及二次电池充放电循环次数性能一般。2,如果二侧均匀涂覆活性物质极片尾部贴近钢壳部份活性物质过量,造成成本上浪费。3,在高容量电池卷绕过程中卷绕较紧,不利于节省电池极芯占用空间,使高容量电池开发难度及制作难度较大,不利于电池成品率的提高。4,如果极片尾部在涂覆好后再进行去除除基体一侧的活性物质,尾侧活性物质粘附性较弱,在充放电过程中脱落。
实用新型内容
本实用新型的目的在于克服现有技术的不足,提供一种镍氢电池负极湿法拉浆用模具。
为实现上述目的,本实用新型采用的技术方案为:
一种镍氢电池负极湿法拉浆用模具,包括相对设置的上下模板,上下模板的相对位置处分别设有凹槽,上下模板的凹槽底部之间距离与负极片主体部分的厚度相当,上下模板之间的距离小于负极片主体部分的厚度。
所述上下模板之间的距离为负极片主体部分厚度的0.5-0.8倍。
所述上下模板之间的距离为负极片主体部分厚度的0.6倍。
本实用新型的有益效果:采用一步即可制作出尾部较主体部分厚度小的负极片,节省电池极芯占用的空间,降低高容量电池开发难度及制作难度,有利于电池成品率的提高,同时可以使活性物质更好的粘附于负极基体,同时减少活性物质的用量,节约成本。
附图说明
图1是采用本实用新型优选实施例的模具制出的负极片横截面示意图。
图2是本实用新型优选实施例的镍氢电池负极湿法拉浆用模具示意图。
具体实施方式
参见图2,一种镍氢电池负极湿法拉浆用模具,包括上模板20及下模板30,上模板20及下模板30通过模具组装件安装及拆卸。上模板20及下模板30相对位置处分别设有凹槽21和31。上模板20及下模板30之间的距离为凹槽21和31底部之间距离的0.6倍。
参见图1,采用上述模具用湿法拉浆制作出的负极片子10,拉浆涂覆过程中制备出尾部的附料量较少,厚度较薄,基体二侧均匀涂覆活性物质的负极极片,其中尾部12厚度为主体部分11厚度的0.6倍。通过此方法,可以节省电池极芯占用的空间,降低高容量电池开发难度及制作难度,有利于电池成品率的提高,同时可以使活性物质更好的粘附于负极基体,同时减少活性物质的用量,节约成本。
以上内容是结合具体的优选实施方式对本实用新型所作的进一步详细说明,不能认定本实用新型的具体实施只局限于这些说明。对于本实用新型所属技术领域的普通技术人员来说,在不脱离本实用新型构思的前提下,作出具体的改变或变化均属于本实用新型的保护范围。
Claims (3)
1.一种镍氢电池负极湿法拉浆用模具,其特征在于:包括相对设置的上下模板,上下模板的相对位置处分别设有凹槽,上下模板的凹槽底部之间距离与负极片主体部分的厚度相当,上下模板之间的距离小于负极片主体部分的厚度。
2.根据权利要求1所述的镍氢电池负极湿法拉浆用模具,其特征在于:所述上下模板之间的距离为负极片主体部分厚度的0.5-0.8倍。
3.根据权利要求2所述的镍氢电池负极湿法拉浆用模具,其特征在于:所述上下模板之间的距离为负极片主体部分厚度的0.6倍。