CN202629358U - 抗冲刷耐磨陶瓷复合管道 - Google Patents

抗冲刷耐磨陶瓷复合管道 Download PDF

Info

Publication number
CN202629358U
CN202629358U CN2012201806740U CN201220180674U CN202629358U CN 202629358 U CN202629358 U CN 202629358U CN 2012201806740 U CN2012201806740 U CN 2012201806740U CN 201220180674 U CN201220180674 U CN 201220180674U CN 202629358 U CN202629358 U CN 202629358U
Authority
CN
China
Prior art keywords
wear
resistant
pipeline
ceramic
layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2012201806740U
Other languages
English (en)
Inventor
陈兵
姜进涛
谢新兵
陈小国
李四化
李畔玲
颜继鹏
谢春兵
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG BORUN PROCESS INDUSTRIAL TECHNOLOGY CORP Ltd
Original Assignee
SHANDONG BORUN PROCESS INDUSTRIAL TECHNOLOGY CORP Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG BORUN PROCESS INDUSTRIAL TECHNOLOGY CORP Ltd filed Critical SHANDONG BORUN PROCESS INDUSTRIAL TECHNOLOGY CORP Ltd
Priority to CN2012201806740U priority Critical patent/CN202629358U/zh
Application granted granted Critical
Publication of CN202629358U publication Critical patent/CN202629358U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种抗冲刷耐磨陶瓷复合管道,属于耐磨管道领域。抗冲刷耐磨陶瓷复合管道,包括外层的管道基体和内层的高铝陶瓷耐磨层,管道基体和高铝陶瓷耐磨层之间通过胶质体粘结层粘接,其特征在于:高铝陶瓷耐磨层由高铝陶瓷矩形单元组合而成,位于同一行的矩形单元并行排列,上、下相邻的矩形单元的边缘不在同一条直线上。本复合管道中的高铝陶瓷矩形单元采用错缝粘结的方式粘结在管道基体内侧,能够防止高铝陶瓷矩形单元大面积脱落,从而保证了耐磨管道的使用年限,延长了其服役寿命,减少了检修周期和维护成本,经济效益可观。

Description

抗冲刷耐磨陶瓷复合管道
技术领域
本实用新型涉及一种抗冲刷耐磨陶瓷复合管道,属于耐磨管道领域。
背景技术
耐磨层是耐磨管道的核心部分,目前高铝陶瓷耐磨管道大多是通过胶粘结方式将陶瓷耐磨层和金属基体粘结在一起成型为复合管路。但由于耐磨管道使用条件非常恶劣,在实际生产的长期严酷条件下,高速流动的物料会对高铝陶瓷片之间的缝隙产生冲刷,导致陶瓷之间缝隙变大,而缝隙中都是胶质体粘结剂,耐磨损能力很差,如果长时间经受冲刷,缝隙往往会很快磨穿,导致陶瓷片脱落,而且在高铝陶瓷耐磨管路中,由于陶瓷片都是上下对齐粘在管路中,这样当物料在流动时会对一条直线上的缝隙不断连续的进行冲刷,一旦有一块陶瓷脱落,会导致其余陶瓷片大面积脱落,使管道失去耐磨特性,大大的降低了耐磨管道的使用寿命,并且影响工厂的生产,造成经济损失。
实用新型内容
根据以上现有技术中的不足,本实用新型要解决的技术问题是:提供一种耐磨性能好、耐磨层不易脱落且使用寿命长的抗冲刷耐磨陶瓷复合管道。
本实用新型解决其技术问题所采用的技术方案是:所述的抗冲刷耐磨陶瓷复合管道,包括外层的管道基体和内层的高铝陶瓷耐磨层,管道基体和高铝陶瓷耐磨层之间通过胶质体粘结层粘接,其特征在于:高铝陶瓷耐磨层由高铝陶瓷矩形单元组合而成,位于同一行的矩形单元并行排列,上、下相邻的矩形单元的边缘不在同一条直线上。
本抗冲刷陶瓷耐磨陶瓷复合管道采用错缝粘结,即上、下相邻的矩形单元边缘不在同一条直线上,当流体冲刷时,由于上、下相邻的矩形单元之间的连接矩形单元间缝隙是相互错开的,避免了因流体对胶质体缝隙的不断冲刷而导致缝隙提前被磨穿,从而防止了高铝陶瓷矩形单元的大面积脱落,这样就保证了耐磨管道的使用年限,大大的延长了其服役寿命,并减少了业主的维护费用和检修周期,带来可观的经济效益。
本实用新型所具有的有益效果是:
本复合管道中的高铝陶瓷矩形单元采用错缝粘结的方式粘结在管道基体内侧,能够防止高铝陶瓷矩形单元大面积脱落,从而保证了耐磨管道的使用年限,延长了其服役寿命,减少了检修周期和维护成本,,经济效益可观。
附图说明
图1是本实用新型的截面图;
图2是本实用新型的展开图。
图中:1、管道基体;2、胶质体粘结层;3、矩形单元。
具体实施方式
下面结合附图对本实用新型的实施例做进一步描述:
如图1、2所示,抗冲刷耐磨陶瓷复合管道,包括外层的管道基体1和内层的高铝陶瓷耐磨层,管道基体1和高铝陶瓷耐磨层之间通过胶质体粘结层2粘接,高铝陶瓷耐磨层由高铝陶瓷矩形单元3组合而成,位于同一行的矩形单元并行排列,上、下相邻的矩形单元的边缘不在同一条直线上,本实施例中,下边矩形单元的边缘对齐上边矩形单元的中心位置(如图2所示)。
本抗冲刷陶瓷耐磨陶瓷复合管道采用错缝粘结,即上、下相邻的矩形单元边缘不在同一条直线上,当流体冲刷时,由于上、下相邻的矩形单元之间的连接矩形单元间缝隙是相互错开的,避免了因流体对胶质体缝隙的不断冲刷而导致缝隙提前被磨穿,从而防止了陶瓷片大面积脱落的现象。

Claims (1)

1.一种抗冲刷耐磨陶瓷复合管道,包括外层的管道基体和内层的高铝陶瓷耐磨层,管道基体和高铝陶瓷耐磨层之间通过胶质体粘结层粘接,其特征在于:高铝陶瓷耐磨层由高铝陶瓷矩形单元组合而成,位于同一行的矩形单元并行排列,上、下相邻的矩形单元的边缘不在同一条直线上。
CN2012201806740U 2012-04-25 2012-04-25 抗冲刷耐磨陶瓷复合管道 Expired - Fee Related CN202629358U (zh)