CN202388858U CN2011204734896U CN201120473489U CN202388858U CN 202388858 U CN202388858 U CN 202388858U CN 2011204734896 U CN2011204734896 U CN 2011204734896U CN 201120473489 U CN201120473489 U CN 201120473489U CN 202388858 U CN202388858 U CN 202388858U
Authority
CN
China
Prior art keywords
environment
steel plate
layer
thickness
bronze powder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011204734896U
Other languages
English (en)
Inventor
王明祥
朱豪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mingyang Technology (Suzhou) Co., Ltd.
Original Assignee
WUJIANG MINGYANG ADVANCED MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUJIANG MINGYANG ADVANCED MATERIAL CO Ltd filed Critical WUJIANG MINGYANG ADVANCED MATERIAL CO Ltd
Priority to CN2011204734896U priority Critical patent/CN202388858U/zh
Application granted granted Critical
Publication of CN202388858U publication Critical patent/CN202388858U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Abstract

本实用新型涉及一种环保型自润滑复合板,包括钢板层,钢板层上下两面均设置有电镀层,所述钢板层的上表面电镀层上设置有青铜粉,青铜粉上面设置有改性聚四氟乙烯摩擦层。本实用新型的优点是,这种环保型自润滑复合板具有很好的自润滑性能和耐磨性能,同时材料中不含金属铅和铅的化合物,以及其他重金属及其化合物,有利于环保,并且材料的摩擦系数小、耐磨性能好、使用寿命长。

Description

环保型自润滑复合板
技术领域
本实用新型涉及一种复合材料,尤其是涉及一种环保型自润滑复合板。 
背景技术
目前自润滑材料有很多,一般自润滑材料为了提高耐磨性能,在材料中会添加了对环境有害的金属及其化合物,使用最多的是金属铅,因为在自润滑材料中加入金属铅可以极大的提高材料的耐磨性。有资料表明,除了铅之外,一些其它有害物质对提高自润滑材料的耐磨性也有帮助,在有些材料体系中,也会加入这些物质。这些有害物质的加入是以牺牲环境为代价的,环境的恶化已经引起了广泛的关注,国内外先后出台了一系列保护环境的政策和法规,如目前有些发达国家对进出口产品的含铅量作了明确的规定和要求,严格限制含铅量超标产品的进口和生产。因此,要实现整个产品的无铅化,就要实现使用材料的无铅化。 
发明内容
本实用新型所要解决的技术问题是提供一种无污染、耐磨性强以及润滑性好的环保型自润复合板。 
为了解决上述技术问题,本实用新型是通过以下技术方案实现的。
这种环保型自润滑复合板,包括钢板层,钢板层上下两面均设置有电镀层,所述钢板层的上表面电镀层上设置有青铜粉,青铜粉上面设置有改性聚四氟乙烯摩擦层。
进一步地,所述电镀层厚度为0.005-0.01mm,钢板层厚度为0.7-2.3mm,青铜粉粒度为40目—160目,厚度为0.2-0.3mm,改性聚四氟乙烯摩擦层厚度为0.01-0.03 mm。
与现有技术相比,本实用新型的有益之处是:这种环保型自润滑复合板具有很好的自润滑性能和耐磨性能,同时材料中不含金属铅和铅的化合物,以及其他重金属及其化合物,有利于环保,并且材料的摩擦系数小、耐磨性能好、使用寿命长。
附图说明:
下面结合附图对本实用新型进一步说明。
图1是本实用新型环保型自润滑复合板结构示意图。
图中:1、电镀层; 2、钢板层; 3、青铜粉; 4、改性聚四氟乙烯摩擦层。
具体实施方式:
下面结合附图及具体实施方式对本实用新型进行详细描述:
图1所示一种环保型自润符合板,包括钢板层2,钢板层2的厚度为0.7-2.3mm,所述钢板层2上下两面均设置有厚度为0.005-0.01mm电镀层1,所述钢板层2的上表面电镀层1上设置有青铜粉3,该青铜粉3的粒度为40目—160目,厚度为0.2-0.3mm;所述青铜粉3上面设置有由成分比为5%-30%玻璃纤维、1%—15%铁的氧化物、1000目-200目10%—30%电解铜粉或雾化铜粉以及25%—85%聚四氟乙烯合成的改性聚四氟乙烯摩擦层4,并且改性聚四氟乙烯摩擦层厚度为0.01-0.03 mm。
实施例1:
选取厚度为1.0mm、镀铜层厚为0.005mm的钢板,青铜粉3的粒度为40目,厚度为0.2mm,改性聚四氟乙烯层4的成分为玻璃纤维10%,铁的氧化物2%,200目的电解铜粉10%,聚四氟乙烯78%。
实施例2:
选取厚度为1.2mm、镀锡层厚为0.007mm的钢板,青铜粉3的粒度为80目,厚度为0.24mm,改性聚四氟乙烯层4的成分为玻璃纤维5%,铁的氧化物10%,500目的电解铜粉20%,聚四氟乙烯65%.
实施例3:
选取厚度为1.5mm、镀铜层厚为0.01mm的钢板,青铜粉3的粒度为160目,厚度为0.28mm,改性聚四氟乙烯层的成分为玻璃纤维30%,铁的氧化物5%,900目的电解铜粉30%,聚四氟乙烯35%。
实施例1、实施例2及实施例3的工艺步骤如下,首先将青铜粉3混合均匀,再将青铜粉3均匀的铺于钢板上,经隧道炉高温烧结后轧平,高温隧道炉的烧结温度为750-930℃;之后在青铜粉3表面均匀的涂上改性聚四氟乙烯层4后经复合轧制,复合轧制好的板材于氮气保护炉中烧结,烧结温度为350-460℃,烧结时间60-90min,烧结后即可得到该环保型自润滑材料。
需要强调的是:以上仅是本实用新型的较佳实施例而已,并非对本实用新型作任何形式上的限制,凡是依据本实用新型的技术实质对以上实施例所作的任何简单修改、等同变化与修饰,均仍属于本实用新型技术方案的范围内。

