CN202329110U - 导电氮化硼蒸发坩埚 - Google Patents

导电氮化硼蒸发坩埚 Download PDF

Info

Publication number
CN202329110U
CN202329110U CN2011204439999U CN201120443999U CN202329110U CN 202329110 U CN202329110 U CN 202329110U CN 2011204439999 U CN2011204439999 U CN 2011204439999U CN 201120443999 U CN201120443999 U CN 201120443999U CN 202329110 U CN202329110 U CN 202329110U
Authority
CN
China
Prior art keywords
crucible
pot body
borazon
evaporator
conduction
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011204439999U
Other languages
English (en)
Inventor
巩长生
宫伯昌
任学美
巩晓
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG PENGCHENG SPECIAL CERAMICS CO Ltd
Original Assignee
SHANDONG PENGCHENG SPECIAL CERAMICS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG PENGCHENG SPECIAL CERAMICS CO Ltd filed Critical SHANDONG PENGCHENG SPECIAL CERAMICS CO Ltd
Priority to CN2011204439999U priority Critical patent/CN202329110U/zh
Application granted granted Critical
Publication of CN202329110U publication Critical patent/CN202329110U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种蒸发坩埚,具体涉及一种导电氮化硼蒸发坩埚,包括锅体,锅体上部开设有物料凹槽,锅体底部开设有凹槽,其特征在于物料凹槽表面复合有防粘涂层。本实用新型结构简单,制作简便,利用氮化硼的优良特性从而使坩埚更加耐高温,并且避免与锅体反应,防粘涂层有效的防止物料与锅体的粘附。

Description

导电氮化硼蒸发坩埚
技术领域
本实用新型涉及一种蒸发坩埚,具体涉及一种导电氮化硼蒸发坩埚。
背景技术
目前用于难熔金属,特别是用于铁、铜、铝、锌等难熔金属以及单晶硅等的熔解冶炼,是在真空状态下,将待蒸发材料通电加热,达到金属材料熔点后熔化蒸发,用于金属涂层的蒸镀。
传统用于难熔金属以及单晶硅熔解的熔解炉主要材料为石墨,现有的石墨坩埚在熔炼过程中其锅体容易被铁、铜渣等沉渣料所粘附,从而导致石墨坩埚锅体出现裂缝,缩短了使用寿命。
实用新型内容
根据以上现有技术的不足,本实用新型所要解决的技术问题是:提供一种导电氮化硼蒸发坩埚,能够解决沉渣料粘附锅体的问题,从而延长坩埚的使用寿命。
本实用新型所述的一种导电氮化硼蒸发坩埚,包括锅体,锅体上部开设有物料凹槽,锅体底部开设有凹槽,物料凹槽表面复合有防粘涂层。
其中,物料凹槽的开口形状优选为圆形。
本实用新型采用氮化硼来代替石墨作为坩埚的制作原料,氮化硼可加热的温度高,并且不与金属发生反应,还能熔解一些普通坩埚难以熔解的金属与非金属材料。
本实用新型在制作好坩埚锅体后,在高温离心作用下将熔融的防粘涂层附于物料凹槽的表面,防粘涂层能有效的防止物料与锅体的粘附。
本实用新型所具有的有益效果是:结构简单,制作简便,利用氮化硼的优良特性从而使坩埚更加耐高温,并且避免与锅体反应,防粘涂层有效的防止物料与锅体的粘附。
附图说明
图1为本实用新型的结构示意图;
图2为图1的俯视图;
图中:1、锅体  2、物料凹槽  3、凹槽  4、防粘涂层。
具体实施方式
以下结合附图对本实用新型做进一步描述。
如图1和图2所示,本实用新型所述的一种导电氮化硼蒸发坩埚,包括锅体1,锅体1上部开设有物料凹槽2,锅体1底部开设有凹槽3,物料凹槽2表面复合有防粘涂层4。
其中,物料凹槽2的开口形状为圆形。
本实用新型采用氮化硼来代替石墨作为坩埚的制作原料,氮化硼可加热的温度高,并且不与金属发生反应,还能熔解一些普通坩埚难以熔解的金属与非金属材料。
本实用新型在制作好坩埚锅体1后,在高温离心作用下将熔融的防粘涂层4附于物料凹槽2的表面,防粘涂层4能有效的防止物料与锅体1的粘附。
本实用新型结构简单,制作简便,利用氮化硼的优良特性从而使坩埚更加耐高温,并且避免与锅体1反应,防粘涂层4有效的防止物料与锅体1的粘附。

Claims (2)

1.一种导电氮化硼蒸发坩埚,包括锅体,锅体上部开设有物料凹槽,锅体底部开设有凹槽,其特征在于物料凹槽表面复合有防粘涂层。
2.根据权利要求1所述的一种导电氮化硼蒸发坩埚,其特征在于物料凹槽的开口形状为圆形。
CN2011204439999U 2011-11-10 2011-11-10 导电氮化硼蒸发坩埚 Expired - Fee Related CN202329110U (zh)