Claims (2)

1.一种环保型自润滑复合板,其特征在于:包括钢板层(2),钢板层(2)上下两面均设置有电镀层(1),所述钢板层(2)的上表面电镀层(1)上设置有青铜粉(3),青铜粉(3)上面设置有改性聚四氟乙烯摩擦层(4)。
2.根据权利要求1所述的环保型自润滑复合板,其特征在于:所述电镀层(1)厚度为0.005-0.01mm,钢板层(2)厚度为0.7-2.3mm,青铜粉(3)粒度为40目—160目,厚度为0.2-0.3mm,改性聚四氟乙烯摩擦层(4)厚度为0.01-0.03 mm。
CN2011204734896U 2011-11-24 2011-11-24 环保型自润滑复合板 Expired - Fee Related CN202388858U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2011204734896U CN202388858U (zh) 2011-11-24 2011-11-24 环保型自润滑复合板

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2011204734896U CN202388858U (zh) 2011-11-24 2011-11-24 环保型自润滑复合板

Publications (1)

Publication Number Publication Date
CN202388858U true CN202388858U (zh) 2012-08-22

Family

ID=46663808

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2011204734896U Expired - Fee Related CN202388858U (zh) 2011-11-24 2011-11-24 环保型自润滑复合板

Country Status (1)

Country Link
CN (1) CN202388858U (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102941706A (zh) * 2012-11-21 2013-02-27 吴江市明阳新材料科技有限公司 一种环保耐磨自润滑轴承材料板制备方法

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102941706A (zh) * 2012-11-21 2013-02-27 吴江市明阳新材料科技有限公司 一种环保耐磨自润滑轴承材料板制备方法

Similar Documents

Publication Publication Date Title
CN104384503B (zh) 一种铁铜基粉末冶金减摩材料及其制备方法
CN102555345A (zh) 一种三层复合自润滑板材及其制造方法
CN101367278A (zh) 一种环保型自润滑材料
CN102941706A (zh) 一种环保耐磨自润滑轴承材料板制备方法
CN202388858U (zh) 环保型自润滑复合板
CN102925740A (zh) 一种以镀铜Ti3AlC2增强受电弓滑板材料的制备方法
CN102994914B (zh) 铁钼石墨系高温自润滑复合材料及其制备方法
CN1085794C (zh) 烧结轴承用复合金属粉末及含油烧结轴承
CN1967001A (zh) 氟聚苯酯弹性金属塑料轴承
CN102490411A (zh) 一种环保型自润滑复合板
KR20160133237A (ko) 복합 소재로 이루어진 슬라이딩층을 포함하는 무급유 베어링 및 이의 제조방법
CN102766840A (zh) 钢换热器管束表面改性锌铝稀土共渗方法及其渗剂
CN111876049A (zh) 一种石墨烯冷涂锌涂料及其制备方法
CN101418390A (zh) 易翻边的铜合金金属材料生产工艺
CN207687192U (zh) 一种含油轴承
CN103317129B (zh) 一种高耐磨轴承
CN216100823U (zh) 一种铝基-塑料多层复合自润滑板材
CN201925347U (zh) 一种机动车发动机用铝青铜轴瓦
CN204097554U (zh) 聚四氟乙烯基耐腐蚀固体润滑膜
CN102002621B (zh) 受流器滑块用炭基复合材料及其制备方法
CN109334161A (zh) 一种高性能自润滑复合材料及其制备方法
CN201283683Y (zh) 一种高性能二层复合自润滑卷制轴承材料
CN104647827A (zh) 一种铜合金-钢双金属复合材料及其制备方法和应用
CN201771968U (zh) 双硬锡镀层轴瓦
CN205366866U (zh) 一种平行导轨

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C56 Change in the name or address of the patentee

Owner name: MINGYANG TECHNOLOGY (SUZHOU) CO., LTD.

Free format text: FORMER NAME: WUJIANG MINGYANG NEW MATERIAL SCIENCE + TECHNOLOGY CO., LTD.

CP01 Change in the name or title of a patent holder

Address after: 215216, No. 281 East Village Road, Tongli Town, Wujiang City, Jiangsu, Suzhou

Patentee after: Mingyang Technology (Suzhou) Co., Ltd.

Address before: 215216, No. 281 East Village Road, Tongli Town, Wujiang City, Jiangsu, Suzhou

Patentee before: Wujiang Mingyang Advanced Material Co., Ltd.

CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20120822

Termination date: 20151